# US 2011/0214785 A1 · Method for forming a tubular medical device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0214785 A1
- Document ID: US20110214785A1
- Status: Published application
- Kind: A1
- Application number: 12/717,256
- Filed: 2010-03-04
- Published: 2011-09-08
- Earliest claimed: 2010-03-04
- Assignees: ICON Medical Corp.
- Inventors: Raymond W. Buckman, JR.; Udayan Patel; Joseph Furst
- Web page: https://patentgrep.com/patent/US20110214785A1

## CPC

- A61L 31/022: {Metals or alloys}
- B22F 5/106: {Tube or ring forms}
- A61F 2/91: made from perforated sheets or tubes, e.g. perforated by laser cuts or etched holes
- B21D 31/00: Other methods for working sheet metal, metal tubes, metal profiles (deforming one surface of tubes helically by rolling B21H3/00; upsetting B21J5/08; working metal by removing material therefrom B23; embossing B44B)
- B22F 3/20: by extruding
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- C22C 27/04: Alloys based on tungsten or molybdenum
- C22F 1/18: High-melting or refractory metals or alloys based thereon
- C22F 1/183: {of titanium or alloys based thereon}
- C23C 8/24: Nitriding
- B22F 2003/247: {Removing material: carving, cleaning, grinding, hobbing, honing, lapping, polishing, milling, shaving, skiving, turning the surface}
- B22F 2003/248: {Thermal after-treatment}
- B22F 2998/10: Processes characterised by the sequence of their steps
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- A61F: FILTERS IMPLANTABLE INTO BLOOD VESSELS; PROSTHESES; DEVICES PROVIDING PATENCY TO, OR PREVENTING COLLAPSING OF, TUBULAR STRUCTURES OF THE BODY, e.g. STENTS; ORTHOPAEDIC, NURSING OR CONTRACEPTIVE DEVICES; FOMENTATION; TREATMENT OR PROTECTION OF EYES OR EARS; BANDAGES, DRESSINGS OR ABSORBENT PADS; FIRST-AID KITS (dental prosthetics A61C)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method and process for at least partially forming a medical device that is at least partially formed of a metal alloy which improves the physical properties of the medical device.

## Claims

### Claim at position 1

1-26. (canceled)

### Claim 27

A method for forming a medical device comprising the steps of:
a) forming a rod or tube having a surface and an outer cross-sectional area, said rod or tube including a metal alloy that is formed of at least about 95 weight percent of a solid solution of molybdenum and rhenium or tungsten and tantalum;
b) drawing down said outer cross-sectional area of said rod or tube by a reducing mechanism;
c) annealing said rod or tube at an annealing temperature in an oxygen reducing environment or inert environment after said rod or tube has been drawn down;
d) cooling said annealed rod or tube at a rate of at least about 100° C. per minute;
e) drawing down said cross-sectional area of said rod or tube by the reducing mechanism after said rod or tube has been annealed; and,
f) annealing said rod or tube at least one additional time at an annealing temperature that is lower temperature than at least one annealing temperature of a previous annealing of said rod or tube.

### Claim 28 (depends on 27)

The method as defined in claim 27, wherein said step of forming said rod or tube includes a process of isostatically pressing metal powder together and subsequently sintering said metal power to form said rod or tube in a controlled atmosphere, said rod or tube having an average density of about 0.7-0.95 a minimum theoretical density of said metal alloy, said rod or tube have an average density of about 12-14 gm/cc, said controlled atmosphere including an inert atmosphere, an oxygen reducing atmosphere, or a vacuum.

### Claim 29 (depends on 28)

The method as defined in claim 28, wherein said tube is formed by gun drilling, EDM cutting, or combinations thereof a passageway at least partially through a longitudinal length of said rod.

### Claim 30 (depends on 27)

The method as defined in claim 27, wherein said step of forming said rod or tube includes a) forming an ingot of metal, b) extruding said ingot through a die to form a rod, c) hollowing out said rod to form a passageway at least partially through a longitudinal length of said rod, and d) polishing a surface of said passageway.

### Claim 31 (depends on 30)

The method as defined in claim 30, wherein said step of hollowing includes gun drilling, EDM cutting, or combinations thereof said rod to form said passageway.

### Claim 32 (depends on 1)

The method as defined in claim 1, wherein said metal alloy includes about 41-49 weight percent rhenium, about 51-59 weight percent molybdenum, and up to about 1 weight percent additional metal, said additional metal including a metal selected from the group consisting of titanium, yttrium, zirconium, or mixtures thereof

### Claim 33 (depends on 27)

The method as defined in claim 27, including the step of nitriding said rod or tube to form a nitride layer on said rod or tube prior to at least one drawing down step, said step of nitriding including a) exposing at least a portion of said rod or tube to a nitriding gas that includes nitrogen, nitrogen and hydrogen, or combinations thereof, and b) exposing at least a portion of said rod or tube to a nitriding gas at a temperature of less than about 400° C. for at least about 1 minute.

