# US 2010/0300506 A1 · Low-cost high-efficiency solar module using epitaxial si thin-film absorber and double-sided heterojunction solar cell with integrated module fabrication

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0300506 A1
- Document ID: US20100300506A1
- Status: Published application
- Kind: A1
- Application number: 12/476,991
- Filed: 2009-06-02
- Published: 2010-12-02
- Earliest claimed: 2009-06-02
- Assignees: Sierra Solar Power, Inc.
- Inventors: Jiunn Benjamin Heng; Chentao Yu; Zheng Xu; Jianming Fu; Peijun Ding
- Web page: https://patentgrep.com/patent/US20100300506A1

## CPC

- H10F 10/166: the Group IV-IV heterojunctions being heterojunctions of crystalline and amorphous materials, e.g. silicon heterojunction [SHJ] photovoltaic cells
- H10F 10/161: comprising multiple PN heterojunctions, e.g. tandem cells
- H10F 10/165: the heterojunctions being Group IV-IV heterojunctions, e.g. Si/Ge, SiGe/Si or Si/SiC photovoltaic cells
- H10F 19/807: {Double-glass encapsulation, e.g. photovoltaic cells arranged between front and rear glass sheets}
- H10F 19/904: {characterised by the shapes of the structures}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/1395: {for thin-film devices}
- H10F 77/148: {Shapes of potential barriers}
- H10F 77/311: {for photovoltaic cells}
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

One embodiment of the present invention provides a double-sided heterojunction solar cell module. The solar cell includes a frontside glass cover, a backside glass cover situated below the frontside glass cover, and a number of solar cells situated between the frontside glass cover and the backside glass cover. Each solar cell includes a semiconductor multilayer structure situated below the frontside glass cover, including: a frontside electrode grid, a first layer of heavily doped amorphous Si (a-Si) situated below the frontside electrode, a layer of lightly doped crystalline-Si (c-Si) situated below the first layer of heavily doped a-Si, and a layer of heavily doped c-Si situated below the lightly doped c-Si layer. The solar cell also includes a second layer of heavily doped a-Si situated below the multilayer structure; and a backside electrode situated below the second layer of heavily doped a-Si.

## Claims

### Claim 1

A method for fabricating a double-sided heterojunction solar cell, comprising:
depositing a layer of heavily doped crystalline-Si (c-Si) on the surface of a metallurgical-grade silicon (MG-Si) substrate;
depositing a layer of lightly doped c-Si;
depositing a first layer of heavily doped amorphous-Si (a-Si);
forming a frontside electrode grid;
laminating a frontside glass cover over the frontside electrode grid;
removing the MG-Si substrate;
depositing a second layer of heavily doped a-Si on the backside of the heavily doped c-Si layer;
forming a backside electrode; and
laminating a backside glass cover over the backside electrode.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming a porous Si layer on the surface of the MG-Si substrate.

### Claim 3 (depends on 2)

The method of claim 2, wherein the MG-Si substrate is removed using one or more of the following techniques:
chemical etching;
applying a shear or piezoelectric force;
applying a temperature gradient;
applying an ultra/mega-sonic force;
applying a tensile or compressive mechanical force; and
pumping a pressurized gas into the porous Si layer.

### Claim 4 (depends on 1)

The method of claim 1, further comprising texturing at least one side of the lightly doped c-Si layer.

### Claim 5 (depends on 1)

The method of claim 1, further comprising placing a layer of adhesive polymer between the frontside glass cover and the frontside electrode grid, and wherein the lamination process comprises applying heat and pressure.

### Claim 6 (depends on 5)

The method of claim 5, further comprising placing a layer of frontside metal wires between the frontside electrode grid and the polymer layer, and wherein the frontside metal wires are soldered to the frontside electrode grid during the lamination process.

### Claim 7 (depends on 5)

The method of claim 5, wherein the refractive index of the polymer matches the glass's refractive index.

