# US 2011/0086442 A1 · Copper contamination detection method and system for monitoring copper contamination

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0086442 A1
- Document ID: US20110086442A1
- Status: Published application
- Kind: A1
- Application number: 12/973,062
- Filed: 2010-12-20
- Published: 2011-04-14
- Earliest claimed: 2007-09-28
- Assignees: International Business Machines Corporation
- Inventors: Jay Sanford Burnham; Joseph Kerry Vaughn Comeau; Leslie Peter Crane; James Randall Elliott; Scott Alan Estes; James Spiros Nakos; Eric Jeffrey White
- Web page: https://patentgrep.com/patent/US20110086442A1

## CPC

- H10P 74/23: {characterised by multiple measurements, corrections, marking or sorting processes}
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of monitoring copper contamination. The method includes method, comprising: (a) ion-implanting an N-type dopant into a region of single-crystal silicon substrate, the region abutting a top surface of the substrate; (c) activating the N-type dopant by annealing the substrate at a temperature of 500° C. or higher in an inert atmosphere; (c) submerging, for a present duration of time, the substrate into an aqueous solution, the aqueous solution to be monitored for copper contamination; and (d) determining an amount of copper adsorbed from the aqueous solution by the region of the substrate.

## Claims

### Claim 1

A method, comprising:
(a) forming a multiplicity of contamination monitors, each contamination monitor comprising an N-type region in a single-crystal silicon substrate, said region abutting a top surface of said substrate;
(b) selecting an unused contamination monitor of said multiplicity of contamination monitors and submerging, for a preset duration of time, said selected contamination monitor of said multiplicity of contamination monitors into an aqueous solution contained in a tank of a processing tool used to fabricate integrated circuits;
after (b), (c) determining an amount of copper in said region of said substrate of said one contamination monitor;
after (c), (d) if said amount of copper exceeds a preset limit, taking a corrective action to prevent copper contamination of said integrated circuits when processed in said tank; and
(e) repeating steps (b) through (d) periodically.

### Claim 2 (depends on 1)

The method of claim 1, further including:
between (d) and (e) determining a copper concentration of said solution based on said amount of copper found in said region of said substrate.

### Claim 3 (depends on 2)

The method of claim 2, further including:
determining said copper concentration of said solution based on an empirically derived curve, table or formula derived from measuring amounts of copper in monitor wafers submerged, for said present duration of time, in respective aqueous solutions having known and different copper concentrations.

### Claim 4 (depends on 1)

The method of claim 1, wherein said determining said amount of copper in said region of said substrate includes performing Total Internal Reflected X-Ray Fluorescence, Secondary Ion Mass Spectroscopy, Time of Flight SIMS, Energy Dispersive X-Ray Fluorescence, Auger Spectroscopy or X-Ray Photo-electron Spectroscopy.

### Claim 5 (depends on 1)

The method of claim 1, further including:
between (d) and (e), based on said determining an amount of copper in said region of said substrate, implementing a corrective action selected from the group consisting of shutting down said tank of said processing tool containing said solution, limiting types of product wafers allowed in said tank, restricting fabrication levels of product wafers allowed in said tank, limiting a number of product wafers that can be processed before shutting down said tank, and shutting down said tank, draining said solution from said tank, cleaning said tank, and refilling said tank with fresh solution.

### Claim 6 (depends on 1)

The method of claim 1, wherein concentrations of N-type dopant in said regions of said multiplicity of contamination monitors is between about 5 E19 atm/cm3 to about 1 E22 atm/cm3.

### Claim 7 (depends on 6)

The method of claim 6, wherein said N-type dopant is arsenic.

### Claim 8 (depends on 6)

The method of claim 6, wherein said N-type dopant is phosphorus.

### Claim 9 (depends on 1)

The method of claim 1, where (a) includes:
ion implanting an N-type dopant into respective regions of each contamination monitor of said multiplicity of contamination monitors to form respective N-type region in each contamination monitor of said multiplicity of contamination monitors; and
activating said N-type dopant by annealing each contamination monitor of said multiplicity of contamination monitors at a temperature of 500° C. or higher in an inert atmosphere in a furnace.

### Claim 10 (depends on 1)

The method of claim 1, where (a) includes:
ion implanting an N-type dopant into respective regions of each contamination monitor of said multiplicity of contamination monitors to form respective N-type region in each contamination monitor of said multiplicity of contamination monitors; and
activating said N-type dopant by annealing each contamination monitor of said multiplicity of contamination monitors at a temperature of 900° C. or higher in an inert atmosphere in a rapid-thermal-anneal tool.

### Claim 11 (depends on 1)

The method of claim 1, wherein (b) includes;
breaking said selected contamination monitor into multiple pieces;
selecting a piece of said multiple pieces;
submerging said selected piece into said solution; and
after submerging said elected piece, performing (c) and (d) on said selected piece.

### Claim 12 (depends on 1)

The method of claim 1, wherein said aqueous solution contains fluorine ions.

### Claim 13 (depends on 1)

The method of claim 1, wherein each substrate of each contamination monitor of said multiplicity of contamination monitors is doped P-type and has a resistivity of between about 10-ohm-cm and about 20 ohm-cm.

### Claim 14 (depends on 1)

The method of claim 1, wherein each substrate of each contamination monitor of said multiplicity of contamination monitors is doped N-type and has a resistivity of between about 50-ohm-cm and about 0.7 ohm-cm.

### Claim 15 (depends on 1)

The method of claim 1, wherein each contamination monitor of said multiplicity of contamination monitors has the same dimensions of diameter and thickness as wafers on which said integrated circuits are fabricated in said processing tool.