# US 2010/0304038 A1 · Titanium carbide or tungsten carbide with combustion synthesis to block porosity in c-c brake discs for antioxidation protection

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0304038 A1
- Document ID: US20100304038A1
- Status: Published application
- Kind: A1
- Application number: 12/473,857
- Filed: 2009-05-28
- Published: 2010-12-02
- Earliest claimed: 2009-05-28
- Assignees: Honeywell International Inc.; University of Notre Dame du Lac
- Inventors: Mark L. La Forest; Allen H. Simpson; Slawomir Fryska; Alexander Mukasyan
- Web page: https://patentgrep.com/patent/US20100304038A1

## CPC

- C04B 41/52: Multiple coating or impregnating {multiple coating or impregnating with the same composition or with compositions only differing in the concentration of the constituents, is classified as single coating or impregnation}
- C04B 41/009: {characterised by the material treated}
- C04B 41/89: for obtaining at least two superposed coatings having different compositions
- F16D 65/12: Discs; Drums for disc brakes
- F16D 69/02: Composition of linings {; Methods of manufacturing}
- C04B 2111/00362: {Friction materials, e.g. used as brake linings, anti-skid materials}
- F16D 2200/0052: Carbon
- F16D 2250/0046: Coating
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F16D: COUPLINGS FOR TRANSMITTING ROTATION; CLUTCHES; BRAKES

## Abstract

A metal powder is applied to the surface of the area of a carbon-carbon composite brake disc to be protected against migration of antioxidant. The metal powder may be titanium powder or tungsten powder. A chemical reaction between the metal powder and carbon is then initiated by heating the powder-coated brake to the ignition temperature via application of electric current (Joule preheating) or by heating it in a furnace. Upon combustion, the metal particles react with carbon in the composite, forming liquid carbide that flows into pores of the composite brake disc to be protected.

## Claims

### Claim 1

A method of protecting a carbon-carbon composite brake disc against migration of anti-oxidant composition through the porosity of the composite brake disc, which comprises:
providing a porous carbon-carbon composite brake disc;
applying a metal powder, selected from the group consisting of titanium powder and tungsten powder, to a surface area of the carbon-carbon composite brake disc to be protected;
instituting a chemical reaction by the application of electric current to the powdered metal, or by heating the powdered metal to its melting point, thereby instituting a combustion reaction which forms titanium carbide or tungsten carbide within the pores of said surface area of the carbon-carbon composite brake disc; and subsequently applying an anti-oxidant solution to the non-friction surfaces of the resulting carbon-carbon composite brake disc.

### Claim 2 (depends on 1)

The method of claim 1, wherein the average diameter of the titanium or tungsten powder particles ranges from 10 to 300 microns.

### Claim 3 (depends on 1)

The method of claim 1, wherein the metal powder is titanium powder and the combustion reaction begins at approximately 1725° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal powder is tungsten powder and the combustion reaction begins at approximately 3422° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein said chemical reaction is instituted by applying an electric current of from 500 to 1000 Amps to the metal powder.

### Claim 6 (depends on 1)

An aircraft landing system brake disc, manufactured by the method of claim 1.

### Claim 7

A method of manufacturing an aircraft brake disc which comprises the steps of:
providing a carbon-carbon composite aircraft brake disc with its non-friction surface presented in a horizontal plane to define an upper flat surface;
dusting tungsten or titanium particles having an average diameter of 20 microns onto said flat surface;
placing the upside down, powder-coated brake disc into a preheated oven having an inert atmosphere;
initiating a combustion reaction comprising a reaction between the tungsten or titanium and carbon present in the composite aircraft brake disc, said combustion reaction forming tungsten carbide or titanium carbide in liquid form;
permitting the liquid tungsten carbide or titanium carbide to flow into pores in said flat surface of the composite brake disc; and
permitting the liquid tungsten carbide or titanium carbide to solidify within said pores, thereby imparting to said flat surface of the carbon-carbon composite aircraft brake disc a resistance to potential migration of anti-oxidant composition through the porosity of the composite brake disc.

### Claim 8 (depends on 7)

The manufacturing method of claim 7, wherein said combustion reaction is initiated by applying an electrical current to the powder-coated carbon-carbon composite brake disc for a period of time sufficient to initiate said combustion reaction.

### Claim 9 (depends on 8)

The manufacturing method of claim 8, wherein said electrical current is a 500-1000 Amp current applied for 2-10 seconds.

### Claim 10 (depends on 7)

The manufacturing method of claim 7, wherein the average diameter of the titanium or tungsten powder particles ranges from 10 to 300 microns.

### Claim 11 (depends on 10)

The manufacturing method of claim 10, wherein the average diameter of the titanium or tungsten powder particles ranges from 20 to 200 microns.