# US 2011/0086213 A1 · Method of producing a silicon carbide bulk single crystal with thermal treatment, and low-impedance monocrystalline silicon carbide substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0086213 A1
- Document ID: US20110086213A1
- Status: Published application
- Kind: A1
- Application number: 12/902,704
- Filed: 2010-10-12
- Published: 2011-04-14
- Earliest claimed: 2009-10-09
- Assignees: SiCrystal GmbH
- Inventors: THOMAS STRAUBINGER; MICHAEL VOGEL; ANDREAS WOHLFART
- Web page: https://patentgrep.com/patent/US20110086213A1

## CPC

- C30B 29/36: Carbides
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A silicon carbide bulk single crystal is produced at a growth temperature of up to 2200° C. by sublimation growth and is subjected to thermal aftertreatment after the sublimation growth. The bulk single crystal is brought to an aftertreatment temperature that is higher than a growth temperature. Very low-stress and low-dislocation SiC substrates can be produced from such a SiC bulk single crystal, the substrates additionally having a particularly low electrical resistivity. The SiC bulk single crystal is positioned within an SiC powder before the thermal aftertreatment and it is completely surrounded by the SiC powder during the thermal aftertreatment.

## Claims

### Claim 1

A method of producing an SiC bulk single crystal, the method which comprises:
growing an SiC bulk single crystal at a growth temperature of up to 2200° C. by way of sublimation growth;
subjecting the SiC bulk single crystal to a thermal aftertreatment following the sublimation growth, and thereby bringing the SiC bulk single crystal to an aftertreatment temperature that is higher than the growth temperature; and
placing the SiC bulk single crystal within an SiC powder prior to the thermal aftertreatment and completely surrounding the SiC bulk single crystal with the SiC powder during the thermal aftertreatment.

### Claim 2 (depends on 1)

The method according to claim 1, which comprises setting a global temperature difference within the SiC bulk single crystal during the thermal aftertreatment to at most 10 K.

### Claim 3 (depends on 2)

The method according to claim 2, which comprises setting the global temperature difference within the SiC bulk single crystal during the thermal aftertreatment to no more than 5 K.

### Claim 4 (depends on 1)

The method according to claim 1, which comprises growing the SiC bulk single crystal in a direction of a central longitudinal axis, and setting an axial temperature difference measured in the direction of the central longitudinal axis within the SiC bulk single crystal during the thermal aftertreatment to at most 2 K.

### Claim 5 (depends on 4)

The method according to claim 4, which comprises setting the axial temperature difference in the direction of the central longitudinal axis during the thermal aftertreatment to no more than 1 K.

### Claim 6 (depends on 1)

The method according to claim 1, which comprises cooling the SiC single crystal at a cooling rate at the end of the thermal aftertreatment of at most 5 K/min.

### Claim 7 (depends on 6)

The method according to claim 6, which comprises setting the cooling rate at the end of the thermal aftertreatment to no more than 1 K/min.

### Claim 8 (depends on 1)

The method according to claim 1, which comprises carrying out the thermal aftertreatment during an aftertreatment duration of at least 24 hours.

### Claim 9 (depends on 8)

The method according to claim 8, which comprises selecting the aftertreatment duration to last no more than 72 hours.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the SiC powder, before the thermal aftertreatment, is composed of SiC grains, of which 50% by weight have a grain size with a maximum grain diameter of at most 500 μm.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the maximum grain diameter is no more than 100 μm.

### Claim 12 (depends on 1)

The method according to claim 1, which comprises providing the SiC powder with a molar ratio between a C fraction and an Si fraction in a range between 0.9 and 1.1 prior to the thermal aftertreatment.

### Claim 13 (depends on 11)

The method according to claim 11, which comprises setting the molar ratio of C to Si at 1.

### Claim 14 (depends on 1)

The method according to claim 1, which comprises performing the thermal aftertreatment with the SiC bulk single crystal accommodated in a crucible completely surrounded by a thermal insulation material.

### Claim 15

A monocrystalline SiC substrate, comprising:
a substrate main surface and a substrate thickness, wherein an electrical resistivity determined for an arbitrary 4 mm2 partial area of the substrate main surface and relative to the substrate thickness is less than 20 mΩcm.

### Claim 16 (depends on 15)

The SiC substrate according to claim 15, wherein the partial area is a square area.

### Claim 17 (depends on 15)

The SiC substrate according to claim 15, wherein the resistivity is less than 15 mΩcm.

### Claim 18 (depends on 15)

The SiC substrate according to claim 15, wherein said substrate main surface has a diameter of at least 100 mm.

### Claim 19 (depends on 15)

The SiC substrate according to claim 15, wherein said diameter is at least 150 mm.

### Claim 20 (depends on 15)

The SiC substrate according to claim 15, wherein said substrate main surface has a diameter of at least 150 mm and the substrate thickness is at most 500 μm.

### Claim 21 (depends on 15)

The SiC substrate according to claim 15, wherein the substrate main surface has a diameter of at least 150 mm and a global dislocation density determined for an entire said substrate main surface is at most 104 cm−2.