# US 2011/0236799 A1 · Manufacturing methods for air electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0236799 A1
- Document ID: US20110236799A1
- Status: Published application
- Kind: A1
- Application number: 13/026,054
- Filed: 2011-02-11
- Published: 2011-09-29
- Earliest claimed: 2010-02-12
- Assignees: ReVolt Technology Ltd.
- Inventors: Trygve Burchardt; Adam Laubach; Anne-Laure Becquet; Christopher Pedicini; James P. McDougall
- Web page: https://patentgrep.com/patent/US20110236799A1

## CPC

- H01M 4/8605: {Porous electrodes}
- H01M 4/8642: {Gradient in composition}
- H01M 4/8657: {layered}
- H01M 4/8663: {Selection of inactive substances as ingredients for catalytic active masses, e.g. binders, fillers}
- H01M 4/8892: {Impregnation or coating of the catalyst layer, e.g. by an ionomer}
- H01M 12/06: with one metallic and one gaseous electrode
- H01M 12/08: composed of a half-cell of a fuel-cell type and a half-cell of the secondary-cell type
- H01M 4/8615: {Bifunctional electrodes for rechargeable cells}
- H01M 50/417: Polyolefins
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 2300/0082: Organic polymers
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods of forming an air electrode of a metal-air battery are provided. One method includes forming a plurality of layers of the air electrode. The plurality of layers include an active layer and a gas diffusion layer. Forming at least one of the active layer or the gas diffusion layer includes forming a first sublayer having a first concentration of a first material and forming a second sublayer having at least one of a second concentration of the first material that differs from the first concentration or a second material that differs from the first material. In another embodiment, a method includes forming a layer of an air electrode such that a gradient of a material is formed in at least a portion of the layer by varying a concentration of the material deposited between a first portion of the layer and a second portion of the layer.

## Claims

### Claim 1

A method of providing an air electrode for a metal-air battery, the method comprising:
forming a plurality of layers of the air electrode, wherein the plurality of layers comprise an active layer and a gas diffusion layer, and wherein forming at least one of the active layer or the gas diffusion layer comprises:
forming a first sublayer having a first concentration of a first material; and
forming a second sublayer having at least one of a second concentration of the first material that differs from the first concentration or a second material that differs from the first material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first sublayer and the second sublayer are part of the active layer, and wherein at least one of the first material or the second material is a catalyst material.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
providing an electrolyte in the metal-air battery; and
providing the air electrode in the metal-air battery such that the first sublayer is nearer to the electrolyte than the second sublayer;
wherein the first concentration is higher than the second concentration.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first sublayer and the second sublayer are part of the active layer, and wherein at least one of the first material or the second material is a surfactant material.

### Claim 5 (depends on 4)

The method of claim 4, further comprising:
providing an electrolyte in the metal-air battery; and
providing the air electrode in the metal-air battery such that the first sublayer is nearer to the electrolyte than the second sublayer;
wherein the first sublayer is formed using a first surfactant material and the second sublayer is formed using a second surfactant material, and wherein the first surfactant material includes surfactants that are removable at a higher temperature than surfactants of the second surfactant material.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
providing an electrolyte in the metal-air battery; and
providing the air electrode in the metal-air battery such that the first sublayer is nearer to the electrolyte than the second sublayer;
wherein the first sublayer is formed using a non-carbon material and the second sublayer is formed using a carbon material.

### Claim 7 (depends on 1)

The method of claim 1, further comprising printing a hydrophobic layer about a periphery of at least one of the first sublayer and the second sublayer.

### Claim 8

A metal-air battery comprising:
an air electrode comprising a plurality of layers, wherein the plurality of layers comprise an active layer and a gas diffusion layer, wherein at least one of the active layer or the gas diffusion layer comprises:
a first sublayer having a first concentration of a first material; and
a second sublayer having at least one of a second concentration of the first material that differs from the first concentration or a second material that differs from the first material.

### Claim 9 (depends on 8)

The metal-air battery of claim 8, wherein the first sublayer and the second sublayer are part of the active layer, and wherein at least one of the first material or the second material is a catalyst material.

### Claim 10 (depends on 9)

The metal-air battery of claim 9, further comprising an electrolyte, wherein the air electrode is provided such that the first sublayer is nearer to the electrolyte than the second sublayer, and wherein the first concentration is higher than the second concentration.

### Claim 11 (depends on 8)

The metal-air battery of claim 8, wherein the first sublayer and the second sublayer are part of the active layer, and wherein at least one of the first material or the second material is a surfactant material.

### Claim 12 (depends on 11)

The metal-air battery of claim 11, further comprising an electrolyte, wherein the air electrode is provided such that the first sublayer is nearer to the electrolyte than the second sublayer, wherein the first sublayer comprises first surfactant material and the second sublayer comprises a second surfactant material, and wherein the first surfactant material includes surfactants that are removable at a higher temperature than surfactants of the second surfactant material.

### Claim 13 (depends on 8)

The metal-air battery of claim 8, further comprising an electrolyte, wherein the air electrode is provided such that the first sublayer is nearer to the electrolyte than the second sublayer, and wherein the first sublayer comprises a non-carbon material and the second sublayer comprises a carbon material.

### Claim 14 (depends on 8)

The metal-air battery of claim 8, wherein the air electrode further comprises a hydrophobic layer positioned about a periphery of at least one of the first sublayer and the second sublayer.

### Claim 15

A method of providing an air electrode of a metal-air battery, the method comprising:
forming a layer of an air electrode such that a gradient of a material is formed in at least a portion of the layer by varying a concentration of the material deposited between a first portion of the layer and a second portion of the layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the material comprises a first material, and wherein the gradient is formed by:
forming a first sublayer having a first concentration of the material; and
forming a second sublayer having at least one of a second concentration of the first material that differs from the first concentration or a second material that differs from the first material.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first sublayer and the second sublayer are part of the active layer, and wherein at least one of the first material or the second material is a catalyst material.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
providing an electrolyte in the metal-air battery; and
providing the air electrode in the metal-air battery such that the first sublayer is nearer to the electrolyte than the second sublayer;
wherein the first concentration is higher than the second concentration.

### Claim 19 (depends on 16)

The method of claim 16, wherein the first sublayer and the second sublayer are part of the active layer, and wherein at least one of the first material or the second material is a surfactant material.

### Claim 20 (depends on 19)

The method of claim 19, further comprising:
providing an electrolyte in the metal-air battery; and
providing the air electrode in the metal-air battery such that the first sublayer is nearer to the electrolyte than the second sublayer;
wherein the first sublayer is formed using a first surfactant material and the second sublayer is formed using a second surfactant material, and wherein the first surfactant material includes surfactants that are removable at a higher temperature than surfactants of the second surfactant material.

### Claim 21 (depends on 16)

The method of claim 16, further comprising:
providing an electrolyte in the metal-air battery; and
providing the air electrode in the metal-air battery such that the first sublayer is nearer to the electrolyte than the second sublayer;
wherein the first sublayer is formed using a non-carbon material and the second sublayer is formed using a carbon material.

### Claim 22 (depends on 16)

The method of claim 16, further comprising printing a hydrophobic layer about a periphery of at least one of the first sublayer and the second sublayer.