- Number: US 2011/0257425 A1
- Document ID: US20110257425A1
- Status: Published application
- Kind: A1
- Application number: 13/088,253
- Filed: 2011-04-15
- Published: 2011-10-20
- Earliest claimed: 2010-04-15
- Assignees: China Petroleum & Chemical Corporation; Shanghai Research Institute of Petrochemical Technology, Sinopec
- Inventors: Juntao Liu; Siqin Li; Lei Li; Linna Zhang
- Web page: https://patentgrep.com/patent/US20110257425A1

## CPC

- C07C 201/04: Preparation of esters of nitrous acid
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

The present invention relates to a process for producing C1-C4 alkyl nitrite, comprising loading a resin catalyst layer and/or a porous filler layer into a reactor, passing nitrogen oxide, oxygen and C1-C4 alkanol as raw materials through the resin catalyst layer and/or porous filler layer in a counter current, parallel current or cross current manner, reacting under the conditions including a reaction temperature of from 0 to 150° C., a reaction pressure of from −0.09 to 1.5 MPa, a molar ratio of C1-C4 alkanol/nitrogen oxide of 1-100:1, a molar ratio of nitrogen oxide/oxygen of 4-50:1, to obtain an effluent containing C1-C4 alkyl nitrite, wherein said nitrogen oxide is NO, or a mixed gas containing NO and one or more selected from N2O3 and NO2.

## Claims

### Claim 1

A process for producing C1-C4 alkyl nitrite, comprising loading a resin catalyst layer and/or a porous filler layer into a reactor, passing nitrogen oxide, oxygen and C1-C4 alkanol as raw materials through the resin catalyst layer and/or porous filler layer in a counter current, parallel current or cross current manner, reacting under the conditions including a reaction temperature of from 0 to 150° C., a reaction pressure of from −0.09 to 1.5 MPa, a molar ratio of C1-C4 alkanol/nitrogen oxide of 1-100:1, and a molar ratio of nitrogen oxide/oxygen of 4-50:1, to obtain an effluent containing C1-C4 alkyl nitrite, wherein said nitrogen oxide is NO, or a mixed gas containing NO and one or more selected from N2O3 and NO2.

### Claim 2 (depends on 1)

The process for producing C1-C4 alkyl nitrite according to claim 1, characterized in that the reactor is a rotating high-gravity reactor; and the porous filler layer is fixed onto the rotor of the rotating high-gravity reactor.

### Claim 3 (depends on 2)

The process for producing C1-C4 alkyl nitrite according to claim 2, characterized in that the resin catalyst is further fixed onto the rotor of the rotating high-gravity reactor.

### Claim 4 (depends on 1)

The process for producing C1-C4 alkyl nitrite according to claim 1, characterized in that the resin catalyst is loaded into the reactor.

### Claim 5 (depends on 1)

The process for producing C1-C4 alkyl nitrite according to claim 1, characterized in that the resin catalyst is an acidic ion exchange resin catalyst.

### Claim 6 (depends on 1)

The process for producing C1-C4 alkyl nitrite according to claim 1, characterized in that the molar number of NO in the nitrogen oxide is greater than that of NO2, if any, in the nitrogen oxide.

### Claim 7 (depends on 1)

The process for producing C1-C4 alkyl nitrite according to claim 1, characterized in that the reaction temperature ranges from 10 to 100° C.; the reaction pressure ranges from −0.05 to 1.0 MPa; the molar ratio of C1-C4 alkanol to nitrogen oxide is 1-50:1; and the molar ratio of nitrogen oxide to oxygen is 4-20:1.

### Claim 8 (depends on 7)

The process for producing C1-C4 alkyl nitrite according to claim 7, characterized in that the reaction temperature ranges from 10 to 60° C.; the reaction pressure ranges from −0.05 to 0.8 MPa; the molar ratio of C1-C4 alkanol to nitrogen oxide is 1-20:1; and the molar ratio of nitrogen oxide to oxygen is 4-10:1.

### Claim 9 (depends on 1)

The process for producing C1-C4 alkyl nitrite according to claim 1, characterized in that the rotor in the rotating high-gravity reactor has a rotating speed of from 100 to 5,000 rpm.

### Claim 10 (depends on 9)

The process for producing C1-C4 alkyl nitrite according to claim 9, characterized in that the rotor in the rotating high-gravity reactor has a rotating speed of from 300 to 3,000 rpm.

### Claim 11 (depends on 1)

The process for producing C1-C4 alkyl nitrite according to claim 1, characterized in that C1-C4 alkanol is selected from the group consisting of methanol, ethanol and n-propanol.

### Claim 12 (depends on 11)

The process for producing C1-C4 alkyl nitrite according to claim 11, characterized in that C1-C4 alkanol is methanol or ethanol.

### Claim 13 (depends on 1)

The process for producing C1-C4 alkyl nitrite according to claim 1, characterized in that the porous filler layer comprises an inert filler web, a porous web, a stent or a porous plate.