# US 2011/0256668 A1 · Method of manufacturing semiconductor apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0256668 A1
- Document ID: US20110256668A1
- Status: Published application
- Kind: A1
- Application number: 13/084,603
- Filed: 2011-04-12
- Published: 2011-10-20
- Earliest claimed: 2010-04-14
- Assignees: Fuji Electric Co., Ltd.
- Inventors: Yuichi URANO
- Web page: https://patentgrep.com/patent/US20110256668A1

## CPC

- H10P 72/7402: {Wafer tapes, e.g. grinding or dicing support tapes}
- H10P 72/7436: {used to support a device or a wafer when forming electrical connections thereto}
- H10P 72/7442: {Separation by peeling}
- H10W 72/011: {Apparatus therefor}
- H10W 72/01935: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01971: {Cleaning, e.g. oxide removal}
- H10W 72/0198: {batch processes}
- H10W 72/352: {comprising metals or metalloids, e.g. solders}
- H10W 72/381: {Auxiliary members}
- H10W 72/5522: {comprising gold [Au]}
- H10W 72/5524: {comprising aluminium [Al]}
- H10W 72/59: Bond pads specially adapted therefor
- H10W 72/865: {Die-attach connectors and bond wires}
- H10W 72/884: {Die-attach connectors and bond wires}
- H10W 72/926: {Multiple bond pads having different sizes}
- H10W 72/932: {Plan-view shape, i.e. in top view}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/944: {Dispositions of multiple bond pads}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 74/00: Encapsulations, e.g. protective coatings
- H10W 74/111: {the semiconductor body being completely enclosed}
- H10W 90/736: {between a chip and a stacked lead frame, conducting package substrate or heat sink}
- H10W 90/756: {between a chip and a stacked lead frame, conducting package substrate or heat sink}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor apparatus includes forming back surface electrode 4 on back surface of semiconductor wafer 20, that bends convexly toward the front surface side due to back surface electrode 4 being formed; treating the back surface with a plasma for removing the deposits on the back surface; sticking removable adhesive tape 23 to the back surface along the warp thereof for maintaining the bending state of semiconductor wafer 20 after the step of sticking; electrolessly plating to form film 26 on the front surface of semiconductor wafer 20; peeling off removable adhesive tape 23; cutting out semiconductor chips; and mounting the semiconductor chip by bonding with a solder for manufacturing a semiconductor apparatus. The manufacturing method prevents external appearance anomalies from occurring on the back surface electrode, improves the reliability, and allows manufacture of the semiconductor apparatuses with a high throughput of non-defective products.

## Claims

### Claim 1

A method of manufacturing a semiconductor apparatus, the method comprising:
forming a back surface electrode on a back surface of a semiconductor wafer, causing the semiconductor wafer to bend;
adhering a first film to the back surface of the semiconductor wafer which is in a bent state as a result of the back surface electrode being formed thereon, in order to maintain the bent state of the semiconductor wafer; and
plating a second film on a front surface of the semiconductor wafer while it is in the bent state, wherein the second film is a front surface electrode, the step of plating being conducted after the step of adhering the first film.

### Claim 2

A method of manufacturing a semiconductor apparatus, the method comprising:
forming a back surface electrode on a back surface of a semiconductor wafer;
adhering a first film to the back surface of the semiconductor wafer, causing the semiconductor wafer to bend convexly toward a front surface side of the semiconductor wafer, the step of adhering being conducted after the step of forming the back surface electrode; and
plating a second film on a front surface of the semiconductor wafer while it is in the bent state, wherein the second film is a front surface electrode.

### Claim 3

A method of manufacturing a semiconductor apparatus, the method comprising:
adhering a first film to a back surface of a semiconductor wafer causing the semiconductor wafer to bend convexly toward a front surface side of the semiconductor wafer due to the back surface electrode being formed on the back surface of the semiconductor wafer and maintaining the bent state of the semiconductor wafer; and
plating a second film on a front surface of the semiconductor wafer while it is in the bent state, the second film being a front surface electrode, the plating being conducted after the adhering.

### Claim 4 (depends on 1)

The method according to claim 1, the method further comprising:
cutting the semiconductor wafer into a plurality of semiconductor chips, the cutting being conducted after the plating.

### Claim 5 (depends on 1)

The method according to claim 1, the method further comprising:
peeling the first film off the semiconductor wafer, the peeling being conducted after the plating and before the cutting.

