PET Polymer with Improved Properties
AssigneeEastman Chemical Company
InventorsFrederick Leslie Colhoun, Perry Michael Murdaugh, SR.
Life of this patent
Estimating the term…
Abstract
Polyester compositions having desirable injection molding properties and that retain good crystallization rates and natural stretch ratio characteristics are described. These polyesters are suitable for the manufacture of beverage containers, bulk continuous filaments, and other articles that can benefit from such improved properties.
Claims16
A polyester comprising:
- i) a carboxylic acid component comprising at least 90 mol % terephthalic acid residues and from 0 to 10 mol % of carboxylic acid comonomer residues;
- ii) a hydroxyl component comprising from 90 to 95 mol % ethylene glycol residues and additional hydroxyl residues in an amount from 5 to 10 mol %;
- wherein the additional hydroxyl residues are chosen from a) diethylene glycol residues and b) mixtures of diethylene glycol residues and hydroxyl comonomer residues;
- based on 100 mol % of carboxylic acid component residues and 100 mol % of hydroxyl component residues in the polyester;
- wherein at least one of the carboxylic acid and hydroxyl components comprises comonomer residues, the molar ratio of the total comonomer residues to diethylene glycol residues being 1.3:1.0 or greater;
- and
- wherein the polyester comprises less than 2.3 mol % of diethylene glycol and has an intrinsic viscosity greater than 0.40 dL/g and less than 0.80 dL/g
4 more elements
Dependencies are inferred from the claim text.