# US 2012/0055287 A1 · Method for simultaneously producing iron, coke, and power

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0055287 A1
- Document ID: US20120055287A1
- Status: Published application
- Kind: A1
- Application number: 13/225,900
- Filed: 2011-09-06
- Published: 2012-03-08
- Earliest claimed: 2010-09-03
- Assignees: Forest Vue Research, LLC
- Inventors: Michael P. Barkdoll
- Web page: https://patentgrep.com/patent/US20120055287A1

## CPC

- C21B 15/02: Metallothermic processes, e.g. thermit reduction
- C21C 2100/06: Energy from waste gas used in other processes
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS

## Abstract

An alternative ironmaking process for simultaneously producing a highly metalized iron/steel product, coke from coal, an iron/steel product from an iron rich feedstock, and, optionally, energy using heat recovery. The simultaneous process is performed in the environment of a non-recovery or heat recovery coke oven. The iron rich feedstock is layered on top of a coal bed. The iron rich feedstock and coal bed are heated in the presence of a reducing gas to reduce the iron oxides of the iron rich feedstock into the iron/steel product and to devolatilize the coal into coke. After quenching the iron/steel product and coke, the iron/steel product is separated from the coke.

## Claims

### Claim 1

A process for simultaneously producing reduced iron from iron rich wastes and coke from coal, said process comprising the steps of:
forming a plurality of shaped cavities in a top surface of a bed comprising coal;
placing a layer of feedstock containing iron oxides on said top surface of said bed;
placing said bed in a coke oven selected from the group consisting of non-recovery coke ovens and heat recovery coke ovens;
maintaining said coke oven at a reduction temperature for a selected cycle time, said reduction temperature being a temperature sufficient to reduce said iron oxides into reduced iron and to devolatilize said coal in said bed into coke;
providing a reducing gas in said coke oven during said selected cycle time, said reducing gas being a gas that causes said iron oxides to reduce to reduced iron at said reduction temperature;
heating said coke oven to a melting temperature greater than the melting point of said reduced iron to fill said shaped receptacles with said reduced iron;
removing said bed and said reduced iron from said coke oven while keeping said bed substantially intact; and
cooling said bed and said reduced iron to a temperature sufficient to solidify said reduced iron.

### Claim 2 (depends on 1)

The process of claim 1 further comprising the step of forming a sloped region around each of said plurality of shaped cavities.

### Claim 3 (depends on 1)

The process of claim 1 further comprising the step of separating said reduced iron from said bed.

### Claim 4 (depends on 1)

The process of claim 1 characterized in that said feedstock is selected from the group consisting of mill scale, hematite fines, magnetite fines, blast furnace dust, blast furnace sludge, basic oxygen furnace dust, basic oxygen furnace sludge, oily mill scale, and thermally treated electric arc furnace dust.

### Claim 5 (depends on 1)

The process of claim 1 characterized in that said reducing gas consists essentially of H2, CH4, and CO.

### Claim 6 (depends on 1)

The process of claim 1 characterized in that said reducing gas is a byproduct of devolatilizing said coal in said bed.

### Claim 7 (depends on 1)

The process of claim 1 characterized in that said iron oxides consists essentially of FeO, Fe2O3, and Fe3O4.

### Claim 8 (depends on 1)

The process of claim 1 wherein said reduction temperature is between about 760° C. (1400° F.) and about 1648° C. (3000° F.).

### Claim 9 (depends on 1)

The process of claim 1 wherein said reduction temperature is between about 1316° C. (2400° F.) and about 1398° C. (2550° F.).

### Claim 10 (depends on 1)

The process of claim 1 wherein said reduction time is selected based on the reduction temperature and the porosity of said iron oxides.

### Claim 11 (depends on 1)

The process of claim 1 characterized in that said reduction time is between about 15 minutes and about 72 hours.

### Claim 12 (depends on 1)

The process of claim 1 characterized in that said reduction time is between about 1.5 hours and about 48 hours.

### Claim 13

A process for simultaneously producing reduced iron from iron rich wastes and coke from coal, said process comprising the steps of:
placing a layer of feedstock containing iron oxides on a bed comprising coal;
placing said bed in a coke oven selected from the group consisting of non-recovery coke ovens and heat recovery coke ovens;
maintaining said coke oven at a reduction temperature for a selected cycle time, said reduction temperature being a temperature sufficient to reduce said iron oxides into reduced iron and to devolatizes said coal in said bed into coke;
providing a reducing gas in said coke oven during said selected cycle time, said reducing gas being a gas that causes said iron oxides to reduce to reduced iron at said reduction temperature;
heating said coke oven to a melting temperature greater than the melting point of said reduced iron;
removing said bed and said reduced iron from said coke oven while keeping said coke bed substantially intact; and
cooling said bed and said reduced iron to a temperature sufficient to solidify said reduced iron.

### Claim 14 (depends on 13)

The process of claim 13 further comprising the step of separating said reduced iron from said bed.

### Claim 15 (depends on 13)

The process of claim 13 characterized in that said feedstock is selected from the group consisting of mill scale, hematite fines, magnetite fines, blast furnace dust, blast furnace sludge, basic oxygen furnace dust, basic oxygen furnace sludge, oily mill scale, and thermally treated electric arc furnace dust.

### Claim 16 (depends on 13)

The process of claim 13 characterized in that said reducing gas consists essentially of H2, CH4, and CO.

### Claim 17 (depends on 13)

The process of claim 13 characterized in that said iron oxides consist essentially of FeO, Fe2O3, and Fe3O4.

### Claim 18 (depends on 13)

The process of claim 13 wherein said reduction temperature is between about 760° C. (1400° F.) and about 1648° C. (3000° F.).

### Claim 19 (depends on 13)

The process of claim 13 wherein said reduction temperature is between about 982° C. (1800° F.) and about 1398° C. (2550° F.).

### Claim 20 (depends on 13)

The process of claim 13 characterized in that said reduction time is between about 15 minutes and about 72 hours.

### Claim 21 (depends on 13)

The process of claim 13 characterized in that said reduction time is between about 1.5 hours and about 48 hours.