# US 2011/0297308 A1 · Method of making automotive body parts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0297308 A1
- Document ID: US20110297308A1
- Status: Published application
- Kind: A1
- Application number: 13/152,617
- Filed: 2011-06-03
- Published: 2011-12-08
- Earliest claimed: 2010-06-08
- Inventors: Stephen Paul Makin; Donald E. Panoz
- Web page: https://patentgrep.com/patent/US20110297308A1

## CPC

- B29C 70/04: comprising reinforcements only, e.g. self-reinforcing plastics
- B29C 70/44: using isostatic pressure, e.g. pressure difference-moulding, vacuum bag-moulding, autoclave-moulding or expanding rubber-moulding
- B29C 70/549: {Details of caul plates, e.g. materials or shape}
- B32B 3/12: characterised by a layer of regularly- arranged cells, e.g. a honeycomb structure
- B32B 5/024: {Woven fabric}
- B32B 5/08: the fibres or filaments of a layer being of different substances {, e.g. conjugate fibres, mixture of different fibres}
- B32B 27/38: comprising epoxy resins
- B60J 5/0481: {plastic}
- B32B 2260/02: Composition of the impregnated, bonded or embedded layer
- B32B 2260/046: Synthetic resin
- B32B 2307/50: having particular mechanical properties
- B32B 2307/558: Impact strength, toughness
- B32B 2605/003: Interior finishings
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B60J: WINDOWS, WINDSCREENS, NON-FIXED ROOFS, DOORS, OR SIMILAR DEVICES FOR VEHICLES; REMOVABLE EXTERNAL PROTECTIVE COVERINGS SPECIALLY ADAPTED FOR VEHICLES (fastening, suspending, closing, or opening of such devices E05)

## Abstract

An automotive body part, such as a body frame or side impact protection system, is prepared from a thermoplastic composite in a pressure vessel at pressures between about 1 and 6 bar and a temperature less than about 285° F.

## Claims

### Claim 1

A method of manufacturing a body part for an automotive vehicle having a defined shape which comprises:
(a) introducing into a mold having the defined shape of the body part at least one layer of a thermoplastic composite;
(b) enclosing the mold in a vacuum bag;
(c) inserting the vacuum bag into a pressure vessel;
(d) subjecting the pressure vessel to a pressure between from about 1 to about 6 bar and a temperature less than about 285° F. for a time sufficient to harden the thermoplastic composite, thereby forming the defined shape of the body part;
(e) decreasing the temperature to less than or equal to 120° F. and then reducing the pressure in the pressure vessel;
(f) removing the body part having the defined shape from the pressure vessel; and
(g) releasing the body part of defined shape from the mold.

### Claim 2 (depends on 1)

The method of claim 1, wherein the thermoplastic composite is a polypropylene composite.

### Claim 3 (depends on 1)

The method of claim 1, wherein the body part is a side impact protection system for an automotive vehicle.

### Claim 4 (depends on 1)

The method of claim 1, wherein at least one layer of a bonding film is further introduced into the mold in step (a) after introduction of the thermoplastic composite.

### Claim 5 (depends on 4)

The method of claim 4, wherein the bonding film is an epoxy resin.

### Claim 6 (depends on 5)

The method of claim 5, wherein the epoxy resin is impregnated with fibers.

### Claim 7 (depends on 4)

The method of claim 4, wherein at least one layer of substrate material is introduced into the mold after introduction of the bonding film.

### Claim 8 (depends on 7)

The method of claim 7, wherein a second bonding film is introduced into the mold after introduction of the at least one layer of substrate material.

### Claim 9 (depends on 8)

The method of claim 8, wherein a second polypropylene thermoplastic composite is introduced into the mold after introduction of the second bonding film.

### Claim 10 (depends on 9)

The method of claim 9, wherein a surface film is introduced into the mold after introduction of the second polypropylene thermoplastic composite.

### Claim 11 (depends on 1)

The method of claim 1, wherein the polypropylene thermoplastic composite comprises axially drawn tape fibers.

### Claim 12 (depends on 11)

The method of claim 11, wherein the polypropylene thermoplastic composite comprises a mat having a plurality of layers of axially drawn tape fibers.

