# US 2011/0248372 A1 · Epitaxial substrate for solid-state imaging device with gettering sink, semiconductor device, back illuminated solid-state imaging device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0248372 A1
- Document ID: US20110248372A1
- Status: Published application
- Kind: A1
- Application number: 13/124,578
- Filed: 2009-10-16
- Published: 2011-10-13
- Earliest claimed: 2008-10-16
- Assignees: Sumco Corporation
- Inventors: Kazunari Kurita
- Web page: https://patentgrep.com/patent/US20110248372A1

## CPC

- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10F 39/028: {performed after manufacture of the image sensors, e.g. annealing, gettering of impurities, short-circuit elimination or recrystallisation}
- H10F 39/802: {Geometry or disposition of elements in pixels, e.g. address-lines or gate electrodes}
- H10P 36/00: Gettering within semiconductor bodies
- C30B 29/06: Silicon
- Y10S 117/904: Laser beam
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A semiconductor wafer is set in a laser irradiation apparatus, and laser beam irradiation is performed while the semiconductor wafer is moved. At this time, a laser beam emitted from a laser generating apparatus is condensed by a condensing lens so that the condensing point (focal point) is positioned at a depth of several tens of gm or so from one surface of the semiconductor wafer. Thereby, the crystal structure of the semiconductor wafer in the position having such a depth is modified, and a gettering sink is formed.

## Claims

### Claim 1

A method of manufacturing an epitaxial substrate for a solid-state imaging device, comprising the steps of:
growing an epitaxial layer on one surface of a semiconductor substrate to form an epitaxial substrate;
forming a gettering sink in which a crystal structure of an arbitrary microscopic region of the semiconductor substrate is changed, by causing a laser beam to be incident on the epitaxial substrate through a condensing means and condensing the laser beam in the microscopic region, to cause a multi-photon absorption process to occur in the microscopic region; and
annealing the epitaxial substrate at a predetermined temperature to capture heavy metals in the gettering sink.

### Claim 2 (depends on 1)

The method of manufacturing an epitaxial substrate for a solid-state imaging device according to claim 1, wherein the laser beam has a wavelength band capable of being transmitted through the epitaxial substrate, and the condensing means condenses the laser beam to an arbitrary position in the thickness direction of the semiconductor substrate.

### Claim 3 (depends on 1)

The method of manufacturing an epitaxial substrate for a solid-state imaging device according to claim 1, wherein the laser beam is an ultra-short pulsed-laser beam having a pulse width in a range of 1.0×10−15 to 1.0×10−8 seconds and a wavelength in a range of 300 to 1,200 nm.

### Claim 4 (depends on 1)

The method of manufacturing an epitaxial substrate for a solid-state imaging device according to claim 1, wherein the semiconductor substrate is made of a single crystal silicon, and the gettering sink includes silicon having an amorphous structure.

### Claim 5 (depends on 1)

The method of manufacturing an epitaxial substrate for a solid-state imaging device according to claim 1, wherein the gettering sink is formed at a position that overlaps a region for forming the solid-state imaging device.

### Claim 6 (depends on 1)

An epitaxial substrate for a solid-state imaging device manufactured by the method of manufacturing an epitaxial substrate for a solid-state imaging device according to claim 1,
wherein the gettering sink is provided to a region that overlaps at least a position for forming a buried-type photodiode included in the solid-state imaging device, with a size in a range of a diameter of 50 to 150 μm and a thickness of 10 to 150 μm.

### Claim 7 (depends on 6)

The epitaxial substrate for a solid-state imaging device according to claim 6, wherein the gettering sink is formed in a range of a density of 1.0×105 to 1.0×107 counts/cm2.

### Claim 8

A method of manufacturing a semiconductor device, comprising at least the steps of:
forming an insulating film on one surface of the semiconductor substrate;
forming a gettering sink in which a crystal structure of an arbitrary microscopic region of the semiconductor substrate is changed, by causing a laser beam to be incident from the other surface of the semiconductor substrate through a condensing means and condensing the laser beam in the microscopic region, to cause a multi-photon absorption process to occur in the microscopic region; and
annealing the semiconductor substrate at a predetermined temperature to capture heavy metals in the gettering sink.

### Claim 9 (depends on 8)

The method of manufacturing a semiconductor device according to claim 8, wherein the laser beam has a wavelength band capable of being transmitted through the semiconductor substrate, and the condensing means condenses the laser beam to an arbitrary position in the thickness direction of the semiconductor substrate.

### Claim 10 (depends on 8)

The method of manufacturing a semiconductor device according to claim 8, wherein the laser beam is an ultra-short pulsed-laser beam having a pulse width in a range of 1.0×10−15 to 1.0×10−8 seconds and a wavelength in a range of 300 to 1,200 nm.

### Claim 11 (depends on 8)

The method of manufacturing a semiconductor device according to claim 8, wherein the semiconductor substrate is made of a single crystal silicon, and the gettering sink includes silicon having an amorphous structure in at least a portion thereof.

### Claim 12 (depends on 8)

The method of manufacturing a semiconductor device according to claim 8, wherein the gettering sink is formed at a position that overlaps at least a region for forming the device.

### Claim 13 (depends on 8)

A semiconductor device, manufactured by the method of manufacturing a semiconductor device according to claim 8, in which the gettering sink is formed in a range of a density of 1.0×105 to 1.0×106 counts/cm2.

