# US 2011/0254438 A1 · Arc tube for discharge bulb

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0254438 A1
- Document ID: US20110254438A1
- Status: Published application
- Kind: A1
- Application number: 13/085,548
- Filed: 2011-04-13
- Published: 2011-10-20
- Earliest claimed: 2010-04-15
- Assignees: Koito Manufacturing Co., Ltd.
- Inventors: Terutoshi SAKO; Yuichiro FUJINO; Takuya SERITA
- Web page: https://patentgrep.com/patent/US20110254438A1

## CPC

- H01J 61/368: {Pinched seals or analogous seals}
- H01J 9/326: {making pinched-stem or analogous seals}
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

An arc tube for a discharge bulb, comprising a sealed glass bulb in which luminous materials are sealed; a plurality of pinch-sealed portions made of quartz glass and formed at both end portions of the sealed glass bulb; a plurality of molybdenum foils each pinch sealed in the corresponding pinch-sealed portion; a pair of electrode rods provided in the sealed glass bulb so as to face each other, wherein each of electrode rods extends from the sealed glass bulb to the corresponding pinch-sealed portion and is connected to one end of the corresponding molybdenum foil; and a plurality of lead wires each connected to the other end of the corresponding molybdenum foil, wherein the molybdenum foils comprise a plurality of closed cavities therein.

## Claims

### Claim 1

An arc tube for a discharge bulb, comprising
a sealed glass bulb in which luminous materials are sealed;
a plurality of pinch-sealed portions made of quartz glass and formed at both end portions of the sealed glass bulb;
a plurality of molybdenum foils each pinch sealed in the corresponding pinch-sealed portion;
a pair of electrode rods provided in the sealed glass bulb so as to face each other, wherein each of electrode rods extends from the sealed glass bulb to the corresponding pinch-sealed portion and is connected to one end of the corresponding molybdenum foil; and
a plurality of lead wires each connected to the other end of the corresponding molybdenum foil,
wherein the molybdenum foils comprise a plurality of closed cavities therein.

### Claim 2 (depends on 1)

The arc tube for of claim 1, wherein an average grain size of crystal grains of the molybdenum foil is in the range of about 3 to 5 μm.

### Claim 3 (depends on 1)

The arc tube according to claim 1, wherein the molybdenum foils are subjected to any one treatment of an oxidation/reduction treatment, a vacuum heat treatment, and a hydrogen treatment, prior to being pinch sealed so that an average grain size of crystal grains of the molybdenum foil is in the range of about 1 to 1.5 μm.

### Claim 4 (depends on 1)

The arc tube according to claim 1, wherein the molybdenum foil is doped with 0.5% yttria (Y2O3).

### Claim 5 (depends on 1)

The arc tube according to claim 1, wherein the pinched-sealed portions are formed at a temperature equal to or greater than 2200° C. and less than or equal to 2300° C.