# US 2011/0111259 A1 · Low-Field Magnetic Domain Wall Injection Pad and High-Density Storage Wire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0111259 A1
- Document ID: US20110111259A1
- Status: Published application
- Kind: A1
- Application number: 12/945,127
- Filed: 2010-11-12
- Published: 2011-05-12
- Earliest claimed: 2009-11-12
- Assignees: Marquette University
- Inventors: Andrew Kunz
- Web page: https://patentgrep.com/patent/US20110111259A1

## CPC

- G11B 5/642: {self supporting magnetic material, e.g. magnetisable wires}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- G11C 11/14: using thin-film elements
- G11C 19/0808: {using magnetic domain propagation}
- G11C 19/0816: {using a rotating or alternating coplanar magnetic field}
- Y10T 428/32: Composite [nonstructural laminate] of inorganic material having metal-compound-containing layer and having defined magnetic layer
- Y10T 428/325: Magnetic layer next to second metal compound-containing layer
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- G11C: STATIC STORES (semiconductor memory devices H10B)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Disclosed herein are magnetic storage devices and uses therefor. The devices comprise an injection pad and a nanowire extending from an outer edge of the injection pad. The injection pad and the nanowire of the disclosed magnetic storage devices have a geometry that is designed to optimize high density memory storage via low magnetic field domain wall shifting. The devices may be utilized, for example, for generating and storing magnetic domain walls for application in memory devices, sensor devices, and logic devices.

## Claims

### Claim 1

A magnetic storage device comprising:
(a) an injection pad; and
(b) a nanowire extending tangentially along an X-axis from an outer edge of the injection pad;
wherein:
the injection pad and nanowire comprise magnetic metal material and are monolithic;
the nanowire has a top width of 20-200 nm extending along a Y-axis perpendicular to the X-axis;
the injection pad has a top surface area parallel to a plane defined by the X-axis and the Y-axis of 3×104−8×105 nm2 (which corresponds to a circular injection pad having a diameter of 200-1000 nm); and
the injection pad and nanowire have a thickness of 1-50 nm along an Z-axis perpendicular to the X-axis and the Y-axis.

### Claim 2 (depends on 1)

The device of claim 1, wherein the magnetic metal material comprises iron, nickel, cobalt, or an alloy thereof.

### Claim 3 (depends on 1)

The device of claim 1, wherein the magnetic metal material comprises an iron alloy.

### Claim 4 (depends on 3)

The device of claim 3, wherein the iron alloy is an iron-nickel alloy.

### Claim 5 (depends on 4)

The device of claim 4, wherein the iron-nickel alloy is permalloy.

### Claim 6 (depends on 1)

The device of claim 1, wherein the nanowire has a top width of 50-100 nm.

### Claim 7 (depends on 1)

The device of claim 1, wherein the nanowire has a length extending from the outer edge of the injection pad of at least about 200 nm.

### Claim 8 (depends on 1)

The device of claim 1, wherein, the nanowire has a length extending from the outer edge of the injection pad of at least about 1000 nm.

### Claim 9 (depends on 1)

The device of claim 1, wherein the injection pad is circular and has a diameter of 200-1000 nm.

### Claim 10 (depends on 1)

The device of claim 1, wherein the injection pad is an equilateral polygon.

### Claim 11 (depends on 1)

The device of claim 1, wherein the injection pad and nanowire have a thickness of 1-10 nm.

### Claim 12 (depends on 1)

The device of claim 1, further comprising one or more notches in the nanowire.

### Claim 13 (depends on 1)

The device of claim 1, further comprising non-magnetic material positioned at the end of the nanowire opposite the injection pad.

### Claim 14

A magnetic storage device comprising:
(a) an injection pad; and
(b) a nanowire extending along an X-axis from an outer edge of the injection pad, the nanowire and the injection pad sharing the outer edge and the outer edge being curved or straight where the nanowire extends from the injection pad;
wherein:
the injection pad and nanowire comprise magnetic metal material and are monolithic;
the nanowire has a top width of 20-200 nm extending along a Y-axis perpendicular to the X-axis;
the injection pad has a top surface area parallel to a plane defined by the X-axis and the Y-axis of 3×104−8×105 nm2 (which corresponds to a circular injection pad having a diameter of 200-1000 nm); and
the injection pad and nanowire have a thickness of 1-50 nm along an Z-axis perpendicular to the X-axis and the Y-axis.

### Claim 15

A magnetic storage device comprising:
(a) an injection pad; and
(b) a nanowire extending along an X-axis from an outer edge of the injection pad, the nanowire and the injection pad sharing the outer edge and the outer edge being non-bent where the nanowire extends from the injection pad;
wherein:
the injection pad and nanowire comprise magnetic metal material and are monolithic;
the nanowire has a top width of 20-200 nm extending along a Y-axis perpendicular to the X-axis;
the injection pad has a top surface area parallel to a plane defined by the X-axis and the Y-axis of 3×104−8×105 nm2 (which corresponds to a circular injection pad having a diameter of 200-1000 nm); and
the injection pad and nanowire have a thickness of 1-50 nm along an Z-axis perpendicular to the X-axis and the Y-axis.

### Claim 16 (depends on 1)

A method of forming domain walls in a magnetic storage device, the method comprising the following steps:
(a) subjecting the device of claim 1 to an external magnetic field oriented along the Y-axis and having an intensity of 20-200 Oersteds;
(b) subjecting the device of claim 1 to an external magnetic field oriented along the X-axis and having an intensity of 5-20 Oersteds; and optionally
wherein step (a) and step (b) are performed simultaneously or separately, and optionally may be repeated one or more times.

### Claim 17 (depends on 16)

The method of claim 16, wherein step (a), step (b), or both are repeated at least eight times.

### Claim 18 (depends on 16)

The method of claim 16, wherein step (a) and step (b) are performed for less than 1 nanosecond.

### Claim 19 (depends on 16)

The method of claim 16, comprising reversing the external magnetic field oriented along the Y-axis and subjecting the device to the reversed external magnetic field oriented along the Y-axis.

### Claim 20 (depends on 16)

The method of claim 16, comprising reversing the external magnetic field oriented along the X-axis and subjecting the device to the reversed external magnetic field oriented along the X-axis.