# US 2010/0303419 A1 · Fiber end face void closing method, a connectorized optical fiber assembly, and method of forming same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0303419 A1
- Document ID: US20100303419A1
- Status: Published application
- Kind: A1
- Application number: 12/788,867
- Filed: 2010-05-27
- Published: 2010-12-02
- Earliest claimed: 2009-05-29
- Assignees: Corning Incorporated
- Inventors: Seldon David Benjamin; Robert Stephen Wagner; Percil Watkins
- Web page: https://patentgrep.com/patent/US20100303419A1

## CPC

- G02B 6/02342: {characterised by cladding features, i.e. light confining region}
- G02B 6/25: Preparing the ends of light guides for coupling, e.g. cutting
- G02B 6/02333: {Core having higher refractive index than cladding, e.g. solid core, effective index guiding}
- G02B 6/3863: {fabricated by using polishing techniques (grinding of the fibre ends B24B19/226)}
- Y10T 225/12: With preliminary weakening
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for closing the holes on the end face of a nano-engineered fiber having a core, a cladding with non-periodically disposed voids, and at least one of a coating and a buffer, comprises the steps of: (i) cleaving the fiber portion, thereby forming a cleaved end face; and (ii) applying a predetermined amount of energy via a laser beam to the cleaved end face, the amount of energy being sufficient to collapse and seal the voids exposed at the cleaved end face only to a depth of less than 11 μm.

## Claims

### Claim 1

A method for closing the voids on the end face of a nano-engineered fiber having a core, a cladding with non-periodically disposed voids, and at least one of a coating and a buffer, the method comprising the steps of:
(i) cleaving the fiber portion, thereby forming a cleaved end face; and
(ii) applying a predetermined amount of energy via a laser beam to the cleaved end face, the amount of energy being sufficient to collapse and seal the voids exposed at the cleaved end face only to a depth of less than 11 μm.

### Claim 2 (depends on 1)

The method of claim 1, wherein said energy is supplied by the output beam of a CO2 laser and the optical axis of the output beam intercepts the fiber end face.

### Claim 3 (depends on 1)

The method of claim 1, wherein said energy is supplied by the output beam of a CO2 laser and said holes to be sealed to a depth of no more than 5 μm and no more than 20 J/cm2 of energy is delivered to the end face of the fiber.

### Claim 4 (depends on 1)

A fiber processed by the method of claim 1, said fiber having an indentation in the fiber section end face, said indentation being less than 0.5 μm deep.

### Claim 5

A method of connectorizing an optical fiber comprising, in order, the steps of:
(a) providing a nano-engineered fiber having a core, a cladding with non-periodically disposed voids, and at least one of a coating and a buffer;
(b) stripping a length of the at least one of the coating and the buffer to expose an end portion of the optical fiber;
(c) mounting the optical fiber within a connector ferrule having a ferrule end face so that the exposed portion of the fiber protruding beyond the ferrule end face; and
(d) cleaving the exposed optical fiber portion that protrudes beyond the ferrule end face, forming a cleaved end face;
(e) applying a predetermined amount of energy to cleaved end-face sufficient to collapse and seal the voids exposed at the cleaved end face, to provide a fiber end face having no voids to a depth of not more than 11 μm.

### Claim 6 (depends on 5)

The method according to claim 5, including polishing the fiber end face to be in a common plane with the ferrule end face.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the optical fiber has an air-fill percent less than about 1% and greater than about 0.02%.

### Claim 8 (depends on 5)

The method according to claim 5, wherein the optical fiber has an air-fill percent less than about 0.7% and greater than about 0.02%.

### Claim 9 (depends on 5)

The method according to claim 5, wherein the optical fiber has an air-fill percent less than about 0.2% and greater than about 0.02%.

### Claim 10 (depends on 5)

The method according to claim 5, wherein the optical fiber has an average airline size less than about 0.3 microns and greater than 0.005 microns in cross-sectional diameter.

### Claim 11 (depends on 5)

The method according to claim 5, wherein the stripped optical fiber has a cross-sectional diameter that does not change by more than about 1% after the voids are collapsed.

### Claim 12 (depends on 5)

The method according to claim 5, wherein the energy is supplied directly to the cleaved end-face of the fiber by a laser.

### Claim 13

A connectorized nano-engineered optical fiber assembly, comprising:
(a) a connector ferrule having at least one bore and a ferrule end face;
(b) at least one nano-engineered fiber having a bare fiber section arranged in the at least one bore, the bare fiber section having a core, a cladding with non-periodically disposed voids formed therein, a bare-fiber diameter, and an end face formed by cleaving that is substantially to be co-planar with the ferrule end face; and
(c) wherein the bare fiber section comprises an airline-free portion that includes the bare fiber section end face that has (i) a void-free bare-fiber diameter substantially the same as the void-inclusive bare-fiber diameter and (ii) an indentation in the bare fiber section end face, said indentation being less than 0.5 μm deep.

### Claim 14 (depends on 13)

The assembly of claim 13, wherein the void-free bare-fiber diameter is within about 1% of the void-inclusive bare-fiber diameter, and the indentation is less than 0.2 μm deep

### Claim 15 (depends on 13)

The assembly of claim 13, wherein the void-inclusive bare-fiber diameter is 125 μm, and wherein the void-free bare-fiber diameter changes by no more than ±1 μm from the void-inclusive bare-fiber diameter; and the indentation depth is 3 nm to 50 nm.

### Claim 16 (depends on 13)

The assembly of claim 13, wherein the nano-engineered fiber has a corresponding mode-field diameter (MFD) at a pre-determined wavelength, and wherein the MFD does not change by more than 1% within the connector ferrule.

### Claim 17 (depends on 13)

The assembly of claim 13, wherein the nano-engineered fiber has a corresponding mode-field diameter (MFD) at a pre-determined wavelength, and wherein the MFD does not change by more than 0.5% within the connector ferrule.

### Claim 18 (depends on 13)

The assembly of claim 13, wherein the optical fiber has an air-fill percent less than about 0.7%.

### Claim 19 (depends on 13)

The assembly of claim 13, wherein the optical fiber has an air-fill percent less than about 0.2%.