### Claim 14

A method of manufacturing a back illuminated solid-state imaging device, comprising at least the steps of:
growing an epitaxial layer on one surface of a semiconductor substrate to form an epitaxial substrate;
forming a gettering sink in which a crystal structure of an arbitrary microscopic region of the semiconductor substrate is changed, by causing a laser beam to be incident to the epitaxial substrate through a condensing means and condensing the laser beam in the microscopic region, to cause a multi-photon absorption process to occur in the microscopic region;
forming a plurality of photodiodes in the epitaxial substrate;
annealing the epitaxial substrate at a predetermined temperature to capture heavy metals in the gettering sink; and
removing a region including the gettering sink by reducing the thickness of the semiconductor substrate.

### Claim 15 (depends on 14)

The method of manufacturing a back illuminated solid-state imaging device according to claim 14, wherein the laser beam has a wavelength band capable of being transmitted through the epitaxial substrate, and the condensing means condenses the laser beam to an arbitrary position in the thickness direction of the semiconductor substrate.

### Claim 16 (depends on 14)

The method of manufacturing a back illuminated solid-state imaging device according to claim 14, wherein the laser beam is an ultra-short pulsed-laser beam having a pulse width in a range of 1.0×10−15 to 1.0×10−8 seconds and a wavelength in a range of 300 to 1,200 nm.

### Claim 17 (depends on 14)

The method of manufacturing a back illuminated solid-state imaging device according to claim 14, wherein the semiconductor substrate is made of a single crystal silicon, and the gettering sink includes silicon having an amorphous structure.

### Claim 18 (depends on 14)

The method of manufacturing a back illuminated solid-state imaging device according to claim 14, wherein the gettering sink is formed at a position that overlaps at least a region for forming the photodiode.

### Claim 19 (depends on 14)

The method of manufacturing a back illuminated solid-state imaging device according to claim 14, wherein a buried oxide film having a SOI structure is further formed between the gettering sink and the epitaxial layer.

### Claim 20

An epitaxial substrate for a solid-state imaging device, comprising a semiconductor substrate; an epitaxial layer formed on one surface of the semiconductor substrate; a gettering sink formed by changing a crystal structure of an arbitrary microscopic region of the semiconductor substrate, by causing a laser beam to be incident on the semiconductor substrate through a condensing means and condensing the laser beam in the microscopic region, to cause a multi-photon absorption process to occur in the microscopic region; and a buried oxide film having a SOI structure formed between the gettering sink and the epitaxial layer.

### Claim 21 (depends on 20)

The epitaxial substrate for a solid-state imaging device according to claim 20, wherein the gettering sink is provided to a region that overlaps at least a position for forming the photodiode, with a size in a range of a diameter of 50 to 150 μm and a thickness of 10 to 150 μm.

### Claim 22 (depends on 20)

The epitaxial substrate for a solid-state imaging device according to claim 20, wherein the gettering sink is formed in a range of a density of 1.0×105 to 1.0×107 counts/cm2.

### Claim 23

A method of manufacturing a silicon wafer, comprising at least:
a slicing step of slicing a silicon single crystal ingot to obtain a silicon wafer;
a multi-photon absorbing step of forming a gettering sink in which a crystal structure of an arbitrary microscopic region is changed, by causing a laser beam to be incident on the silicon wafer through a condensing means and condensing the laser beam in the microscopic region, to cause a multi-photon absorption process to occur in the microscopic region; and
a polishing step of mirror-polishing the silicon wafer through the multi-photon absorbing step.

### Claim 24 (depends on 23)

The method of manufacturing a silicon wafer according to claim 23, further comprising a lapping step of lapping the silicon wafer between the slicing step and the multi-photon absorbing step.

### Claim 25 (depends on 23)

The method of manufacturing a silicon wafer according to claim 23, further comprising an etching step of etching the silicon wafer between the slicing step and the multi-photon absorbing step.

### Claim 26 (depends on 23)

The method of manufacturing a silicon wafer according to claim 23, wherein the laser beam has a wavelength band capable of being transmitted through the silicon wafer, and the condensing means condenses the laser beam to an arbitrary position in the thickness direction of the silicon wafer.

### Claim 27 (depends on 23)

The method of manufacturing a silicon wafer according to claim 23, wherein the laser beam is an ultra-short pulsed-laser beam having a pulse width in a range of 1.0×10−15 to 1.0×10−8 seconds and a wavelength in a range of 300 to 1,200 nm.

### Claim 28 (depends on 23)

The method of manufacturing a silicon wafer according to claim 23, wherein the gettering sink includes silicon having an amorphous structure.

### Claim 29 (depends on 23)

A method of manufacturing an epitaxial wafer, comprising at least an epitaxial step of growing an epitaxial layer made of a silicon single crystal on one surface of the silicon wafer obtained by the method of manufacturing a silicon wafer according to claim 23.

### Claim 30 (depends on 29)

A method of manufacturing a solid-state imaging device, comprising at least an element forming step of forming a buried-type photodiode on one surface of the epitaxial wafer obtained by the method of manufacturing an epitaxial wafer according to claim 29.

### Claim 31 (depends on 30)

The method of manufacturing a solid-state imaging device according to claim 30, further comprising an annealing step of annealing the epitaxial wafer at a predetermined temperature to capture heavy metals in the gettering sink.

### Claim 32 (depends on 30)

The method of manufacturing a solid-state imaging device according to claim 30, wherein the gettering sink is formed at a region that overlaps at least a position for forming the buried-type photodiode, with a size in a range of a diameter of 50 to 150 μm and a thickness of 10 to 150 μm.

### Claim 33 (depends on 30)

The method of manufacturing a solid-state imaging device according to claim 30, wherein the gettering sink is formed so as to have a density in a range of 1.0×105 to 1.0×107 counts/cm2.