# US 2011/0162196 A1 · Process for making high electrical conductivity aluminium plates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0162196 A1
- Document ID: US20110162196A1
- Status: Published application
- Kind: A1
- Application number: 13/063,099
- Filed: 2009-09-10
- Published: 2011-07-07
- Earliest claimed: 2008-09-10
- Assignees: 9128-5270 Quebec Inc.
- Inventors: Michel Lavoie
- Web page: https://patentgrep.com/patent/US20110162196A1

## CPC

- C22F 1/04: of aluminium or alloys based thereon
- C25C 3/16: Electric current supply devices, e.g. bus bars
- H01B 1/023: {Alloys based on aluminium}
- Y10T 29/49002: Electrical device making
- Y10T 29/49975: Removing defects
- Y10T 29/49989: Followed by cutting or removing material
- Y10T 83/04: Processes
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The process can include obtaining a rectangular aluminium panel size; obtaining a cast aluminium ingot having a length and width housing said aluminium panel size; sawing the annealed aluminium ingot along its length and across its width, thereby yielding a plurality of aluminium panels having said aluminium panel size and a given plate thickness; and cutting the plates across the thickness of the aluminium panels.

## Claims

### Claim 1

A process of making bus plates for a current-carrying bus bar assembly, the process comprising:
a. Obtaining a rectangular aluminium panel size;
b. Obtaining an annealed aluminium ingot having a length and width specifically sized to house said aluminium panel size;
c. Sawing the annealed aluminium ingot along its length and across its width, thereby yielding a plurality of aluminium panels having said aluminium panel size and a given bus plate thickness;
d. Cutting the bus plates across the thickness of the aluminium panels.

### Claim 2 (depends on 1)

The process of claim 1, further comprising removing a header and footer of the aluminium ingot prior to said sawing.

### Claim 3 (depends on 1)

The process of claim 1, further comprising obtaining a two-dimensional nested pattern of said bus plates, wherein the rectangular panel size obtained in step a. is selected to contain the two-dimensional nested pattern.

### Claim 4 (depends on 3)

The process of claim 3, wherein in step d. the bus plates are cut according to said two-dimensional nesting pattern.

### Claim 5 (depends on 1)

The process of claim 1, wherein step b. includes casting the aluminium ingot, the casting including adapting the width of a mould for the aluminium ingot to house the width of the rectangular aluminium panel size.

### Claim 6 (depends on 1)

The process of claim 1, wherein step b. includes annealing the aluminium ingot, the annealing including in sequence: raising the temperature of the ingot from room temperature to 460±50° C. on a period of 4±2 hours; maintaining the temperature at 460±50° C. during 30±5 hours; reducing the temperature from 460±50° C. to 250±25° C. during 14±3 hours; and returning the ingot to room temperature.

### Claim 7 (depends on 1)

The process of claim 1, further comprising removing a crust of said cast aluminium ingot prior to said sawing.

### Claim 8 (depends on 1)

The process of claim 1 wherein said aluminium ingot is of aluminium from the 1000′ series.

### Claim 9 (depends on 1)

The process of claim 1 wherein the aluminium panels have a thickness between 5 mm and 50 mm.

### Claim 10 (depends on 9)

The process of claim 9 wherein the thickness of the aluminium panels is within a tolerance of 0.35 mm.

### Claim 11 (depends on 9)

The process of claim 9 wherein the aluminium panels have a planarity of within 0.9 mm/m2.

### Claim 12 (depends on 1)

The process of claim 1, further comprising assembling a plurality of said plates in a stacked arrangement into a bus bar component.

### Claim 13 (depends on 1)

The process of claim 1, further comprising soldering at least one of said plates to other components of a bus bar.

### Claim 14

A process of making high electrical conductivity plates for use in a stacked arrangement as part of a component of an electrical conductor network, the process comprising:
Obtaining a non-overlapping nested two-dimensional pattern of shapes of said plates,
Selecting a width and length of a rectangular aluminium panel size appropriate for housing said nested two-dimensional pattern with a low amount of waste;
Obtaining a cast and subsequently annealed aluminium ingot of the 1000′ series having a width and length selected to house aluminium panels having the selected rectangular panel size;
Sawing a crust off faces of said ingot;
Sawing said ingot into a plurality of rectangular aluminium panels having the rectangular aluminium panel size; and
Cutting said nested two-dimensional pattern of plates in said panels, thereby yielding the plates.

### Claim 15 (depends on 14)

The process of claim 14, further comprising removing a header and footer of the cast aluminium ingot prior to said sawing.

### Claim 16 (depends on 14)

The process of claim 14, wherein the aluminium ingot is annealed in the following sequence: raising the temperature of the ingot from room temperature to 460±50° C. on a period of 4±2 hours; maintaining the temperature at 460±50° C. during 30±5 hours; reducing the temperature from 460±50° C. to 250±25° C. during 14±3 hours; and returning the ingot to room temperature.

### Claim 17

(canceled)

### Claim 18

A process of making high electrical conductivity plates for use in a stacked arrangement in a connector of a large conductor network, including cutting the plates from aluminium panels having given planarity and thickness tolerances, the process being characterized in that the aluminium panels are obtained by sawing an aluminium ingot.

### Claim 19 (depends on 18)

The process of claim 18 further characterized in that a size of the aluminium panels is determined based on a previously determined nesting pattern of plates, and in that the ingot has a size corresponding to the determined aluminium panel size.

### Claim 20 (depends on 19)

The process of claim 19 further characterized in that said plates are cut into said aluminium panels according to said nesting pattern.

### Claim 21

(canceled)

### Claim 22 (depends on 18)

The process of claim 18, wherein the aluminium ingot is annealed prior to sawing, in the following sequence: raising the temperature of the ingot from room temperature to 460±50° C. on a period of 4±2 hours; maintaining the temperature at 460±50° C. during 30±5 hours; reducing the temperature from 460±50° C. to 250±25° C. during 14±3 hours; and returning the ingot to room temperature.

### Claim 23

(canceled)

### Claim 24

(canceled)