# US 2010/0304950 A1 · Optical glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0304950 A1
- Document ID: US20100304950A1
- Status: Published application
- Kind: A1
- Application number: 12/790,141
- Filed: 2010-05-28
- Published: 2010-12-02
- Earliest claimed: 2009-05-28
- Assignees: Asahi Glass Company, Limited
- Inventors: Satoru TOMENO; Yuki Kondo
- Web page: https://patentgrep.com/patent/US20100304950A1

## CPC

- C03C 3/068: containing rare earths
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present invention relates to an optical glass containing, in terms of mass % on the basis of oxides, B2O3: 10 to 20%, SiO2: 0.5 to 12%, ZnO: 5 to 19%, Ta2O5: 2.5 to 17%, Li2O: 0.2 to 3%, ZrO2: 0.6 to 4.9%, WO3: 1 to 20%, La2O3: 25 to 50%, Gd2O3: 0 to 13%, and Y2O3: 0.2 to 20%, provided that La2O3+Gd2O3+Y2O3 is 35 to 60%, in which the optical glass does not substantially contain Nb2O5, and has a refractive index (nd) of 1.82 to 1.86, an Abbe's number (νd) of 37 to 44 and a glass transition point (Tg) of 630° C. or lower.

## Claims

### Claim 1

An optical glass containing, in terms of mass % on the basis of oxides,
B2O3: 10 to 20%,
SiO2: 0.5 to 12%,
ZnO: 5 to 19%,
Ta2O5: 2.5 to 17%,
Li2O: 0.2 to 3%,
ZrO2: 0.6 to 4.9%,
WO3: 1 to 20%,
La2O3: 25 to 50%,
Gd2O3: 0 to 13%, and
Y2O3: 0.2 to 20%, provided that La2O3+Gd2O3+Y2O3 is 35 to 60%,
wherein the optical glass does not substantially contain Nb2O5, and has a refractive index (nd) of 1.82 to 1.86, an Abbe's number (νd) of 37 to 44 and a glass transition point (Tg) of 630° C. or lower.

### Claim 2 (depends on 1)

The optical glass according to claim 1, having a liquidus temperature (TL) of 112.0° C. or lower.

### Claim 3 (depends on 1)

The optical glass according to claim 1, having a liquidus temperature viscosity (ηTL) of 5 dPa·s or more.

### Claim 4 (depends on 1)

The optical glass according to claim 1, wherein a mass % fraction of a content of La2O3 to a total content of La2O3, Gd2O3, Y2O3 and Yb2O3 is 0.67 to 0.90.

### Claim 5 (depends on 2)

The optical glass according to claim 2, wherein, at the liquidus temperature (TL) or lower of the optical glass, a plurality of devitrified substances do not precipitate and only LaBO3 precipitates.

### Claim 6 (depends on 1)

A preform for precision press molding, comprising the optical glass according to claim 1.

### Claim 7 (depends on 1)

An optical element obtained by subjecting the optical glass according to claim 1 to precision press molding.

### Claim 8

An optical glass containing, in terms of mol % on the basis of oxides,
B2O3: 20 to 40%,
SiO2: 1 to 30%,
ZnO: 10 to 34%,
Ta2O5: 0.8 to 8%,
Li2O: 0.5 to 15%,
ZrO2: 0.5 to 10%,
WO3: 3 to 15%,
La2O3: 10 to 25%,
Gd2O3: 0 to less than 5%, and
Y2O3: 0.1 to 15%, provided that La2O3+Gd2O3+Y2O3 is 15 to 30%,
wherein the optical glass does not substantially contain Nb2O5, and has a refractive index (nd) of 1.82 to 1.86 and an Abbe's number (νd) of 37 to 44 and a glass transition point (Tg) of 630° C. or lower.