# US 2011/0210106 A1 · Method For Laser Fusion Cutting Without Cutting Gas

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0210106 A1
- Document ID: US20110210106A1
- Status: Published application
- Kind: A1
- Application number: 13/049,259
- Filed: 2011-03-16
- Published: 2011-09-01
- Earliest claimed: 2008-09-17
- Assignees: Trumpf Laser GmbH
- Inventors: Peter Schaefer; Peter Olschowsky; Hubertus Melbert
- Web page: https://patentgrep.com/patent/US20110210106A1

## CPC

- B23K 26/38: by boring or cutting
- B23K 26/082: Scanning systems, i.e. devices involving movement of the laser beam relative to the laser head
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method for laser fusion cutting of a metal workpiece including applying a laser beam to the workpiece, where a kerf is melted in the workpiece by the laser beam and a laser beam diameter in a working point is configured to expel molten material from the kerf without cutting gas.

## Claims

### Claim 1

A method for laser fusion cutting of a metal workpiece, comprising:
applying a laser beam to the metal workpiece such that a kerf is melted in the workpiece by the laser beam, wherein the laser beam has a power density of 10 kW/mm2 to 50 kW/mm2 and a diameter sufficient to cause molten material to be expelled from the kerf without cutting gas;
producing at least one gas flow directed towards the workpiece to confine air containing metal vapor generated as a result of the laser contacting the workpiece to an area no greater than 150 mm in front of a point at which the laser beam is contacting the workpiece.

### Claim 2

A method for laser fusion cutting of a metal workpiece, the method comprising:
applying a laser beam to the metal workpiece such that a kerf is melted in the workpiece by the laser beam, wherein the laser beam has a diameter sufficient to expel molten material from the kerf without the use of cutting gas.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the laser beam has a diameter at a working point on the workpiece that is at least approximately 1.5 times larger than a laser beam diameter required at the working point for laser fusion cutting of the workpiece using cutting gas.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the laser beam has a diameter at a working point on the workpiece that is approximately 0.3 mm to approximately 3 mm.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the diameter of the laser beam at the working point on the workpiece is approximately 0.5 mm to approximately 1 mm.

### Claim 6 (depends on 2)

The method according to claim 2, wherein a power density of the laser beam and a feed rate of the laser beam relative to the workpiece allow the molten material to be expelled from the kerf without cutting gas.

### Claim 7 (depends on 2)

The method according to claim 2, wherein a power density of the laser beam and a feed rate of the laser beam relative to the workpiece cause the majority of the molten material to be expelled from a side of the workpiece opposite a source of the laser beam without cutting gas.

### Claim 8 (depends on 2)

The method according to claim 2, wherein a power density of the laser beam is less than to a power density required for laser fusion cutting of the workpiece using cutting gas, and a feed rate of the laser beam relative to the workpiece is the same as a feed rate required for laser fusion cutting of the workpiece.

### Claim 9 (depends on 2)

The method according to claim 2, wherein a power density of the laser beam is 10 kW/mm2 to 50 kW/mm2.

### Claim 10 (depends on 2)

The method according to claim 2, wherein a power density of the laser beam is equal to a power density required for laser welding the workpiece.

### Claim 11 (depends on 2)

The method according claim 2, wherein the feed rate of the laser beam relative to the workpiece is 20% to 70% of a feed rate required for laser welding of the workpiece with the same power density and with a welding depth that is equal to the workpiece thickness.

### Claim 12 (depends on 2)

The method according to claim 2, further comprising providing at least one gas flow to propel gas towards the workpiece.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the at least one gas flow confines ambient air containing metal vapor generated during the laser cutting to within 150 mm in front of a point at which the laser beam contacts the workpiece.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the at least one gas flow has a flow rate that does not influence a processing zone of the workpiece that is contacted by the laser beam.

### Claim 15 (depends on 13)

The method according to claim 13, wherein the at least one gas flow is directed in a beam direction of the laser beam at an inclined angle onto a processing zone of the workpiece that is being contacted by the laser beam.

### Claim 16 (depends on 13)

The method according to claim 13, wherein the at least one gas flow is directed in a beam direction of the laser beam at an inclined angle onto an area in front of a processing zone of the workpiece in which the laser beam contacts the workpiece.

### Claim 17 (depends on 13)

The method according to claim 13, wherein the at least one gas flow is divergently directed onto the laser beam.

### Claim 18 (depends on 13)

The method according to claim 13, wherein the ambient air containing the metal vapor is confined by multiple gas flows that are generated around the laser beam and directed onto an area in front of a processing zone of the workpiece in which the laser beam contacts the workpiece.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the ambient air containing metal vapor generated during laser cutting is extracted by suction.