### Claim 8 (depends on 1)

The method of claim 1, further comprising placing a layer of adhesive polymer between the backside glass cover and the backside electrode, and wherein the backside electrode comprises Ag or Al finger grid.

### Claim 9 (depends on 8)

The method of claim 8, further comprising placing a layer of backside metal wires between the backside electrode grid and the polymer layer, wherein the backside metal wires are aligned to corresponding frontside metal wires, thereby forming an electrical connection.

### Claim 10 (depends on 1)

The method of claim 1, further comprising depositing a layer of transparent conductive oxide (TCO) material prior to the formation of at least one electrode.

### Claim 11 (depends on 1)

The method of claim 1, wherein the frontside glass cover is laminated over a plurality of solar cells, and wherein the MG-Si substrates of the plurality of solar cells are removed using a batch process.

### Claim 12 (depends on 11)

The method of claim 11, further comprising applying a mask before depositing the second layer of heavily doped a-Si to protect the frontside glass region between individual solar cells.

### Claim 13 (depends on 1)

The method of claim 1, wherein the lightly doped c-Si layer is deposited using a CVD technique, wherein the thickness of the lightly doped c-Si layer is between 5 μm and 100 μm, and wherein the doping concentration for the lightly doped c-Si layer is between 1×1016/cm3 and 1×1017/cm3.

### Claim 14 (depends on 1)

The method of claim 1, wherein at least one heavily doped a-Si layer is deposited using a CVD technique, wherein the thickness of the at least one heavily doped a-Si layer is between 10 nm and 50 nm, and wherein the doping concentration for the at least one heavily doped a-Si layer is between 1×1017/cm3 and 1×102°/cm3.

### Claim 15 (depends on 1)

The method of claim 1, wherein the heavily doped and lightly doped c-Si layers are n-type doped, wherein the first heavily doped a-Si layer is p-type doped, and wherein the second heavily doped a-Si layer is n-type doped.

### Claim 16 (depends on 1)

The method of claim 1, wherein the heavily doped c-Si layer acts as a back-surface-field (BSF) layer, wherein the heavily doped c-Si layer is deposited using a chemical-vapor-deposition (CVD) technique, wherein the thickness of the heavily doped c-Si layer is between 1 μm and 10μm, and wherein the doping concentration for the heavily doped c-Si layer is between 1×1017/cm3 and 1×102°/cm3.

### Claim 17 (depends on 1)

The method of claim 1, further comprising depositing a passivation layer on at least one side of the lightly doped c-Si layer, wherein the thickness of the passivation layer is between 1 nm and 10 nm, and wherein the passivation layer includes at least one of: undoped a-Si and SiOx.

### Claim 18

A double-sided heterojunction solar cell, comprising:
a frontside glass cover;
a semiconductor multilayer structure situated below the frontside glass cover, comprising:
a frontside electrode grid,
a first layer of heavily doped amorphous Si (a-Si) situated below the frontside electrode,
a layer of lightly doped crystalline-Si (c-Si) situated below the first layer of heavily doped a-Si, and
a layer of heavily doped c-Si situated below the lightly doped c-Si layer;
a second layer of heavily doped a-Si situated below the multilayer structure;
a backside electrode situated below the second layer of heavily doped a-Si; and
a second glass cover situated below the backside electrode.

### Claim 19 (depends on 18)

The solar cell of claim 18, wherein the multilayer structure is epitaxially grown on a metallurgical-Si (MG-Si) substrate.

### Claim 20 (depends on 19)

The solar cell of claim 19, wherein the MG-Si substrate further comprises a layer of porous Si.

### Claim 21 (depends on 20)

The solar cell of claim 20, wherein the MG-Si substrate is removed prior to the formation of the second layer of heavily doped a-Si, and wherein the MG-Si substrate is removed using one or more of the following techniques:
chemical etching;
applying a shear or piezoelectric force;
applying a temperature gradient;
applying an ultra/mega-sonic force;
applying a tensile or compressive mechanical force; and
pumping a pressurized gas into the porous Si layer.

