# US 2010/0310446 A1 · Carbon and Electrospun Nanostructures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0310446 A1
- Document ID: US20100310446A1
- Status: Published application
- Kind: A1
- Application number: 12/857,966
- Filed: 2010-08-17
- Published: 2010-12-09
- Earliest claimed: 2003-07-02
- Assignees: Physical Sciences, Inc.
- Inventors: John D. Lennhoff
- Web page: https://patentgrep.com/patent/US20100310446A1

## CPC

- D01D 5/0038: {the fibre formed by solvent evaporation, i.e. dry electro-spinning}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B 32/162: characterised by catalysts
- D01F 9/22: from polyacrylonitriles
- C01B 2202/02: Single-walled nanotubes
- C01B 2202/06: Multi-walled nanotubes
- Y10S 977/842: for carbon nanotubes or fullerenes
- Y10T 428/30: Self-sustaining carbon mass or layer with impregnant or other layer
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention is directed to the production of nanostructures, e.g., single wall carbon nanotubes (“SWNT”) and/or multi wall carbon nanotubes (“MWNT”), from solutions containing a polymer, such as polyacrylonitrile (PAN). In particular, the invention is directed to the production of nanostructures, for example, SWNT and/or MWNT, from mixtures, e.g., solutions, containing polyacrylonitrile, polyaniline emeraldine base (PANi) or a salt thereof, an iron salt, e.g., iron chloride, and a solvent. In one embodiment, a mixture containing polyacrylonitrile, polyaniline emeraldine base or a salt thereof, an iron salt, e.g., iron chloride, and a solvent is formed and the mixture is electrospun to form nanofibers. In another embodiment, the electrospun nanofibers are then oxidized, e.g., heated in air, and subsequently pyrolyzed to form carbon nanostructures.

## Claims

### Claim 1

Carbon nanotubes produced by a method, comprising the steps of:
(a) forming a polymer solution including an organic solvent and a polymer that includes at least one of a polyacrylonitrile and a polyimide;
(b) electrospinning the polymer solution to form nanofibers having diameters in a range of between about 1 nanometer and about 10 nanometers; and
heating and pyrolyzing the nanofibers to form single wall carbon nanotubes.

### Claim 2 (depends on 1)

The carbon nanotubes of claim 1 wherein the polymer solution includes between about 1 and about 10 weight percent polyacrylonitrile.

### Claim 3 (depends on 1)

The carbon nanotubes of claim 1 wherein the polymer solution includes between about 3 and about 5 weight percent polyacrylonitrile.

### Claim 4 (depends on 1)

The carbon nanotubes of claim 1, wherein the polymer solution further includes a salt.

### Claim 5 (depends on 4)

The carbon nanotubes of claim 4 wherein the salt is an iron salt.

### Claim 6 (depends on 5)

The carbon nanotubes of claim 5, wherein the iron salt includes iron chloride.

### Claim 7 (depends on 5)

The carbon nanotubes of claim 5 wherein the polymer solution includes greater than zero and up to about 0.5 weight percent iron salt.

### Claim 8 (depends on 7)

The carbon nanotubes of claim 7 wherein the polymer solution includes between about 0.05 and about 0.15 weight percent an iron salt.

### Claim 9 (depends on 1)

The carbon nanotubes of claim 1, wherein the polymer includes a conductive polymer.

### Claim 10 (depends on 1)

The carbon nanotubes of claim 1, wherein the conductive polymer includes at least one of polyaniline and polyethylene dioxythiophene.

### Claim 11 (depends on 1)

The carbon nanotubes of claim 1, wherein the polymer solution further includes a metal salt.

### Claim 12 (depends on 11)

The carbon nanotubes of claim 11, wherein the metal salt is iron chloride.

### Claim 13 (depends on 1)

The carbon nanotubes of claim 1 wherein the polymer solution includes greater than zero and up to about 1 weight percent polyaniline emeraldine base or a salt thereof.

### Claim 14 (depends on 13)

The carbon nanotubes of claim 13 wherein the polymer solution includes between about 0.3 and about 0.5 weight percent polyaniline emeraldine base or a salt thereof.

### Claim 15 (depends on 1)

The carbon nanotubes of claim 1, wherein the fibers are pyrolyzed at a temperature in the range of between about 900° C. to about 2,400° C.

### Claim 16 (depends on 15)

The carbon nanotubes of claim 15, wherein the fibers are pyrolyzed at a temperature in the range of between about 1,000° C. to about 2,000° C.

### Claim 17 (depends on 16)

The carbon nanotubes of claim 16, wherein the fibers are pyrolyzed at a temperature in the range of between about 1,100° C. to about 1,600° C.

### Claim 18 (depends on 17)

The carbon nanotubes of claim 17, wherein the fibers are pyrolyzed at a temperature in the range of between about 1,300° C. to about 1,500° C.

### Claim 19 (depends on 18)

The carbon nanotubes of claim 18, wherein the fibers are pyrolyzed at a temperature in the range of between about 1,300° C. to about 1,400° C.

### Claim 20 (depends on 1)

The carbon nanotubes of claim 1, wherein the nanotubes are heated in air at a temperature in a range of between about 300° C. to about 350° C., for a period of time in a range of between about 5 minutes and about 60 minutes, and then placed in a tube furnace with an oxygen-free nitrogen purge, heated to a temperature of about 2,400° C. and then pyrolyzed for a period of time in a range of between about one minute and about five hours.