### Claim 13 (depends on 12)

The method of claim 12, wherein the polypropylene thermoplastic composite further comprises embedded fiber elements in the mat.

### Claim 14 (depends on 1)

The method of claim 1, wherein the pressure vessel is subjected to a temperature between from about 280° to about 285° F.

### Claim 15 (depends on 14)

The method of claim 14, wherein the pressure vessel is subjected to a temperature between from about 280° to about 285° F. for a time between from about 10 minutes to about 2 hours.

### Claim 16 (depends on 1)

The method of claim 1, wherein steps (a) through (g) are repeated at least one time using a mold having a defined body shape which is different from the defined shape of the body part of step (a).

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
(i) introducing into an assembly mold each of the released body parts having different defined shapes;
(ii) enclosing the defined assembly mold in a vacuum bag;
(iii) introducing the defined assembly mold into a pressure vessel;
(iv) subjecting the pressure vessel to a pressure between from about 1 to about 6 bar and a temperature less than about 285° F. for a time sufficient to soften and then harden the thermoplastic composite, thereby forming an assembled body part having the defined shape of the defined assembly;
(v) decreasing the temperature in the pressure vessel to less than or equal to 120° F. and then reducing the pressure in the pressure vessel;
(vi) removing from the pressure vessel an assembled body part having the shape of the defined assembly mold; and
(g) releasing the assembled body part having the defined shape of the defined assembly mold from the mold.

### Claim 18 (depends on 1)

The method of claim 1, wherein prior to application of the vacuum in step (d), a thermo expanding intensifier is introduced into the bag.

### Claim 19 (depends on 18)

The method of claim 18, wherein the thermo expanding intensifier is a silicon mandrel plug, fiberglass or a ferrous material.

### Claim 20

A method of manufacturing a body part having a defined shape which comprises:
(a) introducing into a mold of a defined shape at least one layer of a polypropylene thermoplastic composite;
(b) enclosing the mold in a vacuum bag;
(c) inserting the vacuum bag into a pressure vessel;
(d) subjecting the pressure vessel to a pressure between from about 1 to about 6 bar and a temperature less than about 285° F., wherein the pressure is at least 1 bar when the temperature is 80° F., and maintaining the pressure and temperature in the pressure vessel for a time sufficient for the thermoplastic composite to harden and form a body part having the defined shape of the mold;
(e) decreasing the temperature to less than or equal to 120° F. and then reducing the pressure in the pressure vessel;
(f) removing the body part having the defined shape from the pressure vessel;
(g) releasing the body part of defined shape from the mold;
(h) optionally repeating steps (a) through (g) at least once using a mold having a defined shape which is different from the defined shape of the mold of step (a);
(i) introducing the released body parts of steps (f) and (h) into an assembly mold having a defined shape;
(j) enclosing the assembly mold in a vacuum bag;
(k) inserting the vacuum bag of step (j) into a pressure vessel;
(l) subjecting the pressure vessel to a pressure between from about 1 to about 6 bar and a temperature less than about 285° F. for a time sufficient to soften and then harden the thermoplastic composite, thereby forming an assembled body part having the defined shape of the defined assembly mold;
(m) decreasing the temperature in the pressure vessel to less than or equal to 120° F. and then reducing the pressure in the pressure vessel;
(n) removing an assembled body part having the defined shape of the defined assembly mold from the pressure vessel; and
(o) releasing the assembled body part having the defined shape of the defined assembly mold from the mold.

### Claim 21 (depends on 20)

The method of claim 20, wherein at least one layer of an epoxy resin material is further introduced into the mold in step (a).

### Claim 22 (depends on 21)

The method of claim 21, wherein the body part is a side impact protection system.

### Claim 23 (depends on 20)

The method of claim 20, wherein the polypropylene thermoplastic composite comprises axially drawn tape fibers.

### Claim 24 (depends on 23)

The method of claim 23, wherein the composite comprises a mat having a plurality of layers of axially drawn tape fibers.

### Claim 25 (depends on 24)

The method of claim 24, wherein the epoxy resin is embedded with fibers.

### Claim 26 (depends on 1)

The method of claim 1, wherein the body part is an automotive body part.

### Claim 27 (depends on 20)

The method of claim 20, wherein the body part is an automotive body part.