### Claim 22 (depends on 18)

The solar cell of claim 18, wherein at least one side of the lightly doped c-Si layer is textured.

### Claim 23 (depends on 18)

The solar cell of claim 18, further comprising a first adhesive polymer layer situated between the frontside glass cover and the multilayer structure, and wherein the adhesive polymer layer, the frontside glass cover, and the multilayer structure are laminated together by applying heat and pressure.

### Claim 24 (depends on 23)

The solar cell of claim 23, further comprising a layer of frontside metal wires situated between the frontside electrode grid and the polymer layer; and wherein the frontside metal wires are soldered to the frontside electrode grid during the lamination process.

### Claim 25 (depends on 23)

The solar cell of claim 23, wherein the refractive index of the polymer matches the glass's refractive index.

### Claim 26 (depends on 18)

The solar cell of claim 18, further comprising a second adhesive polymer layer situated between the backside glass cover and the backside electrode, and wherein the backside electrode comprises Ag or Al finger grid.

### Claim 27 (depends on 26)

The solar cell of claim 26, further comprising a layer of backside metal wires situated between the backside electrode grid and the second polymer layer, wherein the backside metal wires are aligned to corresponding frontside metal wires, thereby forming an electrical connection between the solar cell and an adjacent solar cell.

### Claim 28 (depends on 18)

The solar cell of claim 18, further comprising at least one layer of transparent conductive oxide (TCO) material situated between an electrode and a heavily doped a-Si layer.

### Claim 29 (depends on 18)

The solar cell of claim 18, wherein the lightly doped c-Si layer is deposited using a CVD technique, wherein the thickness of the lightly doped c-Si layer is between 5 μm and 100 μm, and wherein the doping concentration for the lightly doped c-Si layer is between 1×1016/cm3 and 1×1017/cm3.

### Claim 30 (depends on 18)

The solar cell of claim 18, wherein at least one heavily doped a-Si layer is deposited using a CVD technique, wherein the thickness of the at least one heavily doped a-Si layer is between 10 nm and 50 nm, and wherein the doping concentration for the at least one heavily doped a-Si layer is between 1×1017/cm3 and 1×102°/cm3.

### Claim 31 (depends on 18)

The solar cell of claim 18, wherein the heavily doped and lightly doped c-Si layers are n-type doped, wherein the first heavily doped a-Si layer is p-type doped, and wherein the second heavily doped a-Si layer is n-type doped.

### Claim 32 (depends on 18)

The solar cell of claim 18, wherein the heavily doped c-Si layer acts as a back-surface-field (BSF) layer, wherein the heavily doped c-Si layer is deposited using a chemical-vapor-deposition (CVD) technique, wherein the thickness of the heavily doped c-Si layer is between 1 μm and 10 μm, and wherein the doping concentration for the heavily doped c-Si layer is between 1×1017/cm3 and 1×102°/cm3.

### Claim 33 (depends on 18)

The solar cell of claim 18, further comprising at least one passivation layer on at least one side of the lightly doped c-Si layer, wherein the thickness of the passivation layer is between 1 nm and 10 nm, and wherein the passivation layer includes at least one of: undoped a-Si and SiOx.

### Claim 34

A double-sided heterojunction solar cell module, comprising:
a frontside glass cover;
a backside glass cover situated below the frontside glass cover; and
a number of solar cells situated between the frontside glass cover and the backside glass cover, wherein each solar cell comprises:
a semiconductor multilayer structure situated below the frontside glass cover, comprising:
a frontside electrode grid,
a first layer of heavily doped amorphous Si (a-Si) situated below the frontside electrode,
a layer of lightly doped crystalline-Si (c-Si) situated below the first layer of heavily doped a-Si, and
a layer of heavily doped c-Si situated below the lightly doped c-Si layer;
a second layer of heavily doped a-Si situated below the multilayer structure; and
a backside electrode situated below the second layer of heavily doped a-Si.

### Claim 35 (depends on 34)

The solar cell module of claim 34, wherein the multilayer structure is epitaxially grown on a metallurgical-Si (MG-Si) substrate.

