# US 2011/0209820 A1 · Piezoelectric composite nanofibers, nanotubes, nanojunctions and nanotrees

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0209820 A1
- Document ID: US20110209820A1
- Status: Published application
- Kind: A1
- Application number: 12/806,981
- Filed: 2010-08-25
- Published: 2011-09-01
- Earliest claimed: 2007-08-21
- Inventors: Yong Shi; Shiyou Xu
- Web page: https://patentgrep.com/patent/US20110209820A1

## CPC

- H10N 30/8554: {Lead-zirconium titanate [PZT] based}
- H10N 30/093: Forming inorganic materials
- H10N 30/702: {based on piezoelectric or electrostrictive fibres}
- Y10T 29/42: Piezoelectric device making
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Piezoelectric nanostructures, including nanofibers, nanotubes, nanojunctions and nanotrees, may be made of piezoelectric materials alone, or as composites of piezoelectric materials and electrically-conductive materials. Homogeneous or composite nanofibers and nanotubes may be fabricated by electrospinning. Homogeneous or composite nanotubes, nanojunctions and nanotrees may be fabricated by template-assisted processes in which colloidal suspensions and/or modified sol-gels of the desired materials are deposited sequentially into the pores of a template. The electrospinning or template-assisted fabrication methods may employ a modified sol-gel process for obtaining a perovskite phase in the piezoelectric material at a low annealing temperature.

## Claims

### Claim at position 1

1-18. (canceled)

### Claim 19

A method of fabricating an article that includes piezoelectric fibers having nanoscale diameters using an electrospinninq apparatus having a hollow, electrically-conductive needle, said method comprising the steps of:
selecting a precursor material comprising lead zirconate titanate, poly(vinyl pyrrolidine) and an alcohol, the precursor material being a sol-gel of the lead zirconate titanate;
providing the precursor material to an inlet opening in the needle at a controlled rate, the precursor material flowing from the inlet opening to an outlet opening in the needle, the outlet opening having a micron-scale diameter;
applying a high electrical voltage across the hollow needle and a substrate proximate to the outlet opening, so as to spin a fiber from the needle;
collecting the fiber on the substrate; and
heating the fiber at a temperature of about 80° C. for about 5 minutes, then heating the fiber at a temperature of about 380° C. for about 5 minutes, then maintaining the fiber at a temperature of about 650° C. for about 1 hour, thereby transforming at least a portion of the lead zirconate titanate into crystals having a perovskite structure.

### Claim 20

(canceled)

### Claim 21 (depends on 19)

The method of claim 19, wherein the substrate has a high electrical resistance.

### Claim 22

A method of fabricating an article that includes piezoelectric fibers having nanoscale diameters using an electrospinning apparatus having a hollow, electrically-conductive needle, said method comprising the steps of:
selecting a precursor material that is transformed into a piezoelectric material upon heating and has a sufficiently low viscosity such that the precursor material flows through the hollow needle;
providing the precursor material to an inlet opening in the needle at a controlled rate, the precursor material flowing from the inlet opening to an outlet opening in the needle, the outlet opening having a micron-scale diameter;
applying a high electrical voltage across the needle and a substrate proximate to the outlet opening, so as to spin a fiber from the needle;
collecting the fiber on the substrate; and
heating the fiber, whereby the fiber is transformed into a piezoelectric fiber.

### Claim 23 (depends on 22)

The method of claim 22, wherein the substrate has a high electrical resistance.

### Claim 24 (depends on 22)

The method of claim 22, wherein the precursor material includes lead zirconate titanate, and said heating step includes the step of maintaining the material at a temperature of about 650° C. until at least a portion of the precursor material is transformed into crystals having a perovskite structure.

