# US 2010/0300634 A1 · Method of making medium density fiberboard

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0300634 A1
- Document ID: US20100300634A1
- Status: Published application
- Kind: A1
- Application number: 12/854,574
- Filed: 2010-08-11
- Published: 2010-12-02
- Earliest claimed: 2006-09-01
- Assignees: Wisconsin Alumni Research Foundation; Biopulping International, Inc.; The United States of America as represented by the Secretary of Agriculture
- Inventors: Masood Akhtar; William R. Kenealy; Eric G. Horn; Ross E. Swaney; Jerrold Winandy
- Web page: https://patentgrep.com/patent/US20100300634A1

## CPC

- D21C 3/04: with acids, acid salts or acid anhydrides {(D21C3/003 and D21C3/222 take precedence)}
- D21C 1/04: with acid reacting compounds
- D21C 5/005: {Treatment of cellulose-containing material with microorganisms or enzymes}
- D21C 11/0007: {Recovery of by-products, i.e. compounds other than those necessary for pulping, for multiple uses or not otherwise provided for (volatile compounds obtained by decomposition of spent liquors in order to regenerate them D21C11/125; compounds obtained by fractionating the liquors in order to regenerate them D21C11/0042)}
- Y10T 428/1303: Paper containing [e.g., paperboard, cardboard, fiberboard, etc.]
- D21C: PRODUCTION OF CELLULOSE BY REMOVING NON-CELLULOSE SUBSTANCES FROM CELLULOSE-CONTAINING MATERIALS; REGENERATION OF PULPING LIQUORS; APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides a method for producing an MDF board from pulp from a fibrous lignocellulose material using a treatment or pretreatment step which exposes the material to oxalic acid or oxalic acid derivatives (particularly dialkyl ester derivatives, particularly in the vapor phase). The treated wood is then subjected to a sugar extraction wash and refined using any one of the several pulping methods to produce a final pulp product. Once this is done the pulp is used to make MDF boards having improved water repellency properties.

## Claims

### Claim 1

A method of making Medium Density Fiberboard (MDF) having improved moisture tolerance comprising:
providing a reduced material in water comprising one or more fibrous lignocelluloses having particle sizes in the range of 1-100 mm in length;
treating the reduced material with a compound having the formula
wherein R1 and R2 are independently a member selected from the group consisting of —OH, halide, substituted amine, unsubstituted amine, —OR3, and
wherein R3 and R4 are independently a branched or unbranched, cyclic or linear, saturated or unsaturated, substituted or unsubstituted C1-10 alkyl, at a temperature in the range of 90-170° C. generating a treated reduced material;
extracting hemicellulose sugars from the treated reduced material generating a pulp;
adding a suitable resin to the fibrous pulp; and
fiberizing the fibrous pulp into medium density fiber board.

### Claim 2 (depends on 1)

The method of claim 1, wherein the reduced material is treated with less than 6 dry wt % of the compound.

### Claim 3 (depends on 2)

The method of claim 2, wherein the reduced material is treated with less than 6 dry wt % of the compound.

### Claim 4 (depends on 2)

The method of claim 2, wherein the reduced material is treated with 0.05-5 dry wt % of the compound.

### Claim 5 (depends on 2)

The method of claim 2, wherein the reduced material is treated with 1-3 dry wt % of the compound.

### Claim 6 (depends on 2, 3, 4, 5)

The method of any one of claims 2-5, wherein R1 and R2 are —OH.

### Claim 7 (depends on 2, 3, 4, 5)

The method of any one of claims 2-5, wherein R1 and R2 are —OR3, and wherein R3 is an ethyl.

### Claim 8 (depends on 2, 3, 4, 5)

The method of any one of claims 2-5, wherein R1 and R2 are —OR3, and wherein R3 is a methyl.

### Claim 9 (depends on 2)

The method of claim 2, wherein the reduced material is treated at a pressure less than 90 psig.

### Claim 10 (depends on 2)

The method of claim 2, wherein the reduced material is treated for a duration less than 4 hours.

### Claim 11 (depends on 2)

The method of claim 2, wherein the reduced material is treated for a duration in the range of 5 min. to 2 hours.

### Claim 12 (depends on 2)

The method of claim 2, wherein the reduced material is treated at a temperature in the range of 130-140° C.

### Claim 13 (depends on 2)

The method of claim 2, wherein the suitable resin is a phenol-formaldehyde resin, and wherein a wax is further added to the fibrous pulp.

### Claim 14 (depends on 13)

The method of claim 13, wherein the medium density fiber board comprises 93.5 wt % fiber, 6 wt % resin, and 0.5% wax.

### Claim 15 (depends on 2)

The method of claim 2, wherein the reduced material is refined by using a processing technique selected from the group consisting of mechanical pulping, thermo-mechanical pulping, and chemical treatment with mechanical pulping.

### Claim 16 (depends on 2)

The method of claim 2, further comprising:
mechanically refining the treated reduced material one or more times to achieve a predetermined level of freeness of the treated reduced material; and
dewatering the refined and treated reduced material one or more times.

### Claim 17 (depends on 16)

The method of claim 16, wherein the treated reduced material is mechanically refined 2-6 times, and wherein a freeness value of 100 ml CSF is achieved.

### Claim 18 (depends on 1)

The method of claim 1, wherein the ratio of water:fibrous lignocellulose is in the range of 4:1 to 8:1.

### Claim 19 (depends on 2)

The method of claim 2, wherein the fibrous lignocellulose includes one or more members selected from the group consisting of southern yellow pine, red pine, spruce, western hemlock, aspen, loblolly pine and recovered paper.

### Claim 20 (depends on 19)

The method of claim 19, wherein the particle size is in the range of 6-14 mm in length.

### Claim 21 (depends on 2)

The method of claim 2, wherein the step of treating the reduced material includes cooking the material at a temperature in the range of 90-170° C.

### Claim 22 (depends on 2)

The method of claim 2, wherein the reduced material is further treated with one or more suitable enzymes and/or acetic acid.

### Claim 23 (depends on 1)

The method of claim 1, wherein the refining step can be performed either before or after the sugar extraction step.

### Claim 24

(canceled)

### Claim 25

(canceled)

### Claim 26

(canceled)

### Claim 27

(canceled)

### Claim 28

(canceled)