# US 2011/0215278 A1 · Semiconducting composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0215278 A1
- Document ID: US20110215278A1
- Status: Published application
- Kind: A1
- Application number: 12/718,649
- Filed: 2010-03-05
- Published: 2011-09-08
- Earliest claimed: 2010-03-05
- Assignees: General Cable Technologies Corporation
- Inventors: Mark R. Easter
- Web page: https://patentgrep.com/patent/US20110215278A1

## CPC

- H01B 3/004: {with conductive additives or conductive layers}
- C08K 3/04: Carbon
- C08K 5/06: Ethers; Acetals; Ketals; Ortho-esters
- C08L 23/06: Polyethylene
- C08L 23/0853: Ethylene vinyl acetate copolymers
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C09J 123/0853: {Vinylacetate}
- H01B 3/427: {Polyethers}
- H01B 3/441: {from alkenes}
- H01B 3/447: {from acrylic compounds}
- H01B 3/448: {from other vinyl compounds}
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

An improved conductor shielding composition for power cables is disclosed. The composition includes a base polymer, conductive carbon black, polyethylene glycol and a waxy additive. Cable shields prepared from the composition exhibit improved aging performance in accelerated cable life tests (ACLT).

## Claims

### Claim 1

A conductor shield composition comprising:
a base polymer selected from the group consisting of copolymers of ethylene and a mono-unsaturated ester, copolymers of ethylene and one or more alpha olefins having three to six carbon atoms, EPR rubbers, low density polyethylene and linear low density polyethylene;
conductive carbon black;
polyethylene glycol; and
a waxy additive different from said base polymer selected from the group consisting of at least one amide wax, at least one ethylene wax of copolymers of ethylene and a mono-unsaturated ester mixture of at least one amide wax and at least one wax of copolymers of ethylene and a mono-unsaturated ester.

### Claim 2 (depends on 1)

The composition of claim 1, wherein said waxy additive is an ethylene vinyl acetate wax that has a molecular weight from about 5,000 Daltons to about 40,000 Daltons and a vinyl acetate content of from about 2% to about 28%.

### Claim 3 (depends on 2)

The composition of claim 2, wherein said at least one ethylene vinyl acetate wax has a vinyl acetate content of from about 8% to about 20%.

### Claim 4 (depends on 2)

The composition of claim 2, Wherein said at least one ethylene vinyl acetate wax has a molecular weight from about 10,000 Daltons to about 25,000 Daltons and a vinyl acetate content of from about 12% to about 15%.

### Claim 5 (depends on 1)

The composition of claim 1, wherein said waxy additive is from about 0.5% to about 5.0% by weight of the composition.

### Claim 6 (depends on 5)

The composition of claim 5, wherein said base polymer is a copolymer of ethylene and vinyl acetate.

### Claim 7 (depends on 6)

The composition of claim 6, wherein said base polymer has a vinyl acetate content between 10% and 15%.

### Claim 8 (depends on 1)

The composition of claim 1, wherein the polyethylene glycol has a molecular weight of about 5000 to about 25,000 Daltons.

### Claim 9 (depends on 1)

The composition of claim 1 having an accelerated cable life testing Weibull Alpha value of 1500 or more.

### Claim 10 (depends on 1)

The composition of claim 1 wherein said base polymer is selected from the group consisting of copolymers of ethylene and a mono-unsaturated ester, copolymers of ethylene and one or more alpha olefins having three to six carbon atoms, low density polyethylene and linear low density polyethylene.

### Claim 11

A conductor shield composition consisting essentially of:
a base polymer selected from the group consisting of copolymers of ethylene and a mono-unsaturated ester, copolymers of ethylene and one or more alpha olefins having three to six carbon atoms, EPR rubbers, low density polyethylene and linear low density polyethylene;
conductive carbon black;
polyethylene glycol; and
a waxy additive different from said base polymer selected from the group consisting of at least one amide wax, at least one ethylene vinyl acetate wax and mixtures of at least one amide wax and at least one ethylene vinyl acetate wax.

### Claim 12 (depends on 11)

The composition of claim 11, wherein said waxy additive is an ethylene vinyl acetate wax that has a molecular weight from about 5,000 Daltons to about 40,000 Daltons and a vinyl acetate content of from about 2% to about 28%.

### Claim 13 (depends on 12)

The composition of claim 12, wherein said at least one ethylene vinyl acetate wax has a vinyl acetate content of from about 8% to about 20%.

### Claim 14 (depends on 12)

The composition of claim 12, Wherein said at least one ethylene vinyl acetate wax has a molecular weight from about 10,000 Daltons to about 25,000 Daltons and a vinyl acetate content of from about 12% to about 15%.

### Claim 15 (depends on 11)

The composition of claim 11, wherein said waxy additive is from about 0.5% to about 5.0% by weight of the composition.

### Claim 16 (depends on 15)

The composition of claim 15, wherein said base polymer is a copolymer of ethylene and vinyl acetate.

### Claim 17 (depends on 16)

The composition of claim 16, wherein said base polymer has a vinyl acetate content between 10% and 15%.

### Claim 18 (depends on 11)

The composition of claim 11, wherein the polyethylene glycol has a molecular weight of about 5000 to about 25,000 Daltons.

### Claim 19 (depends on 11)

The composition of claim 11 having an accelerated cable life testing Weibull Alpha value of 1500 or more.

### Claim 20 (depends on 1)

The composition of claim 1 wherein said base polymer is selected from the group consisting of copolymers of ethylene and a mono-unsaturated ester, copolymers of ethylene and one or more alpha olefins having three to six carbon atoms, low density polyethylene and linear low density polyethylene.