# US 2011/0253219 A1 · Photoelectronically active, chalcogen-based thin film structures incorporating tie layers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0253219 A1
- Document ID: US20110253219A1
- Status: Published application
- Kind: A1
- Application number: 13/047,139
- Filed: 2011-03-14
- Published: 2011-10-20
- Earliest claimed: 2010-03-17
- Assignees: Dow Global Technologies LLC
- Inventors: Jennifer E. Gerbi
- Web page: https://patentgrep.com/patent/US20110253219A1

## CPC

- H10F 10/167: comprising Group I-III-VI materials, e.g. CdS/CuInSe2 [CIS] heterojunction photovoltaic cells
- C23C 14/0623: {Sulfides, selenides or tellurides}
- C23C 14/3464: {using more than one target (C23C14/56 takes precedence)}
- C23C 14/5866: {Treatment with sulfur, selenium or tellurium}
- H10P 14/203: {using transformation of metal, e.g. oxidation or nitridation}
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/3436: {being chalcogenide semiconductor materials not being oxides, e.g. ternary compounds}
- Y02E 10/541: CuInSe2 material PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides improved chalcogen-containing, photovoltaic structures as well as related compositions, photovoltaic devices incorporating these structures, methods of making these structures and devices, and methods of using these structures and devices. According to principles of the present invention, the adhesion of PACB compositions is improved through the use of chalcogen-containing tie layers.

## Claims

### Claim 1

A method of making a chalcogen-containing photoabsorbing structure, comprising the steps of:
(a) forming a first photoactive film comprising at least Cu, In, and at least one chalcogen; and
(b) forming a second, photoactive film or precursor thereof directly or indirectly on the first film, said film comprising at least Cu and In; and
(c) subjecting at least the first film to an annealing and/or chalcogenization treatments under conditions effective to form a crystalline PACB composition, wherein the subjecting step occurs before, during, and/or after formation of the second photoactive film or precursor thereof.

### Claim 2

A method of making a chalcogen-containing photoabsorbing structure, comprising the steps of:
(a) forming a first photoactive film or a precursor thereof comprising at least Cu, In, and at least one chalcogen, wherein at least a portion of said forming occurs at a temperature of less than about 350° C.; and
(b) forming a second photoactive film or precursor thereof directly or indirectly on the first film, wherein the second film comprises at least Cu and In; and
(c) subjecting at least one of the first and second films and/or precursors thereof to an annealing and/or chalcogenization treatment under conditions effective to convert at least one of the first and second films to a crystalline PACB composition.

### Claim 3 (depends on 2)

The method of claim 2, wherein the first film as deposited has a thickness in the range from about 5 nm to about 200 nm.

### Claim 4 (depends on 2)

The method of claim 2, wherein the first film as deposited has a thickness in the range from about 10 nm to about 50 nm.

### Claim 5 (depends on 2)

The method of claim 2, wherein the first film as deposited further comprises at least one of Ga and Al.

### Claim 6 (depends on 5)

The method of claim 5, wherein the atomic ratio of (In+Ga+Al) to the amount of copper in the first film as deposited is greater than 1.

### Claim 7 (depends on 2)

The method of claim 2, wherein the first film as deposited includes from about 60 to about 100 percent of the stoichiometric amount of chalcogen(s) relative to (Cu+In+Ga+Al) in the first film as deposited.

### Claim 8 (depends on 2)

The method of claim 2, wherein at least a majority of the first film is deposited at one or more temperatures below about 350° C.

### Claim 9 (depends on 2)

The method of claim 2, wherein at least a majority of the first film is deposited at one or more temperatures below about 65° C.

### Claim 10 (depends on 2)

The method of claim 2, wherein at least a portion of step (c) occurs prior to forming the second film.

### Claim 11 (depends on 2)

The method of claim 2, wherein the first film is formed via sputtering.

### Claim 12 (depends on 2)

The method of claim 2, wherein the chalcogen(s) of the first film include at least one of Se and/or S.

### Claim 13 (depends on 2)

The method of claim 2, wherein the first film is formed on a surface including at least molybdenum.

### Claim 14 (depends on 2)

The method of claim 2, wherein the second film comprises copper, indium, at least one of selenium or sulfur, and optionally gallium.

### Claim 15

The method of any preceding claim wherein the first film as deposited comprises a PACB crystalline grain structure for which substantially all of the PACB crystalline grain sizes are under about 0.25 microns.

### Claim 16

A photovoltaic device, comprising:
a substrate;
a first PACB region formed directly or indirectly on the substrate, wherein the first PACB region comprises Cu, In, and at least one chalcogen, and wherein at least a major portion of the first PACB region comprises crystalline grains having a size under 100 nm as measured by XTEM and an average thickness for the region of less than about 200 nm; and
a second PACB region formed directly or indirectly on the first PACB region, wherein the second PACB region comprises Cu, In, and at least one chalcogen; wherein the combined thickness of first and second regions is less than 1000 nm.

### Claim 17

A photovoltaic device, comprising:
a substrate;
a first PACB region formed directly or indirectly on the substrate, wherein the first PACB region comprises Cu, In, and at least one chalcogen, and wherein the first PACB region has a thickness under about 200 nm; and
a second PACB region formed directly or indirectly on the first PACB region, wherein the second PACB region comprises Cu, In, and at least one chalcogen, wherein the second PACB region or has a thickness in the range from about 200 nm to about 1000 nm; and wherein the first PACB region has a smaller crystalline grain size as measured by XTEM than the second PACB region.

### Claim 18 (depends on 17)

The device of claim 17, wherein the total thickness of the first and second regions is less than about 500 nm.