# US 2011/0256727 A1 · Method of forming semiconductor patterns

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0256727 A1
- Document ID: US20110256727A1
- Status: Published application
- Kind: A1
- Application number: 13/085,531
- Filed: 2011-04-13
- Published: 2011-10-20
- Earliest claimed: 2010-04-14
- Assignees: ASM Genitech Korea Ltd.
- Inventors: Julien Beynet; Hyung Sang Park; Naoki Inoue
- Web page: https://patentgrep.com/patent/US20110256727A1

## CPC

- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6689: {the compound being a silazane}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Semiconductor patterns are formed by performing trimming simultaneously with the process of depositing the spacer oxide. Alternatively, a first part of the trimming is performed in-situ, immediately before the spacer oxide deposition process in the same chamber in which the spacer oxide deposition is performed whereas a second part of the trimming is performed simultaneously with the process of depositing the spacer oxide. Thus, semiconductor patterns are formed reducing PR footing during PR trimming with direct plasma exposure.

## Claims

### Claim 1

A method of forming semiconductor patterns, the method comprising:
forming a photo resist template having a pattern of lines on a bottom layer, the pattern having a line width and a line spacing, the ratio of the line width to the line spacing being 1: A wherein 1≦A<3;
depositing a spacer oxide conformal over the photo resist template by a Plasma Enhanced Atomic Layer deposition process, using sequential and alternating pulses of a silicon precursor and an oxygen plasma, such that trimming of the photo resist template occurs and the ratio of the line width to the line spacing becomes 1:3 and the thickness of the deposited spacer oxide is about equal to the trimmed line width;
etching back the deposited spacer oxide such that spacer oxide films on upper and bottom surfaces of the pattern are removed, with spacer oxide films on side wall surfaces of the photo resist template remaining;
removing the photo resist template remaining between the spacer oxide films by selective etching; and
patterning the bottom layer by using the remaining spacer oxide films formed as mask.

### Claim 2 (depends on 1)

The method of claim 1, further comprising: trimming, prior to the step of depositing the spacer oxide, the photo resist pattern of lines such that the ratio of the line width to the line spacing becomes 1: B, wherein A<B<3 by exposing the photo resist pattern of lines to pulses of the oxygen plasma, in the same reaction chamber in which the spacer oxide deposition is performed.

### Claim 3 (depends on 2)

The method of claim 2, further comprising: a PR footing reduction step prior to the step of depositing the spacer oxide, in the same reaction chamber in which PR trimming step and the spacer oxide deposition step are performed, the PR footing reduction step comprising a direct plasma exposure step.

### Claim 4 (depends on 3)

The method of claim 3, wherein the PR footing reduction step is performed prior to the PR trimming step.

### Claim 5 (depends on 3)

The method of claim 3, wherein the PR footing reduction step is performed after the PR trimming step.

### Claim 6 (depends on 1)

The method of claim 1, wherein the plasma is a direct plasma.

### Claim 7 (depends on 1)

The method of claim 1, wherein the plasma is a remote plasma.

### Claim 8 (depends on 2)

The method of claim 2, wherein the plasma is a direct plasma.

### Claim 9 (depends on 2)

The method of claim 2, wherein the plasma is a remote plasma.

### Claim 10 (depends on 1)

The method of claim 1, wherein the silicon precursor is SiH2[N(C2H5)2]2.