# US 2011/0301296 A1 · Process for producing propylene block copolymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0301296 A1
- Document ID: US20110301296A1
- Status: Published application
- Kind: A1
- Application number: 13/210,444
- Filed: 2011-08-16
- Published: 2011-12-08
- Earliest claimed: 2006-12-15
- Assignees: Sumitomo Chemical Company, Limited
- Inventors: Yasuki FUJIWARA
- Web page: https://patentgrep.com/patent/US20110301296A1

## CPC

- C08F 297/08: polymerising mono-olefins
- C08F 297/083: {the monomers being ethylene or propylene}
- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A propylene block copolymer comprising 60 to 85% by weight of a propylene polymer component and 15 to 40% by weight of an ethylene-propylene copolymer component, and satisfying the following requirements (I) to (V): (I) the above propylene polymer component has a melting temperature of 160° C. or higher measured according to DSC; (II) the above ethylene-propylene copolymer component has an ethylene content of 40 to 60% by weight measured according to a 13C-NMR spectrum; (III) the above ethylene-propylene copolymer component has a crystallization peak between 90 to 105° C. in its DSC measurement, and the above crystallization peak is 2 to 10 J in its heat of crystallization, per 1 g of the above ethylene-propylene copolymer component; (IV) the above ethylene-propylene copolymer component has a glass transition temperature of −50° C. or lower measured according to DSC; and (V) the above ethylene-propylene copolymer component has an ethylene-propylene binding moiety, and the ethylene-propylene binding moiety has an intensity ratio of a racemic peak to a meso peak of 0.01 to 0.7 measured according to a 13C-NMR spectrum.

## Claims

### Claim 1

(canceled)

### Claim 2

A process for producing a propylene block copolymer comprising 60 to 85% by weight of a propylene polymer component and 15 to 40% by weight of an ethylene-propylene copolymer component, and satisfying the following requirements (I) to (V):
(I) the above propylene polymer component has a melting temperature of 160° or higher measured according to DSC;
(II) the above ethylene-propylene copolymer component has an ethylene content of 40 to 60% by weight measured according to a 13C-NMR spectrum;
(III) the above ethylene-propylene copolymer component has a crystallization peak between 90 to 105° C. in its DSC measurement, and the above crystallization peak is 2 to 10 J in its heat of crystallization, per 1 g of the above ethylene-propylene copolymer component;
(IV) the above ethylene-propylene copolymer component has a glass transition temperature of −50° C. or lower measured according to DSC; and
(V) the above ethylene-propylene copolymer component has an ethylene-propylene binding moiety, and the ethylene-propylene binding moiety has an intensity ratio of a racemic peak to a meso peak of 0.01 to 0.7 measured according to a 13C-NMR spectrum; the process comprising steps of:
(1) polymerizing propylene only, thereby forming a propylene homopolymer, or copolymerizing propylene with one or more olefins selected from the group consisting of ethylene and α-olefins having 4 to 18 carbon atoms, thereby forming a propylene copolymer;
(2) adding a halogen-containing organoaluminum compound and a cyclic organo-nitrogen compound to the reaction mixture of step (1); and
(3) copolymerizing propylene with ethylene in the presence of the reaction mixture of step (2).