# US 2011/0209590 A1 · Method of making a coated cemented carbide insert

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0209590 A1
- Document ID: US20110209590A1
- Status: Published application
- Kind: A1
- Application number: 13/105,300
- Filed: 2011-05-11
- Published: 2011-09-01
- Earliest claimed: 2007-07-13
- Assignees: Seco Tools AB
- Inventors: Erik SUNDSTROM; Jacob SJOLEN; Niklas AHLEN
- Web page: https://patentgrep.com/patent/US20110209590A1

## CPC

- C23C 30/005: {on hard metal substrates}
- B22F 7/06: of composite workpieces or articles from parts, e.g. to form tipped tools {(B22F7/002 takes precedence)}
- C22C 29/08: based on tungsten carbide
- B22F 2005/001: {Cutting tools, earth boring or grinding tool other than table ware}
- B23B 2222/28: Details of hard metal, i.e. cemented carbide
- B23B 2228/08: applied by physical vapour deposition [PVD]
- B23B 2228/10: Coatings
- Y10T 82/10: Process of turning
- Y10T 407/27: comprising tool of specific chemical composition
- Y10T 408/78: Tool of specific diverse material
- Y10T 428/265: 1 mil or less
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B23B: TURNING; BORING (arrangements for copying or controlling B23Q)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Forming coated cemented carbide inserts, particularly useful in fine turning of super alloys. The inserts are characterized by a composition of a cemented carbide of WC, about 4.0 wt-% Co to about 7.0 wt-% Co, about 0.25 wt-% Cr to 0.50 wt-% Cr, and a coercivity (Hc) of about 28 kA/m to about 38 kA/m. The coating comprises a single (Ti1-xSix)N-layer, where x is between about 0.1 and about 0.25, with a crystal structure of NaCl type and a total thickness between about 0.5 μm and about 2.0 μm with a strong (200)-texture.

## Claims

### Claim 1

A method for making a cutting tool insert having a flank face, comprising a cemented carbide body and a coating, comprising the steps of:
providing a substrate made by conventional powder metallurgical methods milling, pressing, and sintering with a composition comprising:
tungsten carbide (WC);
about 4.0 wt-% to about 7.0 wt-% cobalt (Co);
about 0.25 wt-% to about 0.50 wt-% chromium (Cr); and
wherein said composition has a coercivity, Hc, of about 28 kA/m to about 38 kA/m; and
depositing a single layer, comprising (Ti1-xSix)N, wherein x is between about 0.1 and about 0.25;
wherein said layer has a crystal structure of NaCl type and a total thickness of between 0.5 μm and 2.0 μm measured on the middle of said flank face;
wherein said layer has a texture coefficient TC(200)>about 1.5, the texture coefficient (TC) being defined as:
TC

(
hkl
)
=
I

(
hkl
)
I
0

(
hkl
)
[
1
n

∑
n
=
1
n


I

(
hkl
)
I
0

(
hkl
)
]
-
1
where:
I(hkl)=intensity of the (hkl) reflection;
IO(hkl)=standard intensity according to JCPDS card no 38-1420;
n=number of reflections used in the calculation;
(hkl) reflections used are: (111), (200), (220),
using arc evaporation of an alloyed, or Ti+Si composition cathode having a composition comprising:
about 60 at-% Ti to about 90 at-% Ti, and balance Si;
with an evaporation current of between about 50 A and about 200 A and a substrate bias of between about −10 V and about −150 V, and a deposition temperature of between about 400° C. and about 700° C., and grown in an Ar+N2 atmosphere comprising about 0 vol-% Ar to about 50 vol-% Ar, at a total pressure of about 0.5 Pa to about 9.0 Pa.

### Claim 2 (depends on 1)

The method of claim 1, wherein said Co is present at a level of about 4.5 wt-% to about 6.0 wt-%.

### Claim 3 (depends on 1)

The method of claim 1, wherein said Cr is present at a level of about 0.30 wt-% to about 0.45 wt-%.

### Claim 4 (depends on 1)

The method of claim 1, wherein said cemented carbide body has a coercivity, Hc, of about 30 kA/m to about 36 kA/m.

### Claim 5 (depends on 1)

The method of claim 1, wherein x is between about 0.12 and about 0.23.

### Claim 6 (depends on 1)

The method of claim 1, wherein said layer has a total thickness between about 0.7 μm and about 1.5 μm, measured on the middle of the flank face.

### Claim 7 (depends on 1)

The method of claim 1, wherein said layer has a texture coefficient TC(200)>about 2.0.

### Claim 8 (depends on 1)

The method of claim 1, wherein said insert is edge-honed by wet-blasting to an edge radius of between about 0 μm and about 25 μm before said insert is coated.

### Claim 9 (depends on 1)

The method of claim 1, said alloyed, or Ti+Si composite cathode having a composition comprises about 70 at-% Ti to about 90 at-% Ti.

### Claim 10 (depends on 1)

The method of claim 1, wherein said substrate bias is between about −40 V and about −70 V.

### Claim 11 (depends on 1)

The method of claim 1, wherein said deposition temperature is between about 500° C. and about 700° C.

### Claim 12 (depends on 1)

The method of claim 1, wherein said Ar+N2 atmosphere comprises about 0 vol-% Ar to about 20 vol-% Ar.

### Claim 13 (depends on 1)

The method of claim 1, wherein said total pressure is about 1.5 Pa to about 5.0 Pa.

### Claim 14

A method for fine wet turning of a superalloy, comprising the steps of:
providing an insert, said insert comprising:
a. a cemented carbide body having an edge radius, comprising:
tungsten carbide (WC);
about 4.0 wt-% to about 7.0 wt-% cobalt (Co);
about 0.25 wt-% to about 0.50 wt-% chromium (Cr); and
wherein said cemented carbide body has a coercivity, Hc, of about 28 kA/m to about 38 kA/m; and
a single layer coating comprising (Ti1-xSix)N, wherein x is between about 0.1 and about 0.25;
wherein said layer has a crystal structure of NaCl type and a total thickness of between 0.5 μm and 2.0 μm measured on the middle of said flank face;
wherein said layer has a texture coefficient TC(200)>about 1.5, the texture coefficient (TC) being defined as:
TC

(
hkl
)
=
I

(
hkl
)
I
0

(
hkl
)
[
1
n

∑
n
=
1
n


I

(
hkl
)
I
0

(
hkl
)
]
-
1
where:
I(hkl)=intensity of the (hkl) reflection;
IO(hkl)=standard intensity according to JCPDS card no 38-1420;
n=number of reflections used in the calculation;
(hkl) reflections used are: (111), (200), (220); and
wet cutting said superalloy with said insert at a cutting speed of about 35 m/min to about 130 m/min, a cutting depth of about 0.1 mm to about 0.75 mm, and a feed of about 0.05 mm/rev to about 0.25 mm/rev.

### Claim 15 (depends on 14)

The method of claim 14, wherein said superalloy is Inconel 718, Inconel 625, Nimonic 81, Waspaloy, Ti6A14V, or a combination thereof.