# US 2011/0209747 A1 · Polyester film, manufacturing method thereof, polyester film for sealing back face of solar cell, protective film for back face of solar cell, and solar cell module

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0209747 A1
- Document ID: US20110209747A1
- Status: Published application
- Kind: A1
- Application number: 13/035,385
- Filed: 2011-02-25
- Published: 2011-09-01
- Earliest claimed: 2010-02-26
- Assignees: FUJIFILM Corporation
- Inventors: Zemin SHI
- Web page: https://patentgrep.com/patent/US20110209747A1

## CPC

- C08J 5/18: Manufacture of films or sheets
- B29C 48/08: flexible, e.g. films
- B29C 48/91: Heating, e.g. for cross linking
- B29C 48/917: {by applying pressurised gas to the surface of the flat article}
- B29C 48/9175: {by interposing a fluid layer between the supporting means and the flat article}
- B29C 55/143: {firstly parallel to the direction of feed and then transversely thereto}
- B32B 3/085: {spaced apart pieces on the surface of a layer}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/08: of synthetic resin
- B32B 27/306: {comprising vinyl acetate or vinyl alcohol (co)polymers}
- B32B 27/36: comprising polyesters
- H10F 19/85: Protective back sheets
- B29C 48/387: {using a screw extruder and a gear pump}
- B29C 48/914: {Cooling drums}
- B29C 48/9165: {Electrostatic pinning}
- B29K 2067/00: Use of polyesters {or derivatives thereof}, as moulding material
- B29K 2105/256: {Sheets, plates, blanks or films}
- B32B 2255/28: Multiple coating on one surface
- B32B 2307/306: Resistant to heat
- B32B 2307/40: having particular optical properties
- B32B 2307/412: Transparent
- B32B 2307/50: having particular mechanical properties
- B32B 2307/518: bi-axially
- B32B 2307/704: Crystalline
- B32B 2307/712: Weather resistant
- B32B 2307/714: Inert, i.e. inert to chemical degradation, corrosion
- B32B 2307/732: Dimensional properties
- B32B 2307/734: Dimensional stability
- B32B 2457/12: Photovoltaic modules
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- Y02E 10/50: Photovoltaic [PV] energy
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A biaxially oriented polyester film having: an equilibrium moisture content of from 0.1% by mass to 0.25% by mass; a difference between moisture contents measured at 10 cm intervals of from 0.01% by mass to 0.06% by mass; a degree of crystallinity of from 30% to 40%; a concentration of terminal carboxyl groups of from 5 equivalents/ton to 25 equivalents/ton; and a thickness of from 100 μm to 350 μm.

## Claims

### Claim 1

A biaxially oriented polyester film having:
an equilibrium moisture content of from 0.1% by mass to 0.25% by mass;
a difference between moisture contents measured at 10 cm intervals of from 0.01% by mass to 0.06% by mass;
a degree of crystallinity of from 30% to 40%;
a concentration of terminal carboxyl groups of from 5 equivalents/ton to 25 equivalents/ton; and
a thickness of from 100 μm to 350 μm.

### Claim 2 (depends on 1)

The polyester film according to claim 1, having a thickness of from 255 μm to 350 μm.

### Claim 3 (depends on 1)

The polyester film according to claim 1, having an intrinsic viscosity of from 0.6 to 1.3.

### Claim 4 (depends on 1)

The polyester film according to claim 1, wherein an increase in the concentration of terminal carboxyl groups after performing an 80-hour long thermal treatment under an environment of 120° C. and 100% RH is from 30 equivalents/ton to 65 equivalents/ton.

### Claim 5

A manufacturing method of a polyester film, comprising:
cooling a molten film-shaped polyester extruded from an extrusion die at a rate of from 250° C./min to 800° C./min; and
performing a longitudinal stretching in a length direction with a stretching stress of from 5 MPa to 15 MPa and a stretch ratio of from 2.5 times to 4.5 times, and a transverse stretching in a width direction, on the cooled film-shaped polyester, so that a thickness of the polyester film after the longitudinal stretching and the transverse stretching becomes from 100 μm to 350 μm.

### Claim 6 (depends on 5)

The manufacturing method of a polyester film according to claim 5, wherein the thickness of the polyester film after the longitudinal stretching and the transverse stretching becomes from 255 μm to 350 μm.

### Claim 7 (depends on 5)

The manufacturing method of a polyester film according to claim 5, wherein the molten film-shaped polyester is cooled by a cast roll.

### Claim 8 (depends on 5)

The manufacturing method of a polyester film according to claim 5, wherein the transverse stretching is performed with a stretching stress of from 8 MPa to 20 MPa and a stretch ratio of from 3.4 times to 4.5 times.

### Claim 9 (depends on 5)

The manufacturing method of a polyester film according to claim 5, further comprising, after the longitudinal stretching and the transverse stretching, performing a heat setting treatment on the polyester film with a tensile strength of from 1 kg/m to 10 kg/m and at a temperature of from 210° C. to 230° C.

### Claim 10 (depends on 5)

The manufacturing method of a polyester film according to claim 5, wherein solid-phase polymerized pellets are used as a polyester to be extruded from the extrusion die.

### Claim 11 (depends on 5)

A polyester film for sealing a back face of a solar cell, which is a polyester film manufactured by the manufacturing method according to claim 5.

### Claim 12 (depends on 1)

A protective film for a back face of a solar cell, comprising the polyester film according to claim 1.

### Claim 13 (depends on 1)

A solar cell module comprising the polyester film according to claim 1.