# US 2011/0086990 A1 · Ethylene-Alpha Olefin Copolymers and Polymerization Processes for Making the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0086990 A1
- Document ID: US20110086990A1
- Status: Published application
- Kind: A1
- Application number: 12/968,996
- Filed: 2010-12-15
- Published: 2011-04-14
- Earliest claimed: 2006-06-27
- Assignees: Univation Technologies, LLC
- Inventors: Blair Alfred GRAHAM; Mark P. OSSOWSKI; James M. FARLEY; Rainer KOLB
- Web page: https://patentgrep.com/patent/US20110086990A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A process for the production of an ethylene alpha-olefin copolymer is disclosed. The process includes polymerizing ethylene and at least one alpha-olefin by contacting the ethylene and the at least one alpha-olefin with a metallocene catalyst in at least one gas phase reactor at a reactor pressure of from 0.7 to 70 bar and a reactor temperature of from 20° C. to 150° C. to form an ethylene alpha-olefin copolymer. The resulting ethylene alpha-olefin copolymer may have a density of 0.927 g/cc or greater and environmental stress crack resistance (ESCR) of 500 hr or more when measured according to ASTM 1693/B in 10% Igepal.

## Claims

### Claim 1

A process to produce an ethylene alpha-olefin copolymer, the process comprising:
contacting ethylene and at least one alpha-olefin with a metallocene catalyst in at least one gas phase reactor at a reactor pressure of from 0.7 to 70 bar and a reactor temperature of from 20° C. to 150° C. to polymerize an ethylene alpha-olefin copolymer,
wherein the ethylene alpha-olefin copolymer satisfies the following conditions:
a density of 0.927 g/cc or greater, a melt index ratio of (I21/I2) of from 15 to 40, an ESCR value of 500 hr or greater when measured according to ASTM 1693/B in 10% Igepal, a T75-T25 value of 4 or greater wherein T25 is the temperature at which 25% of the eluted polymer is obtained and T75 is the temperature at which 75% of the eluted polymer is obtained in a TREF experiment, and a F80 value of 10% or greater, wherein F80 is the fraction of polymer that elutes below 80° C.

### Claim 2 (depends on 1)

The process of claim 1, wherein the ethylene alpha-olefin copolymer has an ESCR value of 1000 hr or greater when measured according to ASTM 1693/B in 10% Igepal.

### Claim 3 (depends on 1)

The process of claim 1, wherein said density ranges from 0.927 g/cc to 0.965 g/cc.

### Claim 4 (depends on 1)

The process of claim 1, wherein said density ranges from 0.935 g/cc to 0.965 g/cc.

### Claim 5 (depends on 1)

The process of claim 1, wherein said density ranges from 0.940 g/cc to 0.965 g/cc.

### Claim 6 (depends on 1)

The process of claim 1, wherein said melt index ratio (I21/I2) ranges from 15 to 25.

### Claim 7 (depends on 1)

The process of claim 1, wherein the metallocene catalyst is selected from the group consisting of:
bis(n-propylcyclopentadienyl)hafnium Xn, bis(n-butylcyclopentadienyl)hafnium Xn, bis(n-pentylcyclopentadienyl)hafnium Xn, (n-propyl cyclopentadienyl)(n-butylcyclopentadienyl)hafnium Xn, bis[(2-trimethylsilylethyl)cyclopentadienyl]hafnium Xn, bis(trimethylsilyl cyclopentadienyl)hafnium Xn, dimethylsilylbis(n-propylcyclopentadienyl)hafnium Xn, dimethylsilylbis(n-butylcyclopentadienyl)hafnium Xn, bis(1-n-propyl-2-methylcyclopentadienyl)hafnium Xn, (n-propylcyclopentadienyl)(1-n-propyl-3-n-butylcyclopentadienyl)hafnium Xn;
wherein Xn is selected from the group consisting of halogen ions, hydrides, C1-12 alkyls, C2-12 alkenyls, C6-12 aryls, C7-20 alkylaryls, C1-12 alkoxys, C6-16 aryloxys, C7-18 alkylaryloxys, C1-12 fluoroalkyls, C6-12 fluoroaryls, and C1-12 heteroatom-containing hydrocarbons and substituted derivatives thereof.

### Claim 8 (depends on 7)

The process of claim 7, wherein the metallocene catalyst is a supported metallocene catalyst.

### Claim 9 (depends on 8)

The process of claim 8, wherein the metallocene catalyst is activated with at least one activator selected from the group consisting of an alumoxane, a modified alumoxane, an ionizing compound, or mixtures thereof.

### Claim 10 (depends on 9)

The process of claim 9, wherein the activator is an alumoxane.