# US 2010/0303913 A1 · Method for Nanoencapsulation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0303913 A1
- Document ID: US20100303913A1
- Status: Published application
- Kind: A1
- Application number: 12/446,553
- Filed: 2006-10-31
- Published: 2010-12-02
- Earliest claimed: 2006-10-31
- Assignees: William Marsh Rice University
- Inventors: Muhammed K. Gheith; Yu-Lun Fang; Michael S. Wong
- Web page: https://patentgrep.com/patent/US20100303913A1

## CPC

- A61K 9/5169: {Proteins, e.g. albumin, gelatin}
- A61K 9/5089: {Processes}
- A61P 43/00: Drugs for specific purposes, not provided for in groups A61P1/00-A61P41/00
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- A61P: SPECIFIC THERAPEUTIC ACTIVITY OF CHEMICAL COMPOUNDS OR MEDICINAL PREPARATIONS

## Abstract

Methods of nanoencapsulation are described herein. Embodiments of the method utilize the coacervation of a cationic polyelectrolyte with an anionic polyelectrolyte to form a novel capsular matrix. In particular, the novel methods may be used to encapsulate a suspension of a hydrophobic material such as a carotenoid. The disclosed methods do not require lengthy pH adjustments nor do they require the use of any toxic crosslinking agents. In one embodiment, a method of encapsulation comprises dispersing a hydrophobic compound in an organic solvent to form a solution. The method also comprises admixing an anionic polyelectrolyte and a cationic polyelectrolyte with the suspension to form a mixture. In addition, the method comprises quiescently cooling the mixture so as to cause self-crosslinking of a capsular matrix encapsulating the hydrophobic particles.

## Claims

### Claim 1

A method of encapsulation comprising:
a) admixing a hydrophobic compound in an organic solvent to form a mixture;
b) admixing an anionic polyelectrolyte and a cationic polyelectrolyte with the mixture to form a suspension of encapsulated hydrophobic particles;
c) quiescently cooling the suspension so as to cause self-crosslinking of the encapsulated hydrophobic particles to form a capsular matrix.

### Claim 2 (depends on 1)

The method of claim 1, wherein step (a) comprises admixing an amount of said hydrophobic compound in said organic solvent at a concentration greater than the saturation point of said organic solvent so as to form a mixture comprising a solution of the hydrophobic compound and a suspension of undissolved hydrophobic particles.

### Claim 3 (depends on 1)

The method of claim 1 wherein said mixture is a solution.

### Claim 4 (depends on 1)

The method of claim 1 wherein said mixture is an emulsion.

### Claim 5 (depends on 1)

The method of claim 1 wherein said mixture is a suspension.

### Claim 6 (depends on 1)

The method of claim 1 wherein step (b) comprises admixing the anionic polyelectrolyte before the cationic polyelectrolyte.

### Claim 7 (depends on 1)

The method of claim 1 wherein step (b) comprises admixing the cationic polyelectrolyte before the anionic polyelectrolyte.

### Claim 8 (depends on 1)

The method of claim 1 wherein step (b) comprises admixing the cationic polyelectrolyte and the anionic polyelectrolyte simultaneously.

### Claim 9 (depends on 1)

The method of claim 1 wherein step (b) comprises admixing the cationic polyelectrolyte and the anionic polyelectrolyte at a cationic polyelectrolyte to anionic polyelectrolyte weight ratio of at least 2:1.

### Claim 10 (depends on 1)

The method of claim 1 wherein step (a) comprises dispersing the hydrophobic compound at a temperature ranging from 40° C. to 80° C.

### Claim 11 (depends on 1)

The method of claim 1 wherein step (b) comprises admixing the anionic polyelectrolyte and the cationic polyelectrolyte at a temperature ranging from 40° C. to 60° C.

### Claim 12 (depends on 1)

The method of claim 1 wherein step (c) comprises cooling the mixture to a temperature ranging from 20° C. to 30° C.

### Claim 13 (depends on 1)

The method of claim 1 wherein step (c) comprises cooling the mixture at a pH ranging from 5 to 6.

### Claim 14 (depends on 1)

The method of claim 1 further comprising adjusting the pH of the mixture after step (b).

### Claim 15 (depends on 1)

The method of claim 1 further comprising dissolving the capsular matrix in water at a temperature ranging from 40° C. to 60° C. to form a suspension of capsules having an average diameter ranging from 1 nm to 1000 nm.

### Claim 16 (depends on 1)

The method of claim 1 wherein the cationic polyelectrolyte is a gelatin.

### Claim 17 (depends on 1)

The method of claim 1 wherein the cationic polyelectrolyte comprises chitosan, whey protein, albumin, beta-lactoglobulin, potato protein, faba bean legumin, soybean protein, or combinations thereof.

### Claim 18 (depends on 1)

The method of claim 1 wherein the anionic polyelectrolyte is gum arabic.

### Claim 19 (depends on 1)

The method of claim 1 wherein the anionic polyelectrolyte comprises any anionic polysaccharide, alginate, pectin, agar, carrageenan, or combinations thereof.

### Claim 20 (depends on 1)

The method of claim 1 wherein the hydrophobic compound comprises a carotenoid.

### Claim 21 (depends on 20)

The method of claim 20 wherein the carotenoid comprises lutein, antheraxanthin, astaxanthin, canthaxanthin, a-carotene, beta-carotene, cryptoxanthin, diatoxanthin, fucoxanthin, fucoxanthinol, lactucaxanthin, lycopene, neoxanthin, neurosporene, peridinin, phytoene, rhodopin, siphonaxanthin, spheroidene, spirilloxanthin, uriolide, uriolide acetate, violaxanthin, zeaxanthin, or combinations thereof.

### Claim 22 (depends on 1)

The method of claim 1 wherein the hydrophobic compound is selected from the group consisting of phytosterols and coenzymes Q.

### Claim 23 (depends on 1)

The method of claim 1 wherein the encapsulated hydrophobic particles have an average diameter ranging from about 1 nm to about 1000 nm.

### Claim 24 (depends on 1)

The method of claim 1 wherein the organic solvent comprises an alcohol.

### Claim 25 (depends on 1)

The method of claim 1 wherein the hydrophobic compound is an oil.

### Claim 26 (depends on 1)

The method of claim 1, further comprising adding a binder to the capsular matrix to dissolve the capsular matrix.

### Claim 27 (depends on 25)

The method of claim 25, further comprising grinding the capsular matrix into a powder.

### Claim 28 (depends on 25)

The method of claim 25 wherein the binder is a salt.

### Claim 29 (depends on 28)

The method of claim 28 wherein the binder comprises calcium chloride, sodium chloride, sodium bicarbonate, sodium sulfate, calcium carbonate, magnesium sulfate, starch or combinations thereof.

### Claim 30 (depends on 27)

The method of claim 27 wherein said powder is soluble in warm water.

### Claim 31 (depends on 27)

The method of claim 27 wherein said powder is soluble in cold water.

### Claim 32

A capsular matrix comprising:
a self-crosslinked network of capsules encapsulating a plurality of hydrophobic particles, wherein each capsule comprises a cationic polyelectrolyte and an anionic polyelectrolyte.

### Claim 33 (depends on 32)

The capsular matrix of claim 32 wherein said self-crosslinked network of capsules is water-soluble.

### Claim 34 (depends on 32)

The capsular matrix of claim 32 wherein said cationic polyelectrolyte comprises gelatin.

### Claim 35 (depends on 32)

The capsular matrix of claim 32 wherein said anionic polyelectrolyte comprises gum arabic.