# US 2010/0304158 A1 · Surface pre-treatment coating film and process for metallic substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0304158 A1
- Document ID: US20100304158A1
- Status: Published application
- Kind: A1
- Application number: 12/830,289
- Filed: 2010-07-03
- Published: 2010-12-02
- Earliest claimed: 2010-07-03
- Assignees: Shahid Bahonar University of Kerman
- Inventors: Sayed Morteza Madani; Maryam Ehteshamzadeh; Hassan Hashemipour Rafsanjani
- Web page: https://patentgrep.com/patent/US20100304158A1

## CPC

- C23C 24/08: by application of heat or pressure and heat (C23C24/04 takes precedence)
- C23C 18/1216: {Metal oxides (C23C18/1212 takes precedence)}
- C23C 18/1225: {Deposition of multilayers of inorganic material}
- C23C 18/1241: {Metallic substrates}
- C23C 18/1254: {Sol or sol-gel processing}
- C23C 24/00: Coating starting from inorganic powder (spraying of the coating material in molten state C23C4/00; solid state diffusion C23C8/00 - C23C12/00)
- Y10T 428/31663: As siloxane, silicone or silane
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The various embodiments herein provide a method and composition to produce an anti-corrosive layer. According to one embodiment herein, a titanium based sol is synthesized and deposited on a substrate, dried for 120° C. for 1 hour, calcinated upto 400° C. for 1 hour, doped with a corrosion inhibitor, dried and deposited a layer of hybrid silica sol and cured to obtain the anticorrosive layer. According to another embodiment, a surface pre-treatment coating has a composition comprising a titanium dioxide layer, a corrosion inhibitor doped on the titanium dioxide layer, a hybrid silicate layer deposited on the doped titanium layer to form a coating to provide an improved corrosion resistance and self-healing effect.

## Claims

### Claim 1

A surface pre-treatment coating film for metallic substrates comprising:
a substrate;
a titanium dioxide layer deposited on the substrate and doped with a corrosion inhibitor; and
a hybrid silicate layer deposited on the titanium dioxide layer doped with the corrosion inhibitor.

### Claim 2 (depends on 1)

The coating film according to claim 1, wherein the corrosion inhibitor is benzotriazole.

### Claim 3 (depends on 1)

The coating film according to claim 1, wherein the hybrid silicate layer is a mixture of water based silane and wherein the mixture of water based silane includes 3-glycidoxypropyltrimethoxysilane (GPTMS) and tetraethylorthosilicate (TEOS).

### Claim 4

A method of preparing a surface pre-treatment coating film for metallic substrates, the method consisting the steps of:
preparing a substrate;
depositing a titanium dioxide (TiO2) layer on the substrate;
drying the substrate after depositing the TiO2layer;
calcinating the dried substrate;
doping the TiO2 layer with a corrosion inhibitor;
drying the substrate after doping the TiO2 layer with the corrosion inhibitor;
depositing a hybrid silicate layer on the TiO2 layer doped with the corrosion inhibitor; and
curing the substrate after depositing the hybrid silicate layer.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the step of preparing the substrate comprises:
grounding the substrate with emery papers having numbers 200 to 2500 successively;
cleaning the grounded substrate ultrasonically in mixture comprising acetone, ethanol and distilled water for 10 min.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the titanium dioxide (TiO2) layer is deposited on the substrate using a sol-gel method.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the titanium dioxide (TiO2) layer is deposited on the substrate using a controllable hydrolysis of titanium alkoxide.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the step of depositing the titanium dioxide (TiO2) layer on the substrate consists of:
preparing a titanium based sol by using a precursor, a solvent and a catalyst; wherein the precursor is a tetra-n-butyl orthotitanate, the solvent is ethanol, the catalyst is 70% nitric acid and the titanium based sol is a titanium oxide sol;
immersing the substrate in the titanium oxide sol for 100 seconds; and forming a thin film of the titanium dioxide on the substrate by a sol-gel dip coating process at a withdrawal speed of 18 cm/min.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the titanium based sol is prepared and synthesized by dissolving a quantity of titanium alkoxide in 0.685 moles of ethanol to obtain a solution, magnetically stirring the solution for 1 hour, hydrolyzing the solution by drop-wise adding a mixture comprising 0.277 moles of de-ionized water, 0.0441 moles of nitric acid 70% and 0.171 moles of ethanol, stirring the hydrolyzed solution for another 1 hour at room temperature and keeping the solution at room temperature for 24 hrs to obtain a transparent yellow solution.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the titanium alkoxide is 0.029 moles of tetra-n-butyl-orthotitanate.

### Claim 11 (depends on 4)

The method according to claim 4, wherein the substrate is dried at 120° C. for 1 hour after the deposition of the TiO2 layer.

### Claim 12 (depends on 4)

The method according to claim 4, wherein the dried substrate is calcinated up to 400° C. for 1 hour at a rate of 1° C./min in a furnace.

### Claim 13 (depends on 4)

The method according to claim 4, wherein the corrosion inhibitor is benzotriazole.

### Claim 14 (depends on 4)

The method according to claim 4, wherein the step of doping the TiO2 layer with a corrosion inhibitor comprises dipping the substrate in a solution of benzotriazole for 1 hour.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the concentration of benzotriazole solution is 10% by weight.

### Claim 16 (depends on 4)

The method according to claim 4, wherein the substrate is dried at 80° C. for 30 minutes after doping the TiO2 layer with the corrosion inhibitor.

### Claim 17 (depends on 4)

The method according to claim 4, wherein the substrate is dried for 30 minutes at 80° C. after doping the TiO2 layer with the corrosion inhibitor.

### Claim 18 (depends on 4)

The method according to claim 4, wherein the step of depositing the hybrid silicate layer on the TiO2 layer doped with the corrosion inhibitor consists of:
preparing a hybrid silica based sol;
applying the prepared hybrid silica-based sol on the doped TiO2 layer using a sol-gel dip technique by dipping the substrate formed with the doped TiO2 layer at a dipping speed of 18 cm/min and exposing the substrate for a duration of 100 seconds; and drying and the substrate at 120° C. for 1 hour.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the process of preparing the hybrid silica-based sol consists of:
preparing an organosiloxane sol by hydrolyzing a 3-glycidoxypropyltrimethoxysilane (GPTMS), a tetraethylorthosilicate (TEOS) and a 2-propanol in preset volume ratios;
hydrolyzing the organosiloxane sol by adding 5 ml of de-ionized water that is dissolved in 0.5 ml acetic acid in drop-wise to the an organosiloxane sol, after 1 hour since preparation;
stirring the hydrolyzed organosiloxane sol under ultrasonic agitation for 1 hour; and ageing the stirred hydrolyzed organosiloxane sol for 24 hrs for condensation.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the 3-glycidoxypropyltrimethoxysilane (GPTMS), the tetraethylorthosilicate (TEOS) and the 2-propanol are mixed in the preset volume ratios of 6:5:12.