# US 2011/0135557 A1 · Hardmask materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0135557 A1
- Document ID: US20110135557A1
- Status: Published application
- Kind: A1
- Application number: 12/631,691
- Filed: 2009-12-04
- Published: 2011-06-09
- Earliest claimed: 2009-12-04
- Assignees: Novellus Systems, Inc.
- Inventors: Vishwanathan Rangarajan; George Andrew Antonelli; Ananda Banerji; Bart van Schravendijk
- Web page: https://patentgrep.com/patent/US20110135557A1

## CPC

- H10P 14/6336: {in the presence of a plasma [PECVD]}
- C23C 16/30: Deposition of compounds, mixtures or solid solutions, e.g. borides, carbides, nitrides
- C23C 16/325: {Silicon carbide}
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C23C 16/505: using radio frequency discharges
- C23C 16/56: After-treatment
- H01J 37/32091: {the radio frequency energy being capacitively coupled to the plasma}
- H01J 37/32165: {Plural frequencies}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/68: Organic materials, e.g. photoresists
- H10P 50/71: {using masks for conductive or resistive materials}
- H10P 50/73: {using masks for insulating materials}
- H10P 72/0402: {Apparatus for fluid treatment (H10P72/0441, H10P72/0448 take precedence)}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10W 20/088: {involving partial etching of via holes}
- H10P 14/6905: {being a silicon carbide or silicon carbonitride and not containing oxygen, e.g. SiC or SiC:H}
- Y10S 438/932: Boron nitride semiconductor
- Y10S 438/942: Masking
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Hardmask films having high hardness and low stress are provided. In some embodiments a film has a stress of between about −600 MPa and 600 MPa and hardness of at least about 12 GPa. In some embodiments, a hardmask film is prepared by depositing multiple sub-layers of doped or undoped silicon carbide using multiple densifying plasma post-treatments in a PECVD process chamber. In some embodiments, a hardmask film includes a high-hardness boron-containing film selected from the group consisting of SixByCz, SixByNz, SixByCzNw, BxCy, and BxNy. In some embodiments, a hardmask film includes a germanium-rich GeNx material comprising at least about 60 atomic % of germanium. These hardmasks can be used in a number of back-end and front-end processing schemes in integrated circuit fabrication.

## Claims

### Claim 1

A method of forming a hardmask film on a semiconductor substrate, the method comprising:
receiving a semiconductor substrate in a plasma-enhanced chemical vapor deposition (PECVD) process chamber; and
forming a hardmask film having a hardness of greater than about 12 GPa, and a stress of between about −600 MPa and 600 MPa by PECVD, wherein the PECVD hardmask deposition process comprises a process selected from the group consisting of:
(i) depositing doped or undoped multi-layer silicon carbide film using multiple densifying plasma treatments; and
(ii) depositing a high-hardness boron-containing film selected from the group consisting of SixByCz, SixByNz, SixByCzNw, BxNy, and BxCy.

### Claim 2 (depends on 1)

The method of claim 1, wherein the film has a stress of between about −300 MPa and 300 MPa.

### Claim 3 (depends on 1)

The method of claim 1, wherein the film has a stress of between about 0 MPa and 600 MPa.

### Claim 4 (depends on 1)

The method of claim 1, wherein the film has a hardness of at least about 16 GPa.

### Claim 5 (depends on 1)

The method of claim 1, wherein the film has a modulus of at least about 100 GPa.

### Claim 6 (depends on 1)

The method of claim 1, wherein (i) comprises:
(a) introducing a process gas comprising a silicon-containing precursor into the process chamber and forming a plasma to deposit a first sublayer of the silicon carbide hardmask film;
(b) removing the silicon-containing precursor from the process chamber;
(c) introducing a plasma treatment gas into the process chamber and treating the substrate with plasma to densify the deposited sublayer; and
(d) repeating (a)-(c) to form and densify additional sublayers of silicon carbide.

