# US 2011/0133138 A1 · Method for producing coating solution for use in solar collector modules and coating composition produced by the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0133138 A1
- Document ID: US20110133138A1
- Status: Published application
- Kind: A1
- Application number: 12/852,641
- Filed: 2010-08-09
- Published: 2011-06-09
- Earliest claimed: 2009-12-07
- Assignees: Hytc Co., Ltd.
- Inventors: Yook-Jung KIM; Jin-Ho JANG
- Web page: https://patentgrep.com/patent/US20110133138A1

## CPC

- C03C 1/008: {for the production of films or coatings}
- C03C 17/02: with glass (C03C17/34, C03C17/44 take precedence)
- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- C09D 183/04: Polysiloxanes
- C03C 2203/26: using alkoxides
- C03C 2203/30: Additives
- C03C 2203/32: Catalysts
- C03C 2217/732: made of a single layer
- C03C 2218/113: by sol-gel processes
- Y02E 10/50: Photovoltaic [PV] energy
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

There is provided a method for producing a coating solution used on glass for solar collector modules to enhance optical transmittance, comprising: preparing a sol of particles having a diameter of about ten nanometers to about several hundred nanometers by adding a coagulation-inducing agent to a coating solution to induce coagulation of the coating solution by the sol-gel reaction, wherein the coagulation-inducing agent reacts with aluminum alkoxide.

## Claims

### Claim 1

A method for producing a coating solution used on glass for solar collector modules, comprising:
preparing a sol of particles having a diameter of about ten nanometers to about several hundred nanometers by adding a coagulation-inducing agent to a coating solution to induce coagulation of the coating solution by the sol-gel reaction, wherein the coagulation-inducing agent reacts with aluminum alkoxide.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the coagulation-inducing agent comprises at least one selected from the group consisting of a silica sol and an alumina sol.

### Claim 3 (depends on 2)

The method according to claim 2, further comprising:
adding a stabilizing agent to the sol prepared in the sol preparation step.

### Claim 4 (depends on 3)

The method according to claim 3, further comprising:
subjecting the sol prepared in the sol stabilization step to a sol-gel reaction with a metal alkoxide after the sol stabilization step.

### Claim 5 (depends on 4)

The method according to claim 4, further comprising:
mixing about 100 parts by weight of the silica sol with about 10 to about 40 parts by weight of the alumina sol when both silica sol and alumina sol comprise the coagulation-inducing agent.

### Claim 6 (depends on 5)

The method according to claim 5, further comprising:
adding an acidic catalyst to lower the pH into an acidic range when the coagulation-inducing agent is basic, wherein the sol-gel reaction is performed at a temperature of about 50° C. to about 80° C.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the silica sol comprises particles of about 10 nm to about 200 nm in diameter.

### Claim 8 (depends on 6)

The method according to claim 6, wherein the alumina sol comprises particles of about 10 nm to about 200 nm in diameter.

### Claim 9 (depends on 2)

The method according to claim 2, wherein the coagulated particles have a diameter of about 100 nm to about 500 nm.

### Claim 10

A method for producing a coating solution used on glass for solar collector modules to enhance optical transmittance, comprising:
preparing a sol of particles having a diameter of about ten nanometers to about several hundred nanometers by adding a coagulation-inducing agent to a coating solution to induce coagulation of the coating solution by the sol-gel reaction,
adding a stabilizing agent to the sol prepared in the sol preparation step,
subjecting the sol prepared in the sol stabilization step to a sol-gel reaction with a metal alkoxide after the sol stabilization step,
mixing about 100 parts by weight of the silica sol with about 10 to about 40 parts by weight of the alumina sol when both silica sol and alumina sol comprise the coagulation-inducing agent, and
adding an acidic catalyst to lower the pH into an acidic range when the coagulation-inducing agent is basic,
wherein the coagulation-inducing agent reacts with aluminum alkoxide and comprises at least one selected from the group consisting of a silica sol and an alumina sol, and
wherein the sol-gel reaction is performed at a temperature of about 50° C. to about 80° C.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the sol comprises particles of about 10 nm to about 200 nm in diameter.

### Claim 12 (depends on 4)

An anti-reflective coating composition comprising the sol prepared by the method of claim 4, water, an organic solvent, and a catalyst, wherein the metal alkoxide is an alkoxysilane.

### Claim 13 (depends on 12)

The anti-reflective coating composition of claim 12, wherein the method further comprises mixing about 100 parts by weight of the silica sol with about 10 to about 40 parts by weight of the alumina sol when both silica sol and alumina sol comprise the coagulation-inducing agent.

### Claim 14 (depends on 13)

The anti-reflective coating composition of claim 13, wherein the method further comprises adding an acidic catalyst to lower the pH into an acidic range when the coagulation-inducing agent is basic, wherein the sol-gel reaction is performed at a temperature of about 50° C. to about 80° C.

### Claim 15 (depends on 14)

The anti-reflective coating composition of claim 14, wherein the silica sol comprises particles of about 10 nm to about 200 nm in diameter.

### Claim 16 (depends on 15)

The anti-reflective coating composition of claim 15, wherein the alumina sol comprises particles of about 10 nm to about 200 nm in diameter.

### Claim 17 (depends on 10)

An anti-reflective coating composition comprising the sol prepared by the method of claim 10, water, an organic solvent, and a catalyst, wherein the metal alkoxide is an alkoxysilane.