# US 2011/0253524 A1 · Aluminum-scandium alloy film applied to vehicle lamps and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0253524 A1
- Document ID: US20110253524A1
- Status: Published application
- Kind: A1
- Application number: 13/169,376
- Filed: 2011-06-27
- Published: 2011-10-20
- Earliest claimed: 2009-05-11
- Inventors: Jing-Chie Lin; Hsueh-Lung Liao; Jian-Jhong Shen; Sheng-Long Lee
- Web page: https://patentgrep.com/patent/US20110253524A1

## CPC

- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- B32B 15/016: {all layers being formed of aluminium or aluminium alloys}
- C03C 17/09: by deposition from the vapour phase
- C22C 21/00: Alloys based on aluminium
- C23C 14/14: Metallic material, boron or silicon
- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- C23C 26/00: Coating not provided for in groups C23C2/00 - C23C24/00
- C03C 2217/252: Al
- C03C 2217/27: Mixtures of metals, alloys
- Y10T 428/12764: Next to Al-base component
- Y10T 428/31678: Of metal
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An aluminum-scandium (Al—Sc) alloy film applied to vehicle lamps and a manufacturing method thereof are revealed. The Al—Sc alloy film contains a trace of scandium so that both temperature for grain refinement and temperature for recrystallization of the film are increased. This results in a fine and smooth surface of the Al—Sc alloy film and the Al—Sc alloy film has better optical reflectivity. Moreover, the Al—Sc alloy film has high recrystallization temperature and high adhesion strength. After high temperature annealing treatment, the Al—Sc alloy film still has higher corrosion resistance.

## Claims

### Claim 1

A manufacturing method of a Al—Sc alloy film applied to vehicle lamps comprising the steps of:
setting an Al—Sc alloy target and a substrate into a chamber,
pumping the air out of the cavity so as to create a vacuum in the chamber, and
coating an Al—Sc alloy layer on the substrate by introducing an argon gas into the cavity and controlling DC (direct current) power in a planar magnetron.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the substrate is made from plastic or aluminum.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the substrate is made from glass.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the Al—Sc alloy target is formed by melting and blending of pure aluminum and aluminum scandium alloy.

### Claim 5 (depends on 4)

The method as claimed in claim 4, wherein the aluminum scandium alloy contains 0.1% to 1.7% by weight of scandium.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein vacuum pressure in the chamber ranges from 1×10−5 torr to 9×10−5 torr.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the gas is argon.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein pressure of the argon gas introduced ranges from 1×10−3 torr to 3×10−3 torr.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the DC power in the planar magnetron ranges from 90 KW to 100 KW.