# US 2011/0255068 A1 · EUV mirror module

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0255068 A1
- Document ID: US20110255068A1
- Status: Published application
- Kind: A1
- Application number: 12/799,016
- Filed: 2010-04-16
- Published: 2011-10-20
- Earliest claimed: 2010-04-16
- Assignees: Media Lario S.R.L.
- Inventors: Jacques Kools
- Web page: https://patentgrep.com/patent/US20110255068A1

## CPC

- G02B 7/1815: {with cooling or heating systems (cooling arrangements for laser mirrors H01S3/0401)}
- G02B 5/0891: {Ultraviolet [UV] mirrors (apparatus for microlithography exposure G03F7/70; X-ray multilayer structures G21K1/06)}
- G03F 7/7015: {Details of optical elements}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

An EUV mirror module is disclosed that comprises a substrate with a curved upper surface and a curved electroformed mirror. A self-adjusting bonding material is disposed between the substrate and the electroformed mirror. The bonding material is flowable at a melting temperature and self-adjusts to conformally fill the region between substrate to the electroformed mirror and bond the substrate and the electroformed mirror. The substrate may have at least one cooling channel for cooling the mirror module.

## Claims

### Claim 1

An extreme ultraviolet (EUV) mirror module, comprising:
a substrate having a body with a curved upper surface;
a electroformed mirror having front and rear curved surfaces; and
a self-adjusting bonding material disposed between the substrate upper surface and the electroformed mirror rear surface, the bonding material being flowable at a melting temperature and serving to bond the substrate to the electroformed mirror at a temperature below the melting temperature.

### Claim 2 (depends on 1)

The EUV mirror module of claim 1, wherein the substrate and the electroformed mirror are formed from the same material.

### Claim 3 (depends on 2)

The EUV mirror module of claim 2, wherein:
the substrate is formed from a substrate material selected from the group of substrate materials comprising: nickel, nickel alloy, copper, copper alloy, silicon, silicon carbide and ZERODUR; and
the electroformed mirror is formed from a mirror material selected from the group of mirror materials comprising: nickel, nickel alloy, copper and copper alloy.

### Claim 4 (depends on 1)

The EUV mirror module of claim 1, wherein the bonding material comprises at least one of indium, gallium, tin and lead.

### Claim 5 (depends on 1)

The EUV mirror module of claim 1, wherein the melting temperature of the bonding material is between 140° C. and 250° C.

### Claim 6 (depends on 1)

The EUV mirror module of claim 1, wherein the bonding material has a thickness of between 10 microns and 1000 microns.

### Claim 7 (depends on 1)

The EUV mirror module of claim 1, wherein the substrate curved surface is a machined surface.

### Claim 8 (depends on 1)

The EUV mirror module of claim 1, wherein the substrate has a thickness of between 5 cm and 10 cm.

### Claim 9 (depends on 8)

The EUV mirror module of claim 8, wherein the electroformed mirror has a thickness between 1 mm and 2 mm.

### Claim 10 (depends on 1)

The EUV mirror module of claim 1, wherein the substrate includes at least one cooling channel.

### Claim 11 (depends on 10)

The EUV mirror module of claim 10, wherein the substrate includes radially arranged cooling channels.

### Claim 12 (depends on 10)

The EUV mirror module of claim 10, wherein the at least one cooling channel is located a distance D1 from the substrate upper surface, wherein distance D1 is in the range from 5 to 20 mm.

### Claim 13 (depends on 1)

An extreme ultraviolet (EUV) lithography system for illuminating a reflective reticle, comprising:
a source of EUV radiation;
an EUV collector system that includes the EUV mirror module of claim 1, wherein the EUV collector system is configured to receive the EUV radiation and form collected EUV radiation; and
an illuminator configured to receive the collected EUV radiation and form condensed EUV radiation for illuminating the reflective reticle.

### Claim 14 (depends on 13)

The EUV lithography system of claim 13 for forming a patterned image on a photosensitive semiconductor wafer, further comprising:
a projection optical system arranged downstream of the reflective reticle and configured to receive reflected EUV radiation from the reflective reticle and form therefrom the patterned image on the photosensitive semiconductor wafer.

### Claim 15

A method of forming an extreme ultraviolet (EUV) mirror module, comprising:
providing a substrate having a body with a curved upper surface;
providing a electroformed mirror having front and rear curved surfaces;
disposing a self-adjusting bonding material between the substrate upper surface and the electroformed mirror rear surface, the bonding material having a melting point;
heating the bonding material to its melting point, thereby causing the bonding material to flow between the substrate upper surface and the electroformed mirror rear surface; and
cooling the bonding material to below its melting point, thereby forming a thermally conductive bond between the electroformed mirror and the substrate.

### Claim 16 (depends on 15)

The method of claim 15, wherein the bonding material includes at least one of indium, gallium, tin and lead.

### Claim 17 (depends on 15)

The method of claim 15, wherein the melting temperature is between 140° C. and 250° C.

### Claim 18 (depends on 15)

The method of claim 15, further comprising forming at least one cooling channel in the substrate body and flowing a cooling fluid through the at least one cooling channel.

### Claim 19 (depends on 18)

The method of claim 18, further comprising forming a plurality of radial cooling lines in the substrate body.

### Claim 20 (depends on 15)

The method of claim 15, further comprising forming the electroformed mirror and the substrate from the same material.