# US 2011/0236691 A1 · Method for producing fixing-unit member and fixing-unit member

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0236691 A1
- Document ID: US20110236691A1
- Status: Published application
- Kind: A1
- Application number: 13/050,576
- Filed: 2011-03-17
- Published: 2011-09-29
- Earliest claimed: 2010-03-23
- Assignees: Sumitomo Electric Fine Polymer, Inc.
- Inventors: Yasuhiro FUKUMOTO; Hiromi KAMIMURA; Shingo HARADA; Naoki YOKOTA
- Web page: https://patentgrep.com/patent/US20110236691A1

## CPC

- B29C 65/66: by liberation of internal stresses, e.g. shrinking of one of the parts to be joined
- B29C 65/7838: {from the inside, e.g. of tubular or hollow articles (B29C66/3242 takes precedence)}
- B29C 66/7371: {oriented or heat-shrinkable}
- B32B 37/144: {using layers with different mechanical or chemical conditions or properties, e.g. layers with different thermal shrinkage, layers under tension during bonding (constructional features for tensioning B32B38/1825)}
- G03G 15/2057: {relating to the chemical composition of the heat element and layers thereof}
- Y10T 428/3154: Of fluorinated addition polymer from unsaturated monomers
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for producing a fixing-unit member including a base, a rubber elastic layer, and a PFA layer includes a step of forming a primer layer by applying a primer containing a low-melting fluorocarbon resin to the outer circumferential surface of a rubber roller having the rubber elastic layer on the outer circumferential surface of the base; a step of sheathing the rubber roller with a thermally shrinkable tube formed by diametrically expanding a PFA tube so as to have an inner diameter more than the outer diameter of the rubber roller; a step of forming the PFA layer from the thermally shrinkable tube by heating the thermally shrinkable tube so as to be thermally shrunken and fused with the rubber roller; and a reheating step of heating the PFA layer to a temperature equal to or higher than the melting point of the PFA contained in the PFA layer.

## Claims

### Claim 1

A method for producing a fixing-unit member including a base, a rubber elastic layer, and a tetrafluoroethylene-perfluoro(alkyl vinyl ether) copolymer (PFA) layer containing 70 wt % or more of a PFA, the method comprising:
(I) a primer-layer-forming step of forming a primer layer by applying a primer to an outer circumferential surface of a rubber roller prepared by forming the rubber elastic layer on an outer circumferential surface of the base, the primer containing a fluorocarbon resin that has a melting point equal to or lower than a melting point of the PFA contained in the PFA layer;
(II) a rubber-roller-sheathing step of sheathing the rubber roller including the primer layer, with a thermally shrinkable tube formed by diametrically expanding a PFA tube so as to have an inner diameter more than an outer diameter of the rubber roller including the primer layer, the PFA tube containing 70 wt % or more of the PFA and having an inner diameter equal to or less than the outer diameter of the rubber roller including the primer layer;
(III) a PFA-layer-forming step of forming the PFA layer from the thermally shrinkable tube by heating the thermally shrinkable tube around the rubber roller to a temperature equal to or higher than a crystallization temperature of the PFA contained in the thermally shrinkable tube so that the thermally shrinkable tube is thermally shrunken and is fused with the rubber roller including the primer layer, with the primer layer between the thermally shrinkable tube and the outer circumferential surface of the rubber roller; and
(IV) a reheating step of heating the PFA layer to a temperature equal to or higher than the melting point of the PFA contained in the PFA layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in the PFA-layer-forming step, the temperature to which the thermally shrinkable tube is heated is lower than the melting point of the PFA contained in the thermally shrinkable tube.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising, after the reheating step, a rapid-cooling step of cooling the PFA layer at a rate of 200° C./min or higher.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the PFA layer has a thickness of 50 μm or less.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the PFA tube is formed by extrusion in a temperature range of 380° C. to 440° C.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the PFA-layer-forming step is performed while a metal shaft is inserted through the base.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the reheating step is performed without the metal shaft inserted through the base.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the base is composed of a metal or a heat-resistant resin.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the rubber elastic layer is composed of a rubber composition containing a thermally conductive filler and at least one heat-resistant rubber selected from the group consisting of silicone rubber and fluorocarbon rubber.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the fixing-unit member is a fixing roller or a fixing belt.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the fixing-unit member is a pressing roller or a pressing belt.

### Claim 12 (depends on 1)

A fixing-unit member produced by the method according to claim 1.