# US 2011/0254119 A1 · Semiconductor Device and Method of Manufacturing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0254119 A1
- Document ID: US20110254119A1
- Status: Published application
- Kind: A1
- Application number: 13/116,880
- Filed: 2011-05-26
- Published: 2011-10-20
- Earliest claimed: 2008-09-22
- Assignees: Hynix Semiconductor Inc.
- Inventors: Ji H. Seo
- Web page: https://patentgrep.com/patent/US20110254119A1

## CPC

- H10W 10/13: formed using local oxidation of silicon [LOCOS], e.g. sealed interface localised oxidation [SILO] or side-wall mask isolation [SWAMI]
- H10B 41/30: characterised by the memory core region
- H10W 10/0125: {comprising introducing electrical impurities in local oxidation regions, e.g. to alter LOCOS oxide growth characteristics}
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P 30/222: {characterised by the angle between the ion beam and the crystal planes or the main crystal surface (characterised by the angle between the ion beam and the mask H10P30/221)}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing semiconductor devices includes forming a tunnel insulating layer, a conductive layer for a floating gate, and a hard mask layer on a semiconductor substrate, forming a first trench in the semiconductor substrate by partially etching the hard mask layer, the conductive layer for the floating gate, the tunnel insulating layer, and the semiconductor substrate, forming a first ion implantation region having a first impurity concentration into the semiconductor substrate of inner walls of the first trench by performing a first ion implantation process, forming a second trench extending from the first trench by etching the semiconductor substrate of a bottom of the first trench, and forming a second ion implantation region having a second impurity concentration lower than the first impurity concentration into the semiconductor substrate of inner walls of the second trench by performing a second ion implantation process, wherein a depth of the first trench is shallower than that of a junction region.

## Claims

### Claim 1

A method of manufacturing semiconductor devices, comprising:
forming a tunnel insulating layer, a conductive layer for a floating gate, and a hard mask layer over a semiconductor substrate;
forming a first trench in the semiconductor substrate by partially etching the hard mask layer, the conductive layer for the floating gate, the tunnel insulating layer, and the semiconductor substrate;
forming a first ion implantation region having a first impurity concentration into the semiconductor substrate of inner walls of the first trench by performing a first ion implantation process;
forming a second trench extending from the first trench by etching the semiconductor substrate of a bottom of the first trench; and
forming a second ion implantation region having a second impurity concentration lower than the first impurity concentration into the semiconductor substrate of inner walls of the second trench by performing a second ion implantation process,
wherein a depth of the first trench is shallower than that of a junction region.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
forming a liner insulating layer over the entire structure including the first and the second trenches after the second ion implantation process;
forming an insulating layer over the liner insulating layer by filling the first and the second trenches; and
removing the hard mask film.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first ion implantation process is performed using boron or BF2, and the second ion implantation process is performed using boron.

### Claim 4 (depends on 1)

The method of claim 1, wherein a ion implantation energy of the second ion implantation process is higher than that of the first ion implantation process.

### Claim 5 (depends on 1)

The method of claim 1, wherein the second ion implantation process is performed using an incident angle which is vertical to the semiconductor substrate.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
forming the junction region by performing a source drain ion implantation process after exposing an active region of the semiconductor substrate by etching the conductive layer for the floating gate, tunnel insulating layer in a direction of a word line.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second ion implantation region is further formed in the semiconductor substrate of a bottom of the second trench during the second implantation process.

### Claim 8

A method of manufacturing semiconductor devices, comprising:
forming a tunnel insulating layer and a conductive layer for a floating gate over a semiconductor substrate;
forming a first trench in the semiconductor substrate by partially etching the conductive layer for the floating gate, the tunnel insulating layer and the semiconductor substrate;
forming a first ion implantation region in the semiconductor substrate of inner walls of the first trench by performing a first ion implantation process;
forming a second trench extending from the first trench by etching the semiconductor substrate of a bottom of the first trench;
forming a second ion implantation region in the semiconductor substrate of inner walls of the second trench by performing a second ion implantation process;
forming an isolation structure by filling the first and the second trench with an insulating layer;
exposing an active region of the semiconductor substrate by etching the conductive layer for the floating gate and the tunnel insulating layer in a direction of a word line; and
forming a junction region in the semiconductor substrate of the exposed active region by performing a third ion implantation process,
wherein a depth of the first trench is shallower than the junction region.

### Claim 9 (depends on 8)

The method of claim 8, wherein the first ion implantation process is performed using boron or BF2, and the second ion implantation process is performed using boron.

### Claim 10 (depends on 8)

The method of claim 8, wherein the second ion implantation region is further formed in the semiconductor substrate of a bottom of the second trench during the second ion implantation process.

### Claim 11 (depends on 8)

The method of claim 8, wherein a ion implantation energy of the second ion implantation process is higher than that of the first ion implantation process.

### Claim 12 (depends on 8)

The method of claim 8, wherein the second ion implantation process is performed using an incident angle which is vertical to the semiconductor substrate.

### Claim 13

A semiconductor device, comprising:
an isolation structure having a first and a second trench formed in a semiconductor substrate; a first ion implantation region formed in the semiconductor substrate of inner walls of the first trench having a first impurity concentration; and
a second ion implantation region formed in the semiconductor substrate of inner walls of the second trench having a second impurity concentration which is lower than the first impurity concentration,
wherein a depth of the first trench is shallower than that of a junction region.

### Claim 14 (depends on 13)

The device of claim 13, wherein the first trench is the upper part of the isolation structure and the second trench is lower part of the isolation structure which is extending from the first trench.

### Claim 15 (depends on 13)

The device of claim 13, wherein the first ion implantation region maintains the ion concentration of an edge of an active region of the semiconductor substrate at a predetermined concentration or higher.

### Claim 16 (depends on 13)

The device of claim 13, wherein the second ion implantation region prevents the leakage current for punch between the isolation structures.

### Claim 17 (depends on 13)

The device of claim 13, wherein the second ion implantation region is further formed in the semiconductor substrate of a bottom of the trench.