# US 2010/0300878 A1 · Sintered Oxide Compact Target for Sputtering and Process for Producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0300878 A1
- Document ID: US20100300878A1
- Status: Published application
- Kind: A1
- Application number: 12/864,553
- Filed: 2009-06-05
- Published: 2010-12-02
- Earliest claimed: 2008-06-10
- Assignees: Nippon Mining & Metals Co., Ltd.
- Inventors: Kozo Osada; Hiroaki Ohtsuka
- Web page: https://patentgrep.com/patent/US20100300878A1

## CPC

- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- C04B 35/453: based on zinc, tin, or bismuth oxides or solid solutions thereof with other oxides, e.g. zincates, stannates or bismuthates
- C04B 35/6261: {Milling}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/62675: {characterised by the treatment temperature}
- C04B 35/63416: {Polyvinylalcohols [PVA]; Polyvinylacetates}
- C23C 14/086: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C04B 2235/3284: Zinc oxides, zincates, cadmium oxides, cadmiates, mercury oxides, mercurates or oxide forming salts thereof
- C04B 2235/3286: Gallium oxides, gallates, indium oxides, indates, thallium oxides, thallates or oxide forming salts thereof, e.g. zinc gallate
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/604: Pressing at temperatures other than sintering temperatures
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/6585: at an oxygen percentage above that of air
- C04B 2235/77: Density
- C04B 2235/786: Micrometer sized grains, i.e. from 1 to 100 micron
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- H01B 1/08: oxides
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

Provided is a sintered oxide compact target for sputtering comprising indium (In), gallium (Ga), zinc (Zn), oxygen (O) and unavoidable impurities, wherein the composition ratio of the respective elements satisfies the Formula of InxGayZnzOa {wherein 0.2≦x/(x+y)≦0.8, 0.1≦z/(x+y+z)≦0.5, a=(3/2)x+(3/2)y+z}, and the number of ZnGa2O4 spinel phases having an average grain size of 3 μm or larger existing in a 90 μm×90 μm area range of the sintered oxide compact target is 10 or less. With this sintered oxide compact target for sputtering comprising In, Ga, Zn, O and unavoidable impurities, the structure of the sintered compact target is improved, the formation of a phase to become the source of nodules is minimized, and the bulk resistance value is reduced. Whereby provided is a high density IGZO target capable of inhibiting abnormal discharge and which can be used in DC sputtering.

## Claims

### Claim 1

A sintered oxide compact target for sputtering comprising indium (In), gallium (Ga), zinc (Zn), oxygen (O) and unavoidable impurities, wherein a composition ratio of the respective elements satisfies a Formula of InxGayZnzOa, wherein 0.2≦x/(x+y)≦0.8, 0.1≦z/(x+y+z)≦0.5, a=(3/2)x+(3/2)y+z, and the number of ZnGa2O4 spinel phases having an average grain size of 3 μm or larger existing in a 90 μm×90 μm area range of the sintered oxide compact target is 10 or less.

### Claim 2 (depends on 1)

The sintered oxide compact target for sputtering according to claim 1, wherein a maximum grain size of the ZnGa2O4 spinel phases existing in a 90 μm×90 μm area range of the sintered oxide compact target is 5 μm or less.

### Claim 3 (depends on 2)

The sintered oxide compact target for sputtering according to claim 2, wherein a target density is 6.0 g/cm3 or more, and a bulk resistance value is 5.0×10−2 Ω·cm or less.

### Claim 4

A method of producing a sintered oxide compact target for sputtering comprising indium (In), gallium (Ga), zinc (Zn), oxygen (O) and unavoidable impurities, wherein raw material powders of indium oxide (In2O3), gallium oxide (Ga2O3), and zinc oxide (ZnO) are adjusted so that a composition ratio of the respective elements will become a Formula of InxGayZnzOa, wherein 0.2≦x/(x+y)≦0.8, 0.1≦z/(x+y+z)≦0.5, a=(3/2)x+(3/2)y+z, a specific surface area of the In2O3 raw material powder is set to be 10 m2/g or less, the raw material powders are mixed and additionally pulverized, and thereafter sintered at a temperature range of 1400 to 1480-1490° C.

### Claim 5 (depends on 4)

The method of producing a sintered oxide compact target for sputtering according to claim 4, wherein, during the processing of mixing and pulverizing the raw material powders of In2O3, Ga2O3 and ZnO, pulverization is performed until the difference in specific surface area before and after pulverization becomes 2.0 m2/g or more.

### Claim 6 (depends on 1)

The sintered oxide compact target for sputtering according to claim 1, wherein target density is 6.0 g/cm3 or more, and a value of bulk resistance is 5.0×10−2 Ω·cm or less.