### Claim 7 (depends on 6)

The method of claim 6, wherein the silicon carbide is undoped and wherein the silicon-containing precursor is a saturated precursor.

### Claim 8 (depends on 6)

The method of claim 6, wherein the silicon-containing precursor comprises tetramethylsilane (Me4Si).

### Claim 9 (depends on 6)

The method of claim 6, wherein the process gas used during deposition further comprises a carrier gas selected from the group consisting of He, Ne, Ar, Kr, and Xe.

### Claim 10 (depends on 6)

The method of claim 6, wherein the plasma treatment gas is selected from the group consisting of He, Ar, CO2, N2, NH3, and H2.

### Claim 11 (depends on 6)

The method of claim 6, wherein the thickness of each sublayer is less than about 100 Å.

### Claim 12 (depends on 11)

The method of claim 11, wherein the method comprises depositing at least 10 sublayers.

### Claim 13 (depends on 6)

The method of claim 6, wherein
depositing the silicon carbide sublayer comprises flowing a process gas comprising Me4Si and an inert gas and forming a dual frequency plasma, wherein the power level for high frequency plasma is between about 0.04 to 0.2 W/cm2 and the power level for low-frequency plasma is between about 0.17 to 0.6 W/cm2;
removing the silicon carbide precursor comprises purging the process chamber with a gas selected from the group consisting of Ar, He, H2, and mixtures thereof; and
densifying the sublayers comprises flowing a process gas selected from the group consisting of Ar, He, H2, and mixtures thereof and forming a dual frequency plasma, wherein LF/HF power ratio is at least about 1.5.

### Claim 14 (depends on 6)

The method of claim 6, wherein in the formed silicon carbide film the ratio of areas of SiC peak in the IR spectrum relative to SiH is at least about 20 and the ratio of areas of SiC peak in the IR spectrum relative to CH is at least about 50.

### Claim 15 (depends on 6)

The method of claim 6, wherein the formed silicon carbide film has a density of at least about 2 g/cm3.

### Claim 16 (depends on 1)

The method of claim 1, wherein (ii) comprises depositing high-hardness SixByCz film, and wherein the deposition comprises:
flowing a process gas comprising a boron-containing precursor, a silicon-containing precursor and a carrier gas into the process chamber; and
forming a dual frequency plasma, wherein LF/HF power ratio is at least about 1.5,
to deposit a high-hardness SixByCz film on the substrate.

### Claim 17 (depends on 16)

The method of claim 16, wherein the formed high-hardness SixByCz film has a ratio of IR peak areas for BC/[BC+SiC] of at least about 0.35.

### Claim 18 (depends on 1)

The method of claim 1, wherein the formed hardmask layer is deposited over a layer of dielectric having a dielectric constant of less than about 2.8, and wherein the formed hardmask film has an etch selectivity of at least about 8:1 versus the dielectric in a dry plasma etch.

### Claim 19 (depends on 1)

The method of claim 1, wherein the formed hardmask layer is deposited over a layer of polysilicon.

### Claim 20 (depends on 1)

The method of claim 1, wherein the hardmask is formed at a temperature of less than about 400° C.

### Claim 21 (depends on 1)

The method of claim 1, wherein (ii) comprises forming a high-hardness SixByCzNw film.

### Claim 22

A film comprising doped or undoped silicon carbide having hardness of at least about 12 GPa and a stress of between about −600 MPa and 600 MPa.

### Claim 23

An apparatus for depositing a hardmask film, the apparatus comprising:
(a) a process chamber configured for formation of plasma;
(b) a support for a wafer substrate configured for holding the wafer substrate in position during hardmask deposition, and
(c) a controller comprising program instructions for a process selected from the group consisting of:
(i) depositing doped or undoped multi-layer silicon carbide film using multiple densifying plasma treatments; and
(ii) depositing a high-hardness boron-containing film selected from the group consisting of SixByCz, SixByNz, SixByCzNw, BxNy, and BxCy.