# US 2011/0253681 A1 · Method of controlling an indentation depth of an electrode into a metal substrate during welding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0253681 A1
- Document ID: US20110253681A1
- Status: Published application
- Kind: A1
- Application number: 13/060,070
- Filed: 2010-04-07
- Published: 2011-10-20
- Earliest claimed: 2010-04-07
- Assignees: GM Global Technology Operations LLC
- Inventors: Pei-Chung Wang; Daniel C. Hutchinson
- Web page: https://patentgrep.com/patent/US20110253681A1

## CPC

- B23K 11/115: {by means of two electrodes placed opposite one another on both sides of the welded parts}
- B23K 11/253: {the measured parameter being a displacement or a position}
- B23K 11/255: {the measured parameter being a force (B23K11/253 takes precedence)}
- B23K 11/257: {the measured parameter being an electrical current}
- B23K 2101/18: Sheet panels
- B23K 2103/04: Steel {or steel} alloys
- B23K 2103/10: Aluminium or alloys thereof
- B23K 2103/20: Ferrous alloys and aluminium or alloys thereof
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method of controlling an indentation depth of an electrode into a metal substrate during formation of a weld includes selecting a weld force, current, duration, minimum indentation depth, and maximum indentation depth, contacting the substrate with the electrode to apply the force to the substrate, supplying the current to the electrode to initiate formation of the weld according to a first condition in which the depth is less than the minimum, a second condition in which the depth is greater than or equal to the minimum and less than or equal to the maximum, and a third condition in which the depth is greater than the maximum, and comparing the depth, minimum, and maximum. For the first condition, duration is changed. For the second condition, each of the force, current, and duration is maintained until the weld is substantially formed. For the third condition, current ceases to be supplied.

## Claims

### Claim 1

A method of controlling an indentation depth of an electrode into a first metal substrate during formation of a weld between the first metal substrate and a second metal substrate, the method comprising:
selecting each of a weld force, a weld current, a weld duration, a minimum indentation depth of the electrode into the first metal substrate, and a maximum indentation depth of the electrode into the first metal substrate;
after selecting, contacting the first metal substrate with the electrode to thereby apply the weld force to the first metal substrate, wherein the electrode has a distal end having a shape defined by a radius of greater than or equal to about 20 mm;
after contacting, supplying the weld current to the distal end of the electrode to thereby initiate formation of the weld according to at least one of a first condition in which the indentation depth is less than the minimum indentation depth, a second condition in which the indentation depth is greater than or equal to the minimum indentation depth and less than or equal to the maximum indentation depth, and a third condition in which the indentation depth is greater than the maximum indentation depth;
comparing the indentation depth to each of the minimum indentation depth and the maximum indentation depth to determine that formation of the weld is continuing according to one of the first condition, the second condition, and the third condition;
if it is determined that the first condition exists, changing the weld duration until the indentation depth is greater than or equal to the minimum indentation depth;
if it is determined that the second condition exists, maintaining each of the weld force, the weld current, and the weld duration until the weld is substantially formed; and
if it is determined that the third condition exists, ceasing to supply the weld current to the distal end of the electrode until the weld is substantially formed.

### Claim 2 (depends on 1)

The method of claim 1, further including selecting each of a second weld force that is less than the weld force, a second weld current that is less than the weld current, and a second weld duration that is less than the weld duration.

### Claim 3 (depends on 2)

The method of claim 2, wherein said contacting is further defined as disposing the first metal substrate adjacent and in contact with the electrode to thereby apply the second weld force to the first metal substrate.

### Claim 4 (depends on 3)

The method of claim 3, further including, after disposing to thereby apply the second weld force, supplying the second weld current to the distal end of the electrode for the second weld duration to thereby substantially form the weld so that the indentation depth is greater than or equal to the minimum indentation depth and less than or equal to the maximum indentation depth.

### Claim 5 (depends on 2)

The method of claim 2, further including selecting a third weld force that is less than the second weld force.

### Claim 6 (depends on 5)

The method of claim 5, wherein said contacting is further defined as disposing the first metal substrate adjacent and in contact with the electrode to thereby apply the third weld force to the first metal substrate without supplying each of the weld current and the second weld current to the electrode.

### Claim 7 (depends on 1)

The method of claim 1, wherein the distal end has a shape defined by a radius of from about 20 mm to about 80 mm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the distal end has a shape defined by a radius of about 50 mm.

### Claim 9 (depends on 1)

The method of claim 1, wherein the maximum indentation depth is less than or equal to about 0.25 mm.

### Claim 10 (depends on 1)