# US 2010/0314035 A1 · Method for producing vertical alignment liquid crystal display

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0314035 A1
- Document ID: US20100314035A1
- Status: Published application
- Kind: A1
- Application number: 12/860,187
- Filed: 2010-08-20
- Published: 2010-12-16
- Earliest claimed: 1999-10-21
- Assignees: Konica Corporation
- Inventors: Toshiaki SHIBUE; Makoto HONDA; Nobuo KUBO; Noriyasu KUZUHARA; Hiroki UMEDA; Sota KAWAKAMI; Takatoshi YAJIMA
- Web page: https://patentgrep.com/patent/US20100314035A1

## CPC

- B32B 27/08: of synthetic resin
- C08B 3/16: Preparation of mixed organic cellulose esters {, e.g. cellulose aceto-formate or cellulose aceto-propionate}
- C08L 1/14: Mixed esters, e.g. cellulose acetate-butyrate
- C09K 19/2007: {the chain containing -COO- or -OCO- groups}
- C09K 19/2014: {containing additionally a linking group other than -COO- or -OCO-, e.g. -CH2-CH2-, -CH=CH-, -C=C-; containing at least one additional carbon atom in the chain containing -COO- or -OCO- groups, e.g. -(CH2)m-COO-(CH2)n-}
- C09K 19/32: containing condensed ring systems, i.e. fused, bridged or spiro ring systems
- G02B 5/3033: {in the form of a thin sheet or foil, e.g. Polaroid}
- G02F 1/133634: {the refractive index Nz perpendicular to the element surface being different from in-plane refractive indices Nx and Ny, e.g. biaxial or with normal optical axis}
- C09K 2019/0429: {the specific unit being a carbocyclic or heterocyclic discotic unit}
- C09K 2219/03: in the form of films, e.g. films after polymerisation of LC precursor
- C09K 2323/00: Functional layers of liquid crystal optical display excluding electroactive liquid crystal layer characterised by chemical composition
- C09K 2323/02: Alignment layer characterised by chemical composition
- C09K 2323/03: Viewing layer characterised by chemical composition
- C09K 2323/031: Polarizer or dye
- C09K 2323/035: Ester polymer, e.g. polycarbonate, polyacrylate or polyester
- C09K 2323/057: Ester polymer, e.g. polycarbonate, polyacrylate or polyester
- Y10T 428/28: Web or sheet containing structurally defined element or component and having an adhesive outermost layer
- Y10T 428/31786: Of polyester [e.g., alkyd, etc.]
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08B: POLYSACCHARIDES; DERIVATIVES THEREOF (polysaccharides containing less than six saccharide radicals attached to each other by glycosidic linkages C07H; fermentation or enzyme-using processes C12P19/00; sugar industry C13; production of cellulose D21)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The method to produce the vertical alignment type liquid crystal display employs treating an optical film comprising of cellulous ester with an aqueous solution of sodium hydroxide to prepare an alkali-treated optical film; immersing a polyvinyl alcohol film in an aqueous solution containing iodine and boric acid; stretching the polyvinyl alcohol film to prepare a polarizing film; adhering the alkali-treated optical film onto both surfaces of the polarizing film to prepare a polarizing plate; and providing the polarizing plate on both surfaces of a vertical alignment type liquid crystal cell to providing the vertical alignment type liquid crystal display. At least one of the optical film has a retardation value (Rt value) in the thickness direction of from 60 to 300 nm, Rt=[(nx+ny)/2−nz]×d.

## Claims

### Claim 1

A method for producing a vertical alignment type liquid crystal display, comprising steps of:
treating an optical film comprising cellulose ester with an aqueous solution of sodium hydroxide to prepare an alkali-treated optical film;
immersing a polyvinyl alcohol film in an aqueous solution containing iodine and boric acid;
stretching the polyvinyl alcohol film to prepare a polarizing film;
adhering the alkali-treated optical film onto both surfaces of the polarizing film to prepare a polarizing plate; and
providing the polarizing plate on both surfaces of a vertical alignment type liquid crystal cell to providing the vertical alighment type liquid crystal display,
wherein at least one of the optical film has a retardation value (Rt value) in the thickness direction of from 60 to 300 nm,
Rt=[(nx+ny)/2−nz]×d
wherein nx represents the refractive index of the optical film in the direction giving maximum refractive index in the plane of the film, ny represents the refractive index of the optical film in the direction perpendicular to the direction giving maximum refractive index in the plane of the film, nz represents the refractive index of the optical film in the thickness direction and d represents the thickness (in nm) of the optical film.

### Claim 2 (depends on 1)

The method of claim 1, wherein at least one of the optical film has the retardation value (Rt value) in the thickness direction of from 90 to 200 nm.

### Claim 3 (depends on 1)

The method of claim 1, wherein at least one of the optical film has the retardation value (Rt value) in the thickness direction of from 100 to 175 nm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the optical film having retardation value (Rt value) in the thickness direction of from 60 to 300 nm is made by being dried while being stretched, and a stretching factor of the dry and stretching step is between 2 and 50 percent.

### Claim 5 (depends on 4)

The method of claim 4, wherein the stretching factor of the stretching step is 5 to 40 percent.

### Claim 6 (depends on 5)

The method of claim 5, wherein the stretching factor of the stretching step is 10 to 30 percent.

### Claim 7 (depends on 1)

The method of claim 1, wherein the optical film having retardation value (Rt value) in the thickness direction of from 60 to 300 nm is made by peeled from a belt or drum, and a residual solvent amount during the peeling step is from 5 to 100 percent.

### Claim 8 (depends on 7)

The method of claim 7, wherein the residual solvent amount during the peeling step is from 5 to 80%.

### Claim 9 (depends on 8)

The method of claim 8, wherein the residual solvent amount during the peeling step is from 5 to 80%.