# US 2011/0177240 A1 · Method for producing antiglare film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0177240 A1
- Document ID: US20110177240A1
- Status: Published application
- Kind: A1
- Application number: 13/121,386
- Filed: 2009-09-29
- Published: 2011-07-21
- Earliest claimed: 2008-09-29
- Assignees: FUJIFILM Corporation
- Inventors: Yuuki Saiki; Kazuhiro Shiojiri; Kazuhiro Oki
- Web page: https://patentgrep.com/patent/US20110177240A1

## CPC

- G02B 1/111: using layers comprising organic materials
- G02B 5/0215: {the surface having a regular structure}
- B05D 1/265: {Extrusion coatings}
- B05D 7/5385: {the two layers being applied simultaneously}
- B05D 2201/02: Polymeric substrate
- B05D 2252/02: of indefinite length
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

A method for producing an antiglare film includes: a step of preparing coating liquids comprising components capable of being unevenly distributed in an antiglare layer-forming coating liquid and a low-refractive index layer-forming coating liquid, respectively; a coating step of applying the low-refractive index layer-forming coating liquid as an upper layer and the antiglare layer-forming coating liquid as a lower layer on a support to form a coating layer; and a drying step of drying the coating layer and making the coating layer cause phase-separation so as to unevenly distribute the components and form an antiglare layer and a low-refractive index layer. By the production method, an antiglare film which suppresses reflection and glaring of external light in a display and whitening due to irregular reflection can be produced at a low cost.

## Claims

### Claim 1

A method for producing an antiglare film, comprising:
a step of preparing coating liquids comprising components capable of being unevenly distributed in an antiglare layer-forming coating liquid and a low-refractive index layer-forming coating liquid, respectively;
a coating step of applying the low-refractive index layer-forming coating liquid as an upper layer and the antiglare layer-forming coating liquid as a lower layer on a support to form a coating layer; and
a drying step of drying the coating layer and making the coating layer cause phase-separation so as to unevenly distribute the components and form an antiglare layer and a low-refractive index layer.

### Claim 2

A method for producing an antiglare film, comprising:
a step of preparing at least one antiglare layer-forming coating liquid in which at least two resin materials incompatible with each other are dissolved in at least one solvent, and a low-refractive index layer-forming coating liquid in which a resin material and hydrophobic particles are dissolved in a solvent;
a coating step of applying the low-refractive index layer-forming coating liquid as an upper layer and the antiglare layer-forming coating liquid as a lower layer on a support to form a coating layer;
a particle movement step of moving the particles to a gas-liquid interface of the coating layer; and
a drying step of drying the coating layer and making the coating layer cause phase-separation so as to form an antiglare layer and a low-refractive index layer.

### Claim 3 (depends on 2)

The method for producing an antiglare film according to claim 2, wherein 80% or more of the particles in the low-refractive index layer-forming coating liquid are contained in the low-refractive index layer.

### Claim 4 (depends on 2)

The method for producing an antiglare film according to claim 2, wherein, when a ratio of the particles to the solvent in the low-refractive index layer-forming coating liquid is represented by r [-], a time until the solvent decreases to half in the drying step is represented by t [s], and an initial film thickness of the upper layer in the coating step is represented by d [m], the factors, r, t and d, are adjusted so that multiplication of 1/r and t and d satisfies 6×10−2 or more.

### Claim 5

A method for producing an antiglare film, comprising:
a coating liquid preparation step of preparing an antiglare layer-forming coating liquid in which at least two resin materials incompatible with each other are dissolved in at least one solvent, and a low-refractive index layer-forming coating liquid in which a first polymer whose substituent contains a molecular structure to decrease a refractive index of whole polymer and one or more resin materials which form a phase-separation structure with the first polymer are dissolved in at least one solvent;
a coating step of applying the low-refractive index layer-forming coating liquid as an upper layer and the antiglare layer-forming coating liquid as a lower layer on a support to form a coating layer; and
a drying step of drying the coating layer making the low-refractive index layer-forming coating liquid and the antiglare layer-forming coating liquid cause phase-separation so as to form a low-refractive index layer and an antiglare layer.

### Claim 6 (depends on 5)

The method for producing an antiglare film according to claim 5, wherein the molecular structure to decrease the refractive index of the whole polymer, which is contained in the substituent contained in the first polymer is a molecular structure containing a fluorine molecule.

### Claim 7 (depends on 5)

The method for producing an antiglare film according to claim 5, wherein a ratio of the first polymer and the resin material to the solvent in the low-refractive index layer-forming coating liquid, and a ratio of the resin materials to the solvent in the antiglare layer-forming coating liquid are adjusted in the coating liquid preparation step so that an initiation of the phase separation of the low-refractive index layer-forming coating liquid is earlier than an initiation of the phase separation of the antiglare layer-forming coating liquid in the drying step.

### Claim 8 (depends on 7)

The method for producing an antiglare film according to claim 7, wherein the ratio of the first polymer and the resin material to the solvent in the low-refractive index layer-forming coating liquid, and the ratio of the resin materials to the solvent in the antiglare layer-forming coating liquid are adjusted in the coating liquid preparation step so that the initiation of the phase separation of the antiglare layer-forming coating liquid is later than an initiation of spinodal decomposition of the low-refractive index layer-forming coating liquid in the drying step.

### Claim 9 (depends on 1)

The method for producing an antiglare film according to claim 1, wherein the upper layer and the lower layer are simultaneously applied as a multi-layer in the coating step.