# US 2011/0297959 A1 · Chamfered freestanding nitride semiconductor wafer and method of chamfering nitride semiconductor wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0297959 A1
- Document ID: US20110297959A1
- Status: Published application
- Kind: A1
- Application number: 13/212,017
- Filed: 2011-08-17
- Published: 2011-12-08
- Earliest claimed: 2003-04-02
- Assignees: Sumitomo Electric Industries, Ltd.
- Inventors: Masahiro NAKAYAMA; Masato Irikura
- Web page: https://patentgrep.com/patent/US20110297959A1

## CPC

- H10D 62/117: {Shapes of semiconductor bodies}
- B24B 9/065: {of thin, brittle parts, e.g. semiconductors, wafers}
- B24B 21/002: {for grinding edges or bevels}
- H10P 90/128: {by edge treatment, e.g. chamfering}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Technology of making freestanding gallium nitride (GaN) wafers has been matured at length. Gallium nitride is rigid but fragile. Chamfering of a periphery of a GaN wafer is difficult. At present edges are chamfered by a rotary whetstone of gross granules with weak pressure. Minimum roughness of the chamfered edges is still about Ra 10 μm to Ra 6 μm. The large edge roughness causes scratches, cracks, splits or breaks in transferring process or wafer process. A wafer of the present invention is bevelled by fixing the wafer to a chuck of a rotor, bringing an edge of the wafer into contact with an elastic whetting material having a soft matrix and granules implanted on the soft matrix, rotating the wafer and feeding the whetting material. Favorably, several times of chamfering edges by changing the whetting materials of smaller granules are given to the wafer. The chamfering can realize small roughness of Ra 10 nm and Ra 5 μm at edges of wafers.

## Claims

### Claim at position 1

1-20. (canceled)

### Claim 21

A nitride semiconductor wafer having an edge having roughness Ra between 0.01 μm and 0.1 μm.

### Claim 22 (depends on 21)

The nitride semiconductor wafer as claimed in claim 21, wherein the nitride semiconductor is gallium nitride (GaN).

### Claim 23 (depends on 21)

The nitride semiconductor wafer as claimed in claim 21, wherein the nitride semiconductor is aluminum nitride (AIN).

### Claim 24 (depends on 21)

The nitride semiconductor wafer as claimed in claim 21, wherein the nitride semiconductor is indium nitride (InN).