High surface area ceramic catalysts and the manufacture thereof
AssigneeNalco Company
InventorFelice DiMascio
Life of this patent
Estimating the term…
Abstract
A process for making a ceramic catalyst material includes mixing a catalyst precursor material with a mineral particulate to form a mixture; adding a binder, silicon carbide, and a parting agent to the mixture to form unfired spheroids; and heating the unfired spheroids at a temperature effective to oxidize the silicon carbide and the catalyst precursor material to form the ceramic catalyst material. In another embodiment, the process includes the addition of a catalyst metal oxide salt to an aluminosilicate hydrogel aggregate mixture. Once the mixture sets, the set mixture is heated to a temperature to effective to produce a high surface area ceramic catalyst material.
Claims16
A process for making a porous ceramic catalyst material comprising:
- (i) mixing a catalyst precursor material with a mineral particulate to form a mixture;
- (ii) adding a binder, silicon carbide, and a parting agent to the mixture to form unfired spheroids;
- (iii) and heating the unfired spheroids at a temperature effective to oxidize the silicon carbide and the catalyst precursor material to form the porous ceramic catalyst material.
A process for forming a porous ceramic catalyst material, the process comprising:
- (i) mixing a binder, aggregates, and a catalyst precursor, wherein the binder comprises an alkali, alumina, and silica;
- (ii) forming a rigid composite of the mixture;
- and (iii) heating the rigid composite to a temperature greater than 500° C. to form the porous ceramic catalyst material.
Dependencies are inferred from the claim text.