# US 2010/0304955 A1 · Catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0304955 A1
- Document ID: US20100304955A1
- Status: Published application
- Kind: A1
- Application number: 12/599,107
- Filed: 2008-05-09
- Published: 2010-12-02
- Earliest claimed: 2007-05-11
- Assignees: Sasol Technology (Proprietary) Limited
- Inventors: Jan Van De Loosdrecht; Abdool Muthalib Saib
- Web page: https://patentgrep.com/patent/US20100304955A1

## CPC

- C10G 2/332: {of the iron-group}
- B01J 23/8913: {Cobalt and noble metals}
- B01J 23/94: of catalysts comprising metals, oxides or hydroxides of the iron group metals or copper
- B01J 23/96: of catalysts comprising metals, oxides or hydroxides of the noble metals
- B01J 37/0209: {involving a reaction between the support and a fluid}
- B01J 38/10: using elemental hydrogen
- B01J 38/30: in gaseous suspension, e.g. fluidised bed
- C10G 2/30: {from carbon monoxide with hydrogen}
- B01J 21/12: Silica and alumina
- B01J 38/48: Liquid treating or treating in liquid phase, e.g. dissolved or suspended
- C10G 2300/705: Passivation
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

A process for regenerating a spent cobalt Fischer-Tropsch synthesis catalyst includes subjecting a spent particulate cobalt Fischer-Tropsch synthesis catalyst sequentially to a dewaxing treatment, an oxidation treatment at a pressure of 4 to 30 bar(a) and a reduction treatment, thereby regenerating the catalyst.

## Claims

### Claim 1

A process for regenerating a spent cobalt Fischer-Tropsch synthesis catalyst, which process includes subjecting a spent particulate cobalt Fischer-Tropsch synthesis catalyst sequentially to a dewaxing treatment, an oxidation treatment in air and at a pressure of 4 to 30 bar(a), and a reduction treatment, thereby regenerating the catalyst.

### Claim 2 (depends on 1)

A process according to claim 1, which includes subjecting the catalyst to at least one further regeneration cycle comprising an oxidation treatment at a pressure of 4 to 30 bar(a) followed by a reduction treatment.

### Claim 3 (depends on 1)

A process according to claim 1, wherein the dewaxing treatment includes hydrogenolysis; solvent wash or extraction; or solvent wash or extraction followed by hydrogenolysis.

### Claim 4 (depends on 1)

A process according to claim 1, which includes, after the dewaxing treatment and before the oxidation treatment, passivating the catalyst.

### Claim 5 (depends on 1)

A process according to claim 1, wherein the oxidation treatment comprises subjecting the dewaxed catalyst particles to calcination by fluidizing the catalyst particles in the air at an elevated temperature and at the elevated pressure of from 4 to 30 bar(a), thereby to oxidize the catalyst particles.

### Claim 6 (depends on 5)

A process according to claim 5, wherein the fluidization of the dewaxed catalyst particles is effected in a reaction chamber which is at the elevated pressure, with the calcination including heating the catalyst particles up to a temperature T and holding the catalyst particles at the temperature T for a period of time.

### Claim 7 (depends on 6)

A process according to claim 6, wherein the space velocity through the reaction chamber during the fluidization is in the range of 100 to 20000 mln/g catalyst/hour.

### Claim 8 (depends on 5)

A process according to claim 5, wherein the catalyst particles are heated up to the temperature T at a rate of 0.1 to 10° C./min.

### Claim 9 (depends on 6)

A process according to claim 6, wherein the temperature T is in the range of 150° C. to 400° C.

### Claim 10 (depends on 6)

A process according to claim 6, wherein the period of time that the catalyst particles are held at the temperature T° C., is in the range of 0.1 hour to 24 hours.

### Claim 11 (depends on 1)

A process according to claim 1, wherein the elevated pressure at which the oxidation is effected is 4 to 12 bar(a).

### Claim 12

(canceled)

### Claim 13 (depends on 1)

A process according to claim 1, wherein the reduction treatment comprises treating the oxidized catalyst particles with a hydrogen-containing reducing gas at an elevated temperature and at a pressure P where P≧0.8 bar(a).