### Claim 36 (depends on 35)

The solar cell module of claim 35, wherein the MG-Si substrate further comprises a layer of porous Si.

### Claim 37 (depends on 36)

The solar cell module of claim 36, wherein the MG-Si substrate is removed prior to the formation of the second layer of heavily doped a-Si, and where in the MG-Si substrate is removed using one or more of the following techniques:
chemical etching;
applying a shear or piezoelectric force;
applying a temperature gradient;
applying an ultra/mega-sonic force;
applying a tensile or compressive mechanical force; and
pumping a pressurized gas into the porous Si layer.

### Claim 38 (depends on 34)

The solar cell module of claim 34, wherein at least one side of the lightly doped c-Si layer is textured.

### Claim 39 (depends on 34)

The solar cell module of claim 34, further comprising a first adhesive polymer layer situated between the frontside glass cover and the solar cells, and wherein the adhesive polymer layer, the frontside glass cover, and the solar cells are laminated together by applying heat and pressure.

### Claim 40 (depends on 39)

The solar cell module of claim 39, further comprising a layer of frontside metal wires situated between the frontside electrode grid and the polymer layer, and wherein the frontside metal wires are soldered to the frontside electrode grid during the lamination process.

### Claim 41 (depends on 39)

The solar cell module of claim 39, wherein the refractive index of the polymer matches the glass's refractive index.

### Claim 42 (depends on 34)

The solar cell module of claim 34, further comprising a second adhesive polymer layer situated between the backside glass cover and the backside electrode, and wherein the backside electrode comprises Ag or Al finger grid.

### Claim 43 (depends on 42)

The solar cell module of claim 42, further comprising a layer of backside metal wires situated between the backside electrode grid and the second polymer layer, wherein the backside metal wires are aligned to corresponding frontside metal wires, thereby forming an electrical connection between adjacent solar cells.

### Claim 44 (depends on 34)

The solar cell module of claim 34, wherein the frontside glass region between individual solar cells is protected by a mask during a subsequent fabrication process.

### Claim 45 (depends on 34)

The solar cell module of claim 34, wherein each solar cell further comprises at least one layer of transparent conductive oxide (TCO) material situated between an electrode and a heavily doped a-Si layer.

### Claim 46 (depends on 34)

The solar cell module of claim 34, wherein the lightly doped c-Si layer is deposited using a CVD technique, wherein the thickness of the lightly doped c-Si layer is between 5 μm and 100 μm, and wherein the doping concentration for the lightly doped c-Si layer is between 1×1016/cm3 and 1×1017/cm3.

### Claim 47 (depends on 34)

The solar cell module of claim 34, wherein at least one heavily doped a-Si layer is deposited using a CVD technique, wherein the thickness of the at least one heavily doped a-Si layer is between 10 nm and 50 nm, and wherein the doping concentration for the at least one heavily doped a-Si layer is between 1×1017/cm3 and 1×102°/cm3.

### Claim 48 (depends on 34)

The solar cell module of claim 34, wherein the heavily doped and lightly doped c-Si layers are n-type doped, wherein the first heavily doped a-Si layer is p-type doped, and wherein the second heavily doped a-Si layer is n-type doped.

### Claim 49 (depends on 34)

The solar cell module of claim 34, wherein the heavily doped c-Si layer acts as a back-surface-field (BSF) layer, wherein the heavily doped c-Si layer is deposited using a chemical-vapor-deposition (CVD) technique, wherein the thickness of the heavily doped c-Si layer is between 1 μm and 10 μm, and wherein the doping concentration for the heavily doped c-Si layer is between 1×1017/cm3 and 1×102°/cm3.

### Claim 50 (depends on 34)

The solar cell of claim 34, further comprising at least one passivation layer on at least one side of the lightly doped c-Si layer, wherein the thickness of the passivation layer is between 1 nm and 10 nm, and wherein the passivation layer includes at least one of: undoped a-Si and SiOx.