# US 2010/0304134 A1 · Method for peeling pressure-sensitive adhesive optical film, and pressure-sensitive adhesive optical film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0304134 A1
- Document ID: US20100304134A1
- Status: Published application
- Kind: A1
- Application number: 12/864,047
- Filed: 2009-01-20
- Published: 2010-12-02
- Earliest claimed: 2008-01-25
- Assignees: Nitto Denko Corporation
- Inventors: Fumiko Nakano; Yutaka Moroishi; Aimi Matsuura; Toshitsugu Hosokawa; Akiko Tanaka
- Web page: https://patentgrep.com/patent/US20100304134A1

## CPC

- C09J 5/06: involving heating of the applied adhesive
- C09J 7/385: {Acrylic polymers}
- C09J 133/08: Homopolymers or copolymers of acrylic acid esters
- C08F 220/1804: {C4-(meth)acrylate, e.g. butyl (meth)acrylate, isobutyl (meth)acrylate or tert-butyl (meth)acrylate}
- C08K 5/14: Peroxides
- C08L 33/08: Homopolymers or copolymers of acrylic acid esters
- C09J 2301/302: the adhesive being pressure-sensitive, i.e. tacky at temperatures inferior to 30°C
- C09J 2301/502: process for debonding adherents
- G02F 1/1335: Structural association of cells with optical devices, e.g. polarisers or reflectors
- G02F 2202/28: Adhesive materials or arrangements
- Y10T 156/1126: Using direct fluid current against work during delaminating
- Y10T 156/1153: Temperature change for delamination [e.g., heating during delaminating, etc.]
- Y10T 156/1911: Heating or cooling delaminating means [e.g., melting means, freezing means, etc.]
- Y10T 428/28: Web or sheet containing structurally defined element or component and having an adhesive outermost layer
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An object of the invention is to provide a pressure-sensitive adhesive optical film-peeling method capable of easily detaching the pressure-sensitive adhesive optical film from a glass substrate with no damage to the glass substrate or no adhesive deposit on the glass substrate, and to provide a pressure-sensitive adhesive optical film suitable for use in such a peeling method. The invention is directed to a method for peeling a pressure-sensitive adhesive optical film from an optical film-carrying glass substrate including a glass substrate and the pressure-sensitive adhesive optical film bonded thereto, which includes: exposing the optical film-carrying glass substrate to an environment at a temperature of 40 to 98° C. and a relative humidity of 60 to 99% for three minutes or more; and then peeling the pressure-sensitive adhesive optical film from the glass substrate under the environment.

## Claims

### Claim 1

A method for peeling a pressure-sensitive adhesive optical film from an optical film-carrying glass substrate comprising a glass substrate and the pressure-sensitive adhesive optical film bonded thereto, comprising:
exposing the optical film-carrying glass substrate to an environment at a temperature of 40 to 98° C. and a relative humidity of 60 to 99% for three minutes or more; and
then peeling the pressure-sensitive adhesive optical film from the glass substrate under the environment.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the pressure-sensitive adhesive optical film has a pressure-sensitive adhesive layer made from an organic solvent-based pressure-sensitive adhesive composition comprising:
(1) 100 parts by weight of a (meth)acrylic polymer comprising 50% by weight or more of an alkyl (meth)acrylate monomer unit and 0.05 to 2% by weight of a hydroxyl group-containing monomer unit;
(2) 0.01 to 5 parts by weight of a silane coupling agent; and
(3) 0.01 to 5 parts by weight of a crosslinking agent.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the silane coupling agent is an amine type silane coupling agent.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the crosslinking agent is an isocyanate crosslinking agent.

### Claim 5 (depends on 1)

A pressure-sensitive adhesive optical film for use in the method according to claim 1, which comprises an optical film and a pressure-sensitive adhesive layer provided on at least one side of the optical film and which has an adhesive strength of 10 N/25 mm width or less after the pressure-sensitive adhesive optical film is bonded to a glass substrate and exposed to an environment at a temperature of 40 to 98° C. and a relative humidity of 60 to 99% for three minutes or more.

### Claim 6 (depends on 3)

The method according to claim 3, wherein the crosslinking agent is an isocyanate crosslinking agent.

### Claim 7 (depends on 2)

A pressure-sensitive adhesive optical film for use in the method according to claim 2, which comprises an optical film and a pressure-sensitive adhesive layer provided on at least one side of the optical film and which has an adhesive strength of 10 N/25 mm width or less after the pressure-sensitive adhesive optical film is bonded to a glass substrate and exposed to an environment at a temperature of 40 to 98° C. and a relative humidity of 60 to 99% for three minutes or more.

### Claim 8 (depends on 2)

The method according to claim 2, wherein the weight average molecular weight of the (meth)acrylic polymer is 500,000 or more.

### Claim 9 (depends on 2)

The method according to claim 2, wherein the pressure-sensitive adhesive layer is crosslinked and has a gel fraction of 45 to 90% by weight.

### Claim 10 (depends on 2)

The method according to claim 2, wherein the optical film comprises a polarizer.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the optical film comprises a transparent protective film.

### Claim 12 (depends on 2)

The method according to claim 2, wherein, prior to the exposing step, the pressure-sensitive adhesive optical film is bonded to the glass substrate with an adhesive strength of 20 N/25 mm width or more.