# US 2011/0212590 A1 · High temperature implantation method for stressor formation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0212590 A1
- Document ID: US20110212590A1
- Status: Published application
- Kind: A1
- Application number: 12/713,735
- Filed: 2010-02-26
- Published: 2011-09-01
- Earliest claimed: 2010-02-26
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chii-Ming Wu; Chun-Feng Nieh
- Web page: https://patentgrep.com/patent/US20110212590A1

## CPC

- H10P 30/204: {into Group IV semiconductors}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10P 30/208: {of electrically inactive species}
- H10P 30/225: {of a molecular ion, e.g. decaborane}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

An integrated circuit device and method of fabricating the integrated circuit device is disclosed. According to one of the broader forms of the invention, a method involves providing a semiconductor substrate. A combination of a pre-amorphous implantation process, a high temperature carbon implantation process, and/or an annealing process are performed on the substrate to form a stressor region.

## Claims

### Claim 1

A method comprising:
providing a semiconductor substrate;
performing a pre-amorphous implantation process on the substrate;
performing a high temperature implantation process utilizing a temperature greater than about 200° C. on the substrate; and
performing an annealing process on the substrate.

### Claim 2 (depends on 1)

The method of claim 1 wherein performing the high temperature implantation process includes implanting the substrate with carbon or germanium implant species.

### Claim 3 (depends on 1)

The method of claim 1 wherein performing the high temperature carbon implantation process includes utilizing a temperature from about 500° C. to about 600° C.

### Claim 4 (depends on 1)

The method of claim 1 wherein performing the annealing process includes performing a high temperature annealing process.

### Claim 5 (depends on 4)

The method of claim 4 wherein performing the high temperature annealing process includes utilizing a temperature greater than about 900° C.

### Claim 6 (depends on 4)

The method of claim 4 wherein performing the high temperature annealing process includes performing the annealing process for a few milliseconds (ms) or less.

### Claim 7 (depends on 1)

The method of claim 1 wherein performing the annealing process includes utilizing a rapid thermal annealing process or laser thermal annealing process.

### Claim 8 (depends on 1)

The method of claim 1 wherein performing the pre-amorphous implantation process includes implanting the substrate with a silicon or germanium implant species.

### Claim 9 (depends on 1)

The method of claim 1 wherein performing the pre-amorphous implantation process includes utilizing an implantation energy from about 5 KeV to about 40 KeV.

### Claim 10 (depends on 1)

The method of claim 1 wherein performing the high temperature carbon implantation process includes performing the high temperature implantation process for about 5 minutes.

### Claim 11

A method comprising:
forming a gate structure over a substrate;
forming a source and drain region in the substrate, interposed by the gate structure;
performing a pre-amorphous implantation process on the source and drain region; and
thereafter, performing a high temperature carbon implantation process on the source and drain region.

### Claim 12 (depends on 11)

The method of claim 11 further comprising performing a high temperature annealing process on the substrate.

### Claim 13 (depends on 12)

The method of claim 12 wherein performing the high temperature annealing process includes utilizing a temperature from about 900° C. to about 1,400° C.

### Claim 14 (depends on 12)

The method of claim 12 wherein performing the high temperature annealing process includes performing the annealing process from about 0.8 milliseconds to about 100 milliseconds.

### Claim 15 (depends on 11)

The method of claim 11 wherein performing the high temperature carbon implantation process includes utilizing a temperature greater than room temperature.

### Claim 16 (depends on 15)

The method of claim 15 wherein utilizing the temperature greater than room temperature includes utilizing a temperature from about 200° C. to about 600° C.

### Claim 17 (depends on 11)

The method of claim 11 wherein performing the pre-amorphous implantation process includes implanting the source and drain region with a silicon implant species.

### Claim 18 (depends on 11)

The method of claim 11 wherein performing the high temperature implantation process includes utilizing an implantation dosage of about 1×1013 atoms/cm3 to about 1×1017 atoms/cm3.

### Claim 19

A method comprising:
forming a gate structure over a substrate;
forming a source and drain region in the substrate, adjacent the gate structure;
forming an amorphized region in the source and drain region;
implanting the amorphized region utilizing a temperature greater than about 200° C.; and
thereafter, performing a annealing process at a temperature greater than about 900° C., such that the amorphized region re-crystallizes and forms a stressor region.

### Claim 20 (depends on 19)

The method of claim 19 wherein implanting the amorphized region utilizing the temperature greater than about 200° C. includes implanting the source and drain region with a carbon implant species.

### Claim 21 (depends on 19)

The method of claim 19 wherein forming the stressor region includes forming a SiGe or Si:C stressor region.

### Claim 22 (depends on 19)

The method of claim 19 wherein performing the annealing process includes performing the annealing process for a few milliseconds or less.