# US 2011/0212621 A1 · Abrasive composition and method for manufacturing semiconductor integrated circuit device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0212621 A1
- Document ID: US20110212621A1
- Status: Published application
- Kind: A1
- Application number: 13/101,560
- Filed: 2011-05-05
- Published: 2011-09-01
- Earliest claimed: 2008-11-10
- Assignees: Asahi Glass Company, Limited
- Inventors: Iori YOSHIDA; Hiroyuki Kamiya
- Web page: https://patentgrep.com/patent/US20110212621A1

## CPC

- C09K 3/1409: {Abrasive particles per se (preparation of diamond C01B32/25)}
- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- C09K 3/1463: {Aqueous liquid suspensions}
- H10P 52/403: {of conductive or resistive materials}
- H10W 20/062: {by smoothing of conductive parts, e.g. by planarisation}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention relates to a polishing composition used in a step of polishing until a barrier layer adjacent to a copper layer is exposed, in a pattern formation of polishing the copper layer provided on an insulating layer through the barrier layer thereby alternately forming a copper embedded wiring and the insulating layer, the polishing composition including: an alicyclic resin acid; a colloidal silica in which a content thereof in the polishing composition is from 0.1 to 1.5% by mass, an average primary particle size thereof is from 10 to 40 nm, an average secondary particle size thereof is from 30 to 80 nm, and (the average secondary particle size×the content) is in a range of from 10 to 40; and tetramethylammonium ion.

## Claims

### Claim 1

A polishing composition used in a step of polishing until a barrier layer adjacent to a copper layer is exposed, in a pattern formation of polishing the copper layer provided on an insulating layer through the barrier layer thereby alternately forming a copper embedded wiring and the insulating layer, the polishing composition comprising:
an alicyclic resin acid;
a colloidal silica in which a content thereof in the polishing composition is from 0.1 to 1.5% by mass, an average primary particle size thereof is from 10 to 40 nm, an average secondary particle size thereof is from 30 to 80 nm, and (the average secondary particle size×the content) is in a range of from 10 to 40; and
tetramethylammonium ion.

### Claim 2 (depends on 1)

The polishing composition according to claim 1, further comprising potassium ion.

### Claim 3 (depends on 1)

The polishing composition according to claim 1, wherein a content of the tetramethylammonium ion in the polishing composition is from 0.1 to 1.4% by mass in terms of tetramethylammonium hydroxide.

### Claim 4 (depends on 2)

The polishing composition according to claim 2, wherein a content of the potassium ion in the polishing composition is 0.6% by mass or less in terms of potassium hydroxide.

### Claim 5 (depends on 2)

The polishing composition according to claim 2, wherein a ratio of the tetramethylammonium ion/the potassium ion is 0.3 or more in terms of tetramethylammonium hydroxide/potassium hydroxide.

### Claim 6 (depends on 1)

The polishing composition according to claim 1, wherein the alicyclic resin acid is rosin.

### Claim 7 (depends on 1)

The polishing composition according to claim 1, further comprising an oxidizing agent.

### Claim 8 (depends on 1)

The polishing composition according to claim 1, further comprising a complex forming agent.

### Claim 9 (depends on 1)

A method for producing a semiconductor integrated circuit device which comprises an insulating layer having a trench and a copper embedded wiring formed in the trench, the method comprising:
polishing a multilayered structure for the semiconductor integrated circuit device, comprising the insulating layer having formed thereon a barrier layer and a copper layer in this order, with the polishing composition according to claim 1 until the barrier layer adjacent to the copper layer is exposed.

### Claim 10 (depends on 9)

The method for producing a semiconductor integrated circuit device according to claim 9, wherein the barrier layer comprises at least one selected from the group consisting of Ta, TaN, Ti, TiN and Ru.

### Claim 11 (depends on 9)

The method for producing a semiconductor integrated circuit device according to claim 9, wherein the multilayered structure comprises a cap layer between the insulating layer and the barrier layer.

### Claim 12 (depends on 9)

The method for producing a semiconductor integrated circuit device according to claim 9, wherein the insulating layer having a trench is a silicon dioxide film or a film having a dielectric constant of 3 or less.