### Claim 25 (depends on 22)

The method of claim 22, wherein the precursor material is a sol-gel of lead zirconate titanate and said heating step includes the steps of heating the fiber at a temperature of about 80° C. for about 5 minutes, then heating the fiber at a temperature of about 380° C. for about 5 minutes, then maintaining the fiber at a temperature of about 650° C. for about 1 hour, thereby transforming at least a portion of the lead zirconate titanate into crystals having a perovskite structure.

### Claim 26 (depends on 25)

The method of claim 25, wherein the sol gel includes poly(vinyl pyrrolidine) and an alcohol.

### Claim 27 (depends on 22)

The method of claim 22, comprising the further step of depositing an electrically-conductive material on at least a portion of the piezoelectric fiber.

### Claim 28 (depends on 22)

The method of claim 22, wherein the substrate has a trench therein, and said collecting step includes the step of collecting the fiber such that it extends across said trench.

### Claim 29 (depends on 22)

The method of claim 22, wherein the substrate has an electrode thereupon and said collecting step includes the step of applying an electrical voltage at said electrode so as to control the position of the fiber.

### Claim 30 (depends on 22)

The method of claim 22, comprising the further step of depositing a dielectric material on at least a portion of the piezoelectric fiber.

### Claim 31 (depends on 22)

The method of claim 22, wherein the electrospinning device includes a dielectric tube that is within the hollow needle, the dielectric tube having an inlet opening that is hydraulically isolated from the inlet opening and the outlet opening of the hollow needle, whereby said fiber is spun as a hollow fiber.

### Claim 32 (depends on 22)

The method of claim 22, wherein the electrospinning device includes a dielectric tube that is within the hollow needle, the dielectric tube having an inlet opening that is hydraulically isolated from the inlet opening and outlet opening of the hollow needle, the dielectric tube having an outlet opening proximate to the outlet opening of the hollow needle and having a micron-scale diameter, said method comprising the further steps of selecting another precursor material including a substance that is electrically-conductive in a solid state and has a viscosity such that the another precursor material flows through the dielectric tube, providing the another precursor material to the inlet opening in the dielectric tube at a controlled rate during the step of providing the precursor material to the inlet opening in the hollow needle such that the another precursor material moves from the inlet opening in the dielectric tube to the outlet opening in the dielectric tube, and said heating step converting the substance to a solid state, whereby the piezoelectric fiber has a solid electrically-conductive core.

### Claim 33 (depends on 32)

The method of claim 32, wherein the substance includes indium titanium oxide.

### Claim 34 (depends on 32)

The method of claim 32, comprising the further step of depositing an electrically-conductive material on at least a portion of the piezoelectric fiber.

### Claim 35 (depends on 22)

The method of claim 22, wherein the hollow needle is one of a plurality of hollow needles, each hollow needle of the plurality of hollow needles having an outlet opening having a micron-scale diameter and an inlet opening, the plurality of hollow needles being substantially parallel to one another, wherein the precursor material is provided to the inlet opening of each hollow needle of the plurality of hollow needles at a controlled rate during said providing step, so as to spin a plurality of fibers from the plurality of hollow needles.

### Claim 36 (depends on 35)

The method of claim 35, wherein the substrate has an electrode thereupon and said collecting step includes the further step of applying another electrical voltage at the electrode so as to align fibers from the plurality of fibers such that they are substantially parallel with one another.

### Claim 37 (depends on 22)

The method of claim 22, comprising the further step of applying an electrode to the piezoelectric fiber.

### Claim 38 (depends on 37)

The method of claim 37, comprising the further step of applying a dielectric material to the piezoelectric fiber and the electrode.

### Claim 39 (depends on 22)

The method of claim 22, wherein said providing and collecting steps are repeated so as to collect a plurality of fibers on the substrate, and said heating step transforming the plurality of fibers to a plurality of piezoelectric fibers, said method comprising the further steps of forming an electrode across the plurality of piezoelectric fibers and applying a dielectric material to the electrode and the plurality of piezoelectric fibers, thereby encapsulating the electrode and the plurality of piezoelectric fibers with the dielectric material.