# US 2011/0031165 A1 · Processes for removing hydrogen sulfide from refined hydrocarbon streams

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2011/0031165 A1
- Document ID: US20110031165A1
- Status: Published application
- Kind: A1
- Application number: 12/535,252
- Filed: 2009-08-04
- Published: 2011-02-10
- Earliest claimed: 2009-08-04
- Inventors: Larry John KARAS; Sherif Eldin; Malcolm Craig Winslow
- Web page: https://patentgrep.com/patent/US20110031165A1

## CPC

- C10G 75/02: by addition of corrosion inhibitors
- C10G 29/22: containing oxygen as the only hetero atom
- C10G 2300/104: Light gasoline having a boiling range of about 20 - 100 °C
- C10G 2300/1044: Heavy gasoline or naphtha having a boiling range of about 100 - 180 °C
- C10G 2300/1051: Kerosene having a boiling range of about 180 - 230 °C
- C10G 2300/1055: Diesel having a boiling range of about 230 - 330 °C
- C10G 2300/1059: Gasoil having a boiling range of about 330 - 427 °C
- C10G 2300/1077: Vacuum residues
- C10G 2300/207: Acid gases, e.g. H2S, COS, SO2, HCN
- C10G 2300/4075: Limiting deterioration of equipment
- C10G 2300/80: Additives
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

A method for reducing the amount of hydrogen sulfide present in refined hydrocarbon streams and reducing the amount of corrosion in processing equipment contacting the refined hydrocarbon stream. The method includes adding a corrosion inhibitor to the refined hydrocarbon stream in contact with the processing equipment to protect the processing equipment and adding glyoxal to the refined hydrocarbon stream in contact with the protected processing equipment. The corrosion inhibitor includes an organic soluble compound having a nitrogen-containing ring.

## Claims

### Claim 1

A method for reducing the amount of hydrogen sulfide present in a refined hydrocarbon stream and reducing the amount of corrosion in processing equipment contacting the refined hydrocarbon stream, said method comprising adding a corrosion inhibitor to the refined hydrocarbon stream in contact with the processing equipment to protect the processing equipment and adding glyoxal to the refined hydrocarbon stream in contact with the protected processing equipment, wherein said corrosion inhibitor comprises an organic soluble compound having a nitrogen-containing ring.

### Claim 2 (depends on 1)

The method of claim 1 wherein the refined hydrocarbon stream is selected from the group consisting of gas oil, naphtha, FCC slurry, diesel fuel, fuel oil, jet fuel, gasoline, kerosene and vacuum residua.

### Claim 3 (depends on 1)

The method of claim 1 wherein the refined hydrocarbon stream is at an elevated temperature.

### Claim 4 (depends on 3)

The method of claim 3 wherein the refined hydrocarbon stream is at a temperature of from about ambient to about 150° C.

### Claim 5 (depends on 1)

The method of claim 1 wherein the processing equipment is a pipeline or a holding tank.

### Claim 6 (depends on 5)

The method of claim 5, wherein the processing equipment is made of carbon steel.

### Claim 7 (depends on 1)

The method of claim 1, wherein the corrosion inhibitor comprises a five-membered or six-membered nitrogen-containing ring.

### Claim 8 (depends on 7)

The method of claim 7, wherein corrosion inhibitor is an imidazoline derivative.

### Claim 9 (depends on 8)

The method of claim 8, wherein the corrosion inhibitor is a fatty acid imidazoline.

### Claim 10 (depends on 8)

The method of claim 8, wherein the fatty acid imidazoline has the following structure:
wherein R and R′ are each, separately, a C6 to C36 alkyl, alkylene or aromatic group.

### Claim 11 (depends on 7)

The method of claim 7, wherein the nitrogen-containing ring is a pyrimidine derivative.

### Claim 12 (depends on 11)

The method of claim 11 wherein the pyrimidine derivative is a fatty acid pyrimidine.

### Claim 13 (depends on 12)

The method of claim 12 wherein the fatty acid pyrimidine has the following structure:
wherein Ra and Rb are each, separately, a C6 to C36 alkyl, alkylene or aromatic group.

### Claim 14 (depends on 1)

The method of claim 1 wherein the corrosion inhibitor is injected into the refined hydrocarbon stream.

### Claim 15 (depends on 1)

The method of claim 1 wherein the corrosion inhibitor is present from about 2 ppm by volume to about 100 ppm by volume, based on the volume of the refined hydrocarbon stream.

### Claim 16 (depends on 1)

The method of claim 1, wherein the corrosion inhibitor provides a protective coating onto the processing equipment after at least about 5 minutes of adding the corrosion inhibitor to the refined hydrocarbon stream in contact with the processing equipment.

### Claim 17 (depends on 1)

The method of claim 1, wherein glyoxal is added to the refined hydrocarbon stream in an amount of from about 1 ppm to about 3000 ppm by volume, based on the volume of the refined hydrocarbon stream.

### Claim 18 (depends on 1)

The method of claim 1, wherein the corrosion inhibitor continues to be added to the refined hydrocarbon stream after the glyoxal has been added.

### Claim 19 (depends on 18)

The method of claim 18, wherein the corrosion inhibitor continues to be added in an amount of from about 1 ppm by volume to about 20 ppm by volume, based on the volume of the refined hydrocarbon stream.

### Claim 20 (depends on 1)

The method of claim 1, wherein the glyoxal further comprises a catalyst.

### Claim 21 (depends on 20)

The method of claim 20, wherein the catalyst is a quaternary ammonium salt.

### Claim 22 (depends on 21)

The method of claim 21, wherein the catalyst has formula I:
R1R2R3R4N+X− I
wherein R1, R2, R3 and R4 are each independently an alkyl group having from 1 to 30 carbon atoms, an aryl group having from 6 to 30 carbon atoms or an arylalkyl group having from 7 to 30 carbon atoms; and X is a halide, sulfate, nitrate or carboxylate.

### Claim 23 (depends on 22)

The method of claim 22, wherein the quaternary ammonium salt is alkyl benzyl ammonium chloride or benzyl cocoalkyl (C12-C18) dimethylammonium chloride.

### Claim 24 (depends on 21)

The method of claim 21, wherein the catalyst is present from about 0.01 to about 15 percent by weight based on the weight of glyoxal.