# US 2010/0304042 A1 · Method for forming superhigh stress layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0304042 A1
- Document ID: US20100304042A1
- Status: Published application
- Kind: A1
- Application number: 12/475,595
- Filed: 2009-05-31
- Published: 2010-12-02
- Earliest claimed: 2009-05-31
- Inventors: Hsiu-Lien Liao; Teng-Chun Tsai; Jei-Ming Chen; Yu-Tuan Tsai; Chien-Chung Huang
- Web page: https://patentgrep.com/patent/US20100304042A1

## CPC

- C23C 16/0218: {in a reactive atmosphere (C23C16/0227 takes precedence)}
- C23C 16/345: {Silicon nitride}
- H10P 14/6514: {by exposure to a plasma}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming super high stress layer is provided. First, a substrate is provided. Second, an ammonia-related pretreatment is performed on the substrate. The flow rate of ammonia is not less than s.c.c.m. and the high-frequency source power is set to be not less than 800 W. Later, the super high stress layer is formed on the substrate having undergone the ammonia-related pretreatment.

## Claims

### Claim 1

A method for forming a super high stress layer, comprising:
providing a substrate;
performing an ammonia-related pretreatment on said substrate under a high-frequency source power, wherein the flow rate of ammonia in said ammonia-related pretreatment is not less than 1000 s.c.c.m. and said high-frequency source power is set to be not less than 800 W; and
forming said super high stress layer on said substrate which has undergone said ammonia-related pretreatment.

### Claim 2 (depends on 1)

The method of claim 1, wherein a PVCVD procedure is carried out to obtain said super high stress layer on said substrate which has undergone said ammonia-related pretreatment.

### Claim 3 (depends on 1)

The method of claim 1, before said ammonia-related pretreatment further comprising:
performing a silicide procedure on said substrate.

### Claim 4 (depends on 1)

The method of claim 1, wherein said super high stress layer has a stress not greater than −3.5 GPa.

### Claim 5 (depends on 1)

The method of claim 1, wherein said ammonia-related pretreatment is carried out for not less than 25 seconds.

### Claim 6 (depends on 1)

The method of claim 1, wherein said ammonia-related pretreatment is carried out under a temperature not less than 400° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein said ammonia-related pretreatment is carried out on said substrate in the presence of an auxiliary gas.

### Claim 8 (depends on 7)

The method of claim 7, wherein said auxiliary gas is selected from a group consisting of N2, Ar, H2 and silane.

### Claim 9 (depends on 1)

The method of claim 1, wherein said super high stress layer has a compression stress.

### Claim 10 (depends on 1)

The method of claim 1, wherein said substrate comprises a PMOS.

### Claim 11

A method for forming a super high stress layer, comprising:
providing a substrate;
performing a silicide procedure on said substrate;
performing an ammonia-related pretreatment on said substrate under a temperature not greater than 400° C. and a under high-frequency source power, wherein the flow rate of ammonia in said ammonia-related pretreatment is not less than 1000 s.c.c.m. and said high-frequency source power is set to be not less than 800 W; and
forming said super high stress layer on said substrate which has undergone said ammonia-related pretreatment.

### Claim 12 (depends on 11)

The method of claim 11, wherein said super high stress layer has a compression stress.

### Claim 13 (depends on 11)

The method of claim 11, wherein said super high stress layer has a stress less than −3.5 GPa.

### Claim 14 (depends on 11)

The method of claim 11, wherein said ammonia-related pretreatment is carried out for not less than 25 seconds.

### Claim 15 (depends on 11)

The method of claim 11, wherein said substrate comprises an element with a critical dimension less than 65 Å.

### Claim 16 (depends on 11)

The method of claim 11, wherein said ammonia-related pretreatment is carried out on said substrate in the presence of an auxiliary gas.

### Claim 17 (depends on 16)

The method of claim 16, wherein said auxiliary gas is selected from a group consisting of N2, Ar, H2 and silane.

### Claim 18 (depends on 1)

The method of claim 1, wherein said substrate comprises a PMOS.

### Claim 19 (depends on 11)

The method of claim 11, wherein said super high stress layer comprises a nitride.

### Claim 20 (depends on 1)

The method of claim 1, wherein a PVCVD procedure is carried out to obtain said super high stress layer on said substrate which has undergone said ammonia-related pretreatment.