# US 2011/0236680 A1 · Method for producing components for high temperature applications and metal component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0236680 A1
- Document ID: US20110236680A1
- Status: Published application
- Kind: A1
- Application number: 13/132,331
- Filed: 2009-12-02
- Published: 2011-09-29
- Earliest claimed: 2008-12-02
- Assignees: Paul Hettich GmbH & Co. KG
- Inventors: Peter Jahrling; Lars Schrubke; Willi Crigat
- Web page: https://patentgrep.com/patent/US20110236680A1

## CPC

- B05D 7/14: to metal, e.g. car bodies (involving a chemical reaction between the metal and the coating C23)
- C23C 18/122: {Inorganic polymers, e.g. silanes, polysilazanes, polysiloxanes}
- C23C 18/1233: {Organic substrates}
- C23C 18/1254: {Sol or sol-gel processing}
- C23C 18/127: {Preformed particles}
- C23C 18/1283: {Control of temperature, e.g. gradual temperature increase, modulation of temperature}
- C23C 18/1295: {with after-treatment of the deposited inorganic material}
- C23C 18/143: {Radiation by light, e.g. photolysis or pyrolysis}
- C23C 26/00: Coating not provided for in groups C23C2/00 - C23C24/00
- B05D 3/0254: {After-treatment}
- Y10T 428/269: including synthetic resin or polymer layer or component
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for the production of a component, the method steps including: providing a blank; applying an inorganic-organic hybrid polymer layer to a surface of the blank to form a coated blank; heating the coated blank until a curing of the polymer layer occurs; and cooling the coated blank. A component produced according to the method.

## Claims

### Claim 1

A method for the production of a component, the method steps comprising:
providing a blank;
applying an inorganic-organic hybrid polymer layer to a surface of the blank to form a coated blank;
heating the coated blank until a curing of the polymer layer occurs; and
cooling the coated blank.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the applying of the inorganic-organic hybrid polymer layer onto the surface of the blank occurs by a sol-gel method, which sol-gel method comprises the following steps:
formation of a sol by hydrolysis;
applying the sol onto the surface of the blank; and
forming an adhesive gel layer by polycondensation.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the applying of the inorganic-organic hybrid polymer layer onto the surface of the blank includes polyetheretherketone and occurs according to the sol-gel method.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the applying of the sol in the applying of the inorganic-organic hybrid polymer layer occurs by spraying onto the surface of the blank.

### Claim 5 (depends on 1)

The method according to claim 1, further comprising the step of curing of the inorganic-organic hybrid polymer layer by ultraviolet radiation, which step is performed between either the applying and heating steps or after the heating step.

### Claim 6 (depends on 2)

The method according to claim 2, wherein further inorganic materials are added to the sol, including one or both of silicon oxide and titanium oxide.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the inorganic-organic hybrid polymer layer includes a silicon-, aluminum- or titanium-containing inorganic-organic hybrid polymer having a temperature resistance up to 600° C.

### Claim 8 (depends on 1)

The method according to claim 1, wherein in a heat-up phase, a first time-dependent temperature gradient is 8 to 12 K/min up to a middle temperature and a second time-dependent temperature gradient is 12 to 30 K/min up to a target temperature.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the coated blank is tempered at least 25 minutes, at a target temperature of 450 to 550° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the coated blank is tempered at least 25 minutes, at a target temperature of 650 to 750° C.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the target temperature is kept constant over a period of 25 to 40 minutes.

### Claim 12 (depends on 11)

The method according to claim 11, wherein a time-dependent temperature gradient of controlled cooling of the blank is 15 to 25 K/min.

### Claim 13 (depends on 9)

The method according to claim 9, characterized wherein the coated blank is tempered in a forced-air method with an air throughput of 50 to 70 L/min.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the surface of the blank is smoothed prior to the applying of the inorganic-organic hybrid polymer layer.

### Claim 15 (depends on 1)

The method according to claim 1, wherein a metal compound of one or both of aluminum and manganese is diffused into the hybrid polymer layer during the heating of the coated blank for protection from corrosion.

### Claim 16 (depends on 1)

The component, for use in domestic appliances, the component comprising a coating produced according to the method of claim 1.

### Claim 17 (depends on 16)

The component according to claim 16, wherein the inorganic-organic hybrid polymer layer includes either a dye or pigments.

### Claim 18 (depends on 16)

The component according to claim 16, wherein the hybrid polymer layer includes at least a mass fraction of a metal of at least 12%, the metal including, one or both of aluminum and manganese, for protection from corrosion.

### Claim 19 (depends on 1)

The component according to claim 1, wherein the component includes a substrate metallic base body, an intermediate layer arranged above the base body, and which intermediate layer includes silicon oxide and at least one metal, the at least one metal including one or both of aluminum and manganese, and the component further includes a cover layer including silicon oxide, the intermediate layer forming a protection from corrosion of the substrate in case of injury of the cover layer.

### Claim 20 (depends on 19)

The component according to claim 19, wherein the cover layer has a mass fraction, for at least silicon, of at least 35%.

### Claim 21 (depends on 19)

The component according to claim 19, wherein the intermediate layer has at least one mass fraction, of aluminum, of between 10 to 12%.

### Claim 22 (depends on 19)

The component according to claim 19, wherein the intermediate layer thickness of the coating is 20 to 30 μm.

### Claim 23 (depends on 16)

The component according to claim 16, wherein the component is arranged as a rail of a pull-out guide for baking ovens.

### Claim 24 (depends on 16)

The component according to claim 16, wherein the component is configured to be used as a rail in domestic appliances, the domestic appliances including one or more of baking ovens, refrigerators, washing machines, and a furniture fitting.

### Claim 25 (depends on 1)

The method according to claim 1, wherein the inorganic-organic hybrid polymer layer includes a silicon-, aluminum- or titanium-containing inorganic-organic hybrid polymer having a temperature resistance up to 800° C.

### Claim 26 (depends on 1)

The method according to claim 1, wherein the coated blank is tempered at least 20 minutes, at a target temperature of 200 to 600° C.

### Claim 27 (depends on 1)

The method according to claim 1, wherein the coated blank is tempered at least 20 minutes, at a target temperature of 500 to 800° C.

### Claim 28 (depends on 9)

The method according to claim 9, wherein the target temperature is kept constant over a period of 15 to 90 minutes.

### Claim 29 (depends on 11)

The method according to claim 11, wherein a time-dependent temperature gradient of controlled cooling of the blank is 5 to 40 K/min.

### Claim 30 (depends on 9)

The method according to claim 9, wherein the coated blank is tempered in a forced-air method with an air throughput of 30 to 90 L/min.

### Claim 31 (depends on 16)

The component according to claim 16, wherein the hybrid polymer layer includes at least a mass fraction of a metal of 7%, the metal including, one or both of aluminum and manganese, for protection from corrosion.

### Claim 32 (depends on 19)

The component according to claim 19, wherein the cover layer has a mass fraction, for at least silicon, of at least 30%.

### Claim 33 (depends on 19)

The component according to claim 19, wherein the intermediate layer has at least one mass fraction, for at least aluminum, of 7%.

### Claim 34 (depends on 19)

The component according to claim 19, wherein the intermediate layer thickness of the coating is 10 to 40 μm.