# US 2011/0257420 A1 · Catalyst with bimodal pore size distribution and the use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0257420 A1
- Document ID: US20110257420A1
- Status: Published application
- Kind: A1
- Application number: 13/167,359
- Filed: 2011-06-23
- Published: 2011-10-20
- Earliest claimed: 2006-09-29
- Assignees: SD Lizenzverwertungsgesellschaft mbH & Co. KG
- Inventors: Christian GUECKEL
- Web page: https://patentgrep.com/patent/US20110257420A1

## CPC

- B01J 35/69: bimodal
- B01J 23/688: {with manganese, technetium or rhenium}
- B01J 35/647: {2-50 nm}
- B01J 35/651: {50-500 nm}
- B01J 35/657: {larger than 1000 nm}
- C07D 301/10: with catalysts containing silver or gold
- C07D 303/04: containing only hydrogen and carbon atoms in addition to the ring oxygen atoms
- B01J 35/612: {less than 10 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)

## Abstract

The invention pertains to a catalyst useful for the epoxidation of an olefin. More particularly, the invention pertains to an improved catalyst useful for the epoxidation of ethylene to ethylene oxide. The catalyst has improved selectivity in the epoxidation process. The catalyst comprises a solid support having a surface, which has a first mode of pores which have a diameter ranging from about 0.01 μm to about 5 μm and having a differential pore volume peak in the range of from about 0.01 μm to about 5 μm. The surface then has a second mode of pores, different from the first mode of pores, which second mode of pores have a diameter ranging from about 1 μm to about 20 μm and have a differential pore volume peak in the range of from about 1 μm to about 20 μm. On the bimodal pore surface is a catalytically effective amount of silver or a silver-containing compound, a promoting amount of rhenium or a rhenium-containing compound, and a promoting amount of one or more alkali metals or alkali-metal-containing compounds.

## Claims

### Claim 1

A method for the oxidation of an olefin to an olefin oxide, the method comprising the vapor phase oxidation of an olefin with molecular oxygen in a fixed-bed tubular reactor in the presence of a catalyst for the epoxidation of an olefin to an olefin oxide, the catalyst comprising: (i) a support having a bimodal pore size distribution, with a first mode of pores having a mean diameter ranging from about 0.01 μm to about 5 μm, and a second mode of pores having a mean diameter ranging from about 5 μm to about 30 μm, (ii) a catalytically effective amount of silver, (iii) a promoting amount of rhenium, and (iv) a promoting amount of one or more alkali metals.

### Claim 2 (depends on 1)

The method of claim 1, wherein said olefin is ethylene and said olefin oxide is ethylene oxide.

### Claim 3 (depends on 1)

The method of claim 1, wherein said first mode of pores has a mean diameter ranging from about 0.1 μm to about 4 μm, and said second mode of pores has a mean diameter ranging from about 5 μm to about 20 μm.

### Claim 4 (depends on 1)

The method of claim 1, wherein said first mode of pores comprises at most 50% of a total pore volume and said second mode of pores comprises at least 50% of the total pore volume.

### Claim 5 (depends on 1)

The method of claim 1, wherein said first mode of pores comprises at most 40% of a total pore volume and said second mode of pores comprises at least 60% of the total pore volume.

### Claim 6 (depends on 1)

The method of claim 1, wherein said support is selected from alumina, charcoal, pumice, zirconia, titania, kieselguhr, fuller's earth, silicon carbide, silica, magnesia, clays, artificial zeolites, natural zeolites, ceramics, and combinations thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein said support comprises alumina.

### Claim 8 (depends on 1)

The method of claim 1, wherein said support comprises alumina having a surface area of less than about 1 m2/g.

### Claim 9 (depends on 1)

The method of claim 1, wherein said catalyst further comprises a promoting amount of one or more Group IIA metal-containing compound, one or more transition metal-containing compound, one or more sulfur-containing compound, one or more fluorine-containing compound, one or more phosphorus-containing compound, one or more boron-containing compound, or a combination thereof.

### Claim 10 (depends on 9)

The method of claim 9, wherein the Group IIA metal-containing compound is selected from beryllium, magnesium, calcium, strontium, barium, and combinations thereof.

### Claim 11 (depends on 9)

The method of claim 9, wherein the transition metal-containing compound is selected from an element selected from Groups IVA, VA, VIA, VIIA and VIIIA of the Periodic Table of the Elements, and combinations thereof.

### Claim 12 (depends on 9)

The method of claim 9, wherein the transition metal-containing compound is selected from molybdenum, tungsten, chromium, titanium, hafnium, zirconium, vanadium, thorium, tantalum, niobium, and combinations thereof.

### Claim 13 (depends on 9)

The method of claim 9, wherein the transition metal-containing compound is molybdenum, tungsten, or a combination thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein the catalyst further comprises a promoting amount of gallium, germanium, sulfur, phosphorus, boron, a halogen, or a combination thereof, on the surface of the support.

### Claim 15 (depends on 1)

The method of claim 1, wherein said alkali metal-containing compound is selected from lithium, sodium, potassium, rubidium, cesium, and combinations thereof.

### Claim 16 (depends on 1)

The method of claim 1, wherein said alkali metal-containing compound comprises cesium.

### Claim 17 (depends on 1)

The method of claim 1, wherein said rhenium is present in an amount of about 0.001 wt % to about 1 wt % based on the total weight of the catalyst.

### Claim 18 (depends on 1)

The method of claim 1, wherein the epoxidation process is conducted at a temperature of about 180° C. to about 330° C.

### Claim 19 (depends on 1)

The method of claim 1, wherein the epoxidation process is conducted at a temperature of about 200° C. to about 325° C.

### Claim 20 (depends on 1)

The method of claim 1, wherein the epoxidation process is conducted at a temperature of about 225° C. to about 270° C.