### Claim 6 (depends on 1)

The method according to claim 1, the method further comprising:
bonding a metal body to each of a front surface side and a back surface side of the semiconductor chip cut out through the step of cutting, the metal bodies functioning as radiators and being connected electrically to the front surface electrode and the back surface electrode, respectively; and
sealing at least the semiconductor chip entirely.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the front surface of the semiconductor wafer is absorbed during adhering such that it flattens the semiconductor wafer, and the first film is stuck to the back surface of the flattened semiconductor wafer.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the first film is adhering such that it covers at least the back surface electrode on the semiconductor wafer.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first film is adhering such that it covers the back surface of the semiconductor wafer entirely.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the first film is adhering such that the first film extends outwardly from a back surface edge of the semiconductor wafer.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the first film extends outwardly from the back surface edge of the semiconductor wafer for 1 mm or less.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the first film is stuck in the adhering such that it is pulled outwardly such that a tensile force is exerted on it.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the first film is heated at 40° C. or higher and 60° C. or lower during adhering.

### Claim 14 (depends on 1)

The method according to claim 1, wherein a rigidity of the film or the tape is lower than a rigidity of the semiconductor wafer.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the first film is 40 μm or more and 80 μm or less in thickness.

### Claim 16 (depends on 1)

The method according to claim 1, wherein the first film contains one of the polymers selected from the group consisting of (polyimide, polyphenylene sulfide, polyethylene terephthalate, and aromatic polyamide) as one of main components.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the first film exhibits an adhesive strength which is lowered by heat or an ultraviolet ray.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the first film comprises an adhesive layer which contacts the back surface of the semiconductor wafer, and the adhesive layer is hardened by heat or by an ultraviolet ray such that its adhesive strength is lowered.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the first film comprises an adhesive layer which contacts the back surface of the semiconductor wafer, and the adhesive layer comprises a polymer made mainly from an acrylate as a main component.

### Claim 20 (depends on 17)

The method according to claim 17, wherein the first film comprises an adhesive layer in contact with the back surface of the semiconductor wafer, which decreases in adhesive strength and generates vapor when heated or exposed to ultraviolet light.

### Claim 21 (depends on 1)

The method according to claim 1, wherein the back surface electrode comprises a laminate film comprising a gold electrode layer laminated as an outermost layer of the laminate film.

### Claim 22 (depends on 1)

The method according to claim 1, wherein the second film is formed by an electroless plating method.

### Claim 23 (depends on 1)

The method according to claim 1, wherein the second film comprises a laminate film comprising a first plate layer made from nickel and a second plate layer on the first plate layer, the second plate layer being made from gold.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the first plate layer is plated in an electroless plating bath kept at 75° C. or higher and 85° C. or lower.

### Claim 25 (depends on 23)

The method according to claim 23, wherein the second plate layer is plated in an electroless plating bath kept at 70° C. or higher and 80° C. or lower.

### Claim 26 (depends on 23)

The method according to claim 23, wherein the first plate layer comprises an alloy made from nickel and phosphorus and a phosphorus concentration in the first plate layer is 2 wt % or higher and 8 wt % or lower.

### Claim 27 (depends on 23)

The method according to claim 23, wherein the plate film is 3 μm or more and 6 μm or less in thickness.

### Claim 28 (depends on 1)

The method according to claim 1, wherein the method further comprises forming an electrode containing aluminum as a main component on the front surface of the semiconductor wafer before forming the back surface electrode on the back surface of the semiconductor wafer, and the second film is formed when plating on the electrode containing aluminum as the main component thereof.

### Claim 29 (depends on 1)

The method according to claim 1, wherein the method further comprises thinning the semiconductor wafer from the back surface side before forming the back surface electrode on the back surface of the semiconductor wafer, and the back surface electrode is formed on the back surface of the thinned semiconductor wafer.

### Claim 30 (depends on 29)

The method according to claim 29, wherein the semiconductor wafer is thinned in the step of thinning to be 80 μm or more and 140 μm or less in thickness.

### Claim 31 (depends on 1)

The method according to claim 1, the method further comprising:
plasma treating the back surface of the semiconductor wafer with a plasma for removing deposits sticking to the back surface of the semiconductor wafer, the plasma treating being conducted after forming the back surface electrode and before the adhering.

### Claim 32 (depends on 31)

The method according to claim 31, wherein the front surface and the back surface of the semiconductor wafer are treated with a plasma simultaneously in the step of plasma treating for removing deposits sticking to the front surface and the back surface of the semiconductor wafer simultaneously.

### Claim 33 (depends on 31)

The method according to claim 31, wherein oxygen is used as a raw material in the step of plasma treating.

### Claim 34 (depends on 31)

The method according to claim 31, wherein a capacitively coupled plasma generation mechanism is used in the plasma treating.

### Claim 35 (depends on 31)

The method according to claim 31, wherein a batch-type plasma treating apparatus that treats a plurality of the semiconductor wafers collectively is used in the plasma treating.

### Claim 36 (depends on 35)

The method according to claim 35, wherein a plasma treating apparatus that treats the front surface and the back surface of the semiconductor wafer simultaneously is used in the step of plasma treating.