### Claim 34 (depends on 33)

The method as defined in claim 33, including the step of removing said nitride layer on said rod or tube prior to annealing said rod or tube.

### Claim 36 (depends on 27)

The method as defined in claim 27, including the step of protecting said rod or tube from oxygen when said rod or tube is exposed to temperatures of greater than about 400-500° C.

### Claim 37 (depends on 27)

The method as defined in claim 27, wherein said step of drawing down said cross-sectional area of said rod or tube by a reducing mechanism that reduces said cross-sectional area by less than about 20% each time said rod or tube is processed by said reducing mechanism.

### Claim 38 (depends on 37)

The method as defined in claim 37, wherein said step of drawing down includes the step of inserting a close-fitting rod in said passageway of said tube prior to using said reducing mechanism on said tube.

### Claim 39 (depends on 27)

The method as defined in claim 27, wherein said step of annealing said rod or tube includes the steps of a) annealing the rod or tube at an annealing temperature of at least about 1480° C. for a time period of at least about 5 minutes for a time period of at least about 5 minutes when said rod or tube has wall thickness of greater than about 0.015 inch, b) annealing the rod or tube at an annealing temperature of about 1450-1480° C. for a time period of at least about 5 minutes when said rod or tube has wall thickness of about 0.008-0.015 inch, and c) annealing the rod or tube at an annealing temperature of less than about 1450° C. for a time period of at least about 5 minutes when said rod or tube has wall thickness of less than about 0.008 inch.

### Claim 40 (depends on 27)

The method as defined in claim 27, wherein said medical device is a stent.

### Claim 41 (depends on 27)

The method as defined in claim 27, where said rod or tube after completion of all of the annealing steps has an average grain size of 4-14 ASTM.

### Claim 42 (depends on 27)

The method as defined in claim 27, wherein one or more portions of the rod or tube includes smaller tubular structures or segments affixed to each other, each of said tubular structures or segments can be annealed prior to and/or after separation from the initial rod or tube, secondary forming, being affixed to additional segments to construct the tubular device, secondary pickle and/or electropolish processes, or combinations thereof.

### Claim 43 (depends on 27)

The method as defined in claim 27, wherein said initial tube has a wall thickness of about 0.001-0.100 inch.

### Claim 44

A method for forming a stent comprising the steps of:
a) forming a tube having a surface and an outer cross-sectional area, said tube formed of a metal alloy comprising about 41-49 weight percent rhenium, about 51-59 weight percent molybdenum;
b) drawing down said outer cross-sectional area of said tube by a reducing mechanism;
c) nitriding said tube to form a nitride layer on said tube prior to at least one of said drawing down steps, said step of nitriding including i) exposing at least a portion of said tube to a nitriding gas that includes nitrogen, nitrogen and hydrogen, or combinations thereof, and b) exposing at least a portion of said tube to a nitriding gas at a temperature of less than about 400° C. for at least about 1 minute, said nitride layer removed prior to said tube being annealed;
d) annealing said tube at an annealing temperature in an oxygen reducing environment or inert environment after said tube has been drawn down;
e) cooling said annealed tube at a rate of at least about 100° C. per minute;
f) drawing down said cross-sectional area of said tube by the reducing mechanism after said rod or tube has been annealed, said step of drawing down said cross-sectional area of said tube reduces said cross-sectional area by less than about 20% each time said tube is processed by said reducing mechanism;
g) annealing said rod or tube at least one additional time at an annealing temperature that is lower temperature than at least one annealing temperature of a previous annealing of said rod or tube, said steps of annealing said tube include the steps of a) annealing said tube at an annealing temperature of at least about 1480° C. for a time period of at least about 5 minutes for a time period of at least about 5 minutes when said tube has wall thickness of greater than about 0.015 inch, b) annealing said tube at an annealing temperature of about 1450-1480° C. for a time period of at least about 5 minutes when said tube has wall thickness of about 0.008-0.015 inch, and c) annealing said tube at an annealing temperature of less than about 1450° C. for a time period of at least about 5 minutes when said tube has wall thickness of less than about 0.008 inch;
h) protecting said tube from oxygen when said tube is exposed to temperatures of greater than about 400-500° C.; and,
i) cutting said tube to form said stent, said stent formed of a cut tube having an average grain size of 4-14 ASTM.

### Claim 45 (depends on 44)

The method as defined in claim 44, wherein said step of drawing down includes the step of inserting a close-fitting rod in said passageway of said tube prior to using said reducing